Internationale Stahläquivalente
| Europa (EN) | Deutschland (DIN) | USA (AISI) | Japan (JIS) | GUS (GOST) |
|---|---|---|---|---|
| 1.4713 | X10CrAl7 | 10CR17CU | ||
| 1.4724 | X10CrAl13 | 405 | 10CR13CU | |
| 1.4742 | X10CrAl18 | 442 | ||
| 1.4762 | X10CrAl24 | 446 | ||
| 1.4878 | X12CrNiTi18−9 | 321 H | 12X18H10T | |
| 1.4828 | X15CrNiSi20−12 | 309 | 20X20H14C2 | |
| 1.4845 | X12CrNi25−21 | 310 S | 20CR23NI18 | |
| 1.4841 | X15CrNiSi25−20 | 314 | 20CR25H20C2 |
Quelle: www.uvis.ua
| Europa (EN) | Deutschland (DIN) | USA (AISI) | Japan (JIS) | GUS (GOST) |
|---|---|---|---|---|
| 1.4003 | X2CrNi12 | |||
| 1.4512 | X2CrTi12 | 409 | SUH 409 | |
| 1.4000 | X6Cr13 | 410S | SUS 410 S | 08KH13 |
| 1.4002 | X6CrAl13 | 405 | SUS 405 | |
| 1.4006 | X12CrN13 | 410 | SUS 410 | 12KH13 |
| 1.4024 | X15Cr13 | (410) | SUS 410 J1 | |
| 1.4021 | X20Cr13 | (420) | SUS 420 J1 | 20Х13 |
| 1.4028 | X30Cr13 | (420) | SUS 420 J2 | 30KH13 |
| 1.4031 | X39Cr13 | SUS 420 J2 | 40KH13 | |
| 1.4034 | X46Cr13 | (420) | 40KH13 | |
| 1.4016 | X6Cr17 | 430 | SUS 430 | 12Х17 |
| 1.4520 | X2CrTi17 | |||
| 1.4510 | X3CrTi17 | 439 | SUS 430 LX | 08CR17TI |
| 1.4113 | X6CrMo17−1 | 434 | SUS 434 | |
| 1.4509 | X2CrTiNb18 | 441 | ||
| 1.4521 | X2CrMoTi18−2 | 444 | SUS 444 | |
| 1.4589 | X5CrNiMoTi15−2 | |||
| 1.4310 | X10CrNi18−8 | (301) | SUS 301 | |
| 1.4318 | X2CrNiN18−7 | 301 LN | SUS 301 LN | |
| 1.4301 | X5CrNI18−10 | 304 | SUS 304 | 08CR18NI10 |
| 1.4303 | X4CrNi18−12 | (305) | SUS 305 | 12X18H12 |
| 1.4306 | X2CrNi19−11 | 304 L | SUS 304 L | 03CR18NI11 |
| 1.4541 | X6CrNiTi18−10 | 321 | SUS 321 | 08CR18NITI10T |
| 1.4550 | X6CrNiNb18−10 | 347 | SUS 347 | |
| 1.4401 | X5CrNiMo17−12−2 | 316 | SUS 316 | |
| 1.4404 | X2CrNiMo17−12−2 | 316 L | SUS 316 L | |
| 1.4571 | X6CrNiMoTi17−12−2 | 316 Ti | SUS 316 Ti | 10X17H13M2T |
| 1.4561 | X1CrNiMoTi18−13−2 | |||
| 1.4435 | X2CrNiMo18−14−3 | 316 L | SUS 316 L | 03CR17H14M2 |
| 1.4439 | X2CrNiMoN17−13−5 | S 31 726 | SUS 317 | |
| 1.4539 | X1NiCrMoCu25−20−5 | N 8 904 | ||
| 1.4565 | X3CrNiMnMoNbN 23−17−5-3 | S 34 565 | ||
| 1.4462 | X2CrNiMoN22−5-3 | S 31 803 | SUS 329 J3L | |
| Europa (EN) | Deutschland (DIN) | USA (AISI) | Japan (JIS) | GUS (GOST) |
Quelle: www.uvis.ua
| GUS (GOST) | Euronormen (EN) | Deutschland (DIN) | USA (AISI) |
|---|---|---|---|
| 03 X17 H13 M2 | 1.4404 | X2 CrNiMo 17−12−2 | 316 L |
| 03 X17 H14 M3 | 1.4435 | X2 CrNiMo 18−4-3 | - |
| 03 X18 H11 | 1.4306 | X2 CrNi 19−11 | 304 L |
| 03 X18 H10 T-U | 1.4541-MOD | - | - |
| 06 CHN28-MDT | 1.4503 | X3 NiCrCuMoTi 27−23 | - |
| 06 X18 H11 | 1.4303 | X4 CrNi 18−11 | 305 L |
| 08 X12 T1 | 1.4512 | X6 CrTi 12 | 409 |
| 08 Х13 | 1.4000 | X6 Cr 13 | 410S |
| 08 CR17 H13 M2 | 1.4436 | X5CrNiMo 17−13−3 | 316 |
| 08 X17 H13 M2 T | 1.4571 | X6 CrNiMoTi 17−12−2 | 316Ti |
| 08 CR17 T | 1.4510 | X6 CrTi 17 | 430Ti |
| 08 X18 H10 | 1.4301 | X5 CrNi 18−10 | 304 |
| 08 CR18 H12 T | 1.4541 | X6 CrNiTi 18−10 | 321 |
| 10 X23 H18 | 1.4842 | X12 CrNi 25−20 | 310S |
| 10X13 | 1.4006 | X10 Cr13 | 410 |
| 12 X18 H10 T | 1.4878 | X12 CrNiTi 18−9 | - |
| 12 X18 H9 | - | - | 302 |
| 15 X5 M | 1.7362 | X12 CrCo 5 | 501 |
| 15 X25 T | 1.4746 | X8 CrTi 25 | - |
| 20X13 | 1.4021 | X20 Cr 13 | 420 |
| 20 X17 H2 | 1.4057 | X20 CrNi 17−2 | 431 |
| 20 X23 H13 | 1.4833 | X7 CrNi 23−14 | 309 |
| 20 X23 H18 | 1.4843 | X16 CrNi 25−20 | 310 |
| 20 X25 H20 C2 | 1.4841 | X56 CrNiSi 25−20 | 314 |
| 03 X18 AH11 | 1.4311 | X2 CrNiN 18−10 | 304LN |
| 03 X19 H13 M3 | 1.4438 | X2 18−5-4 | 317L |
| 03 X23 H6 | 1.4362 | X2 CrNiN 23−4 | - |
| 02 X18 M2 BT | 1.4521 | X2 CrMoTi 18−2 | 444 |
| 02 X28 H30 MDB | 1.4563 | X1 NiCrMoCu 31−27−4 | - |
| 03 X17 H13 AM3 | 1.4429 | X2 CrNiMoN 17−13−3 | 316LN |
| 03 X22 H5 AM2 | 1.4462 | X2 CrNiMoN 22−5-3 | - |
| 03 X24 N13 G2 C | 1.4332 | X2 CrNi 24−12 | 309L |
| 08 X16 N13 M2 B | 1.4580 | X1 CrNiMoNb 17−12−2 | 316 Cd |
| 08 CR18 H12 B | 1.4550 | X6 CrNiNb 18−10 | 347 |
| 08 CRNINB 18−10 347 CD 08 X18 H12 B 1 4550 X6 CRNINB 18−10 347 | 1.4583 X10 CrNiMoNb | X10 CrNiMoNb 18−12 | 318 |
| 08X19AH9 | - | - | 304N |
| 08X19H13M3 | 1.4449 | X5 CrNiMo 17−13 | 317 |
| 08X20H11 | 1.4331 | X2 CrNi 21−10 | 308 |
| 08X20H20TU | 1.4847 | X8 CrNiAlTi 20−20 | 334 |
| 08X25H4M2 | 1.4460 | X3 CrnImOn 27−5-2 | 329 |
| 08X23H13 | - | - | 309S |
| 09X17H7U | 1.4568 | X7 CrNiAl 17−7 | 631 |
| 1X16H13M2 B | 1.4580 | X6 CrNiMoNb 17−12−2 | 316Cd |
| 10X13 EDELSTAHL | 1.4724 | X10 CrAlSi 13 | 405 |
| 12X15 | 1.4001 | X7 Cr 14 | 429 |
| 12X17 | 1.4016 | X6 Cr17 | 430 |
| 12X17M | 1.4113 | X6 CrMo 17−1 | 434 |
| 12X17MB | 1.4522 | X2 CrMoNb | 436 |
| 12X18H12 | 1.3955 | GX12 CrNi 18−11 | 305 |
| 12X17 G9 AH4 | 1.4373 | X12 CrMnNiN 18−9-5 | 202 |
| 15X9M | 1.7386 | X12 CrMo 9−1 | 504 |
| 15X12 | - | - | 403 |
| 15X13H2 | - | - | 414 |
| 15X17H7 | 1.4310 | X12 CrNi 17−7 | 301 |
| Legierungssorte nach GOST 1583−93 | Europäische Norm | USA | Japan | Frankreich | Italien | Vereinigtes Königreich |
|---|---|---|---|---|---|---|
| EN 1676 | ASTM, B179, B26, B85, AA, SAE | JIS, H5202, H2211, H2118 | NFA57−702 | UN14514 | BS14 | |
| AK8 (AL34) |
ENAB-42 100 (ENAB AlSi7Mg0,3) |
358.0 356.2 (A03562) |
AC4C.1 | A-S7G | - | - |
| AK7 | ENAB-42 000 (ENAB AlSi7Mg) |
357.0 356.1 (A03561) |
AC4C.1 | - | AlSi7Mg | - |
| AK7h (AL9) |
ENAB-42 000 (ENAB AlSi7Mg) |
356.0 356.1 (A03561) SG70A |
AC4C.1 | A-S7GU3 | AlSi7MgTi | LM2 |
| AK7pch (AL9−1) |
ENAB-42 100 (ENAB AlSi7Mg0,3) |
356.2 (A03562) |
AC4C.2 | A-S7G | AlSi7Mg | - |
| AK12 (AL2) |
ENAB-44 100 (ENAB AlSi12 (b)) |
A413.1 (A4131) |
AC3C.1 | A-S12G A-S13 |
G-Al-Si13 | LM6 |
Quelle: www. aluminium-union.ru
| GUS, GOST | USA AISI, ASTM, ASME |
Deutschland DIN |
Japan JIS |
China GB UK |
UK B.S. |
Italien UNI |
Frankreich AFNOR NF |
|---|---|---|---|---|---|---|---|
| 03CR17H14M3 | 316L SA-240TP316L |
X2CrNiMo18−14−3 | SUS 316L | 00Cr17Ni14Mo2 00Cr17Ni14Mo3 |
316S13 LW 22 |
X2CrNiMo 18−14−3 X2CrNiMo1713KG |
Z 3 CND 17−12−03 |
| 03X18H11 | 304 L SA-240TP304L |
X2 Cr Ni 19−11 GX2 Cr Ni 19−11 |
SUS304 L | - | 304S11 LW 20 LWCF 20 S 536 304 C12 (LT 196) 305 S 11 |
X2 CrNi 18 11 X 3 CrNi 18 11 GX 2 CrNi 19 10 |
Z 1 CN 18−12 Z 2 CN 18−10 Z 3 CN 19−10M Z 3 CN 18−10 Z 3 CN 19−11 Z 3 CN 19−11FF |
| 03CRNI28MDT 06CR28MDT |
- | X3NiCrCuMoTi2730 | - | - | - | - | - |
| 06X18H11 | 305 3008 |
X4CrNi18−12 | SUS 305 SUS 305J1 |
- | 305S17 305S19 |
X7 CrNi18 10 X8 CrNi 19 10 |
Z 5 CN 18−11FF |
| 07C16H6 | 301 A 167 301 A 240 301 A 666 301 |
X12CrNi17−7 X10CrNi18−8 |
SUS 301 | - | 301 S 21 301 S 22 Cr Ni 17/7 |
X10CrNi18−8 X12CrNi17−07 |
Z 11 CN 17−08 Z 11 CN 18−08 Z 12 CN 18−09 |
| 08kp | A 622 | St 50−2 | SPHE | - | BS 1449 1 HR |
- | 3C |
| 08X13 | 403 409 410 S 429 SA-240 TP 410S |
X6 Cr 13 X7 Cr 14 |
SUS 403 SUS 410S SUS429 |
- | 403 S17 | X6 Cr 13 | Z6 C13 Z8 C12 Z8 C13FF |
| 08X17H13M2T 10X17H13M2T |
316 Ti A 167 316Ti A 213 F316H A 240 316Ti A 368 316Ti SA-240 TP 316Ti SA-479 316Ti |
X6CrNiMoTi 12 122 X 10 CrNiMoTi 18−12 |
SUS 316Ti | 0Cr18Ni12Mo3Ti 1Cr18Ni12Mo3Ti |
320 S 33 CrNiMo 17/12/2 ¼ Ti |
X 6 CrNiMoTi 17 13 | Z6 CNDT 17.12 |
| 08CRNI17TI | 430Ti 439 |
X 6 CrTi 17 X3CrTi 17 |
SUS 430LX | - | - | X 3 CrTi 17 X 6 CrTi 17 |
Z 4 CT 17 |
| 08X18H10 | 304 304 H SA-240 TP 304 |
X5 Cr Ni 18 10 | SUS 304 | - | 304S11 304S15 304S16 304S17 304S31 LW21 LWCF 21 |
X 5 Cr Ni 18 10 | Z4 CN 19−10 FF Z5 CN 17−06 Z6CN 18.09 Z7 CN 18−09 |
| 08CR18NI12B | 347 A 167 347 A 240 347 A 313 347 A 580 347 |
X 6 CrNiNb 18 10 X6CrNiNb 18−10 |
SUS 347 | 0Cr18Ni11Nb 1Cr18Ni11Nb 1Cr19Ni11Nb |
347 S 20 347 S 31 ANC 3 Güteklasse B CrNi 18/9/Nb CrNi 18/9 0,10C/Nb |
X 6 CrNiNb 18 11 | Z 6 CNNb 18−10 |
| 08 SA | A 620 | DC 04 DC04 + ZE Fe P04 / St 14 St 14 St 4 |
SPCE | - | DC 04 / FeP 04 HR 1 HR 2 |
DC 04 / FeP 04 | DC 04 / FeP 04 |
| 09G2S | A 516−55 A 516−60 A 516−65 A 561 Gr70 |
- | SM41B SB49 |
- | - | - | - |
| 09CR17NI7U | - | X 7 CrNiAl 17 7 X7CrNiAl17−7 |
SUS 631 | 0Cr17Ni7Al | 301 S 81 | - | Z 9 CNA 17−07 |
| 10 | C1010 A 108 1010 A 29 M1010 A 510 1010 A 575 M1010 SA-29 M1010 |
C 10 C10E Ck 10 |
S 10 C S 9 CK SACM 1 |
10 | 040 A 10 045 M 10 En2A En32A HS 10 |
1 C 10 2 C 10 2 C 15 C 10 |
C 10 RR XC 10 |
| 10C13CU | A 268 TP405 | X10CrAl13 X10CrAlSi13 |
- | - | - | X 10 CrAl 12 | Z 13 C 13 |
| 10X23H18 20X23H18 |
SA-240 TP 310S | - | - | - | - | - | - |
| 12К | A 201 Gr AFx | ASt 35 | - | - | - | - | - |
| 12X13 15X13L |
410 430 A 183 F6 A 193 B6 A 479 410 |
X 10 Cr 13 X12 Cr13 GX 12 Cr 12 |
SUS 410 | - | 410C21 410S21 ANC 1A |
X 10 Cr13 X 12 Cr13 |
Z10C13 Z12C13 |
| 12Х17 | 430 A 182 F 430 A 240 430 SA-182 Güteklasse F 430 SA-240 Typ 430 |
X6Cr17 | SUS 430 | 1Cr15 1Cr17 ML1Cr17 |
17Cr 430S17 430S18 |
X 6 Cr 17 X 8 Cr 17 |
Z 8 C 17 |
| 12X18H10T 06X18H10T 08X18H10T 09CR18NI10T |
321 A 213 TP321H SA-240 TP 321 |
X6 Cr Ni Ti 18 10 X10 Cr Ni Ti 189 |
SUS 321 | - | 321S12 | - | Z6 CNT 18.10 |
| 12XM | A 182 Güteklasse F12 A213 Güteklasse T12 A 335 Güteklasse P12 A 387A, B, C |
13CrMo-44 | - | - | - | - | - |
| 12X2M | A 182 Güteklasse F22 A335 Güteklasse P22 387 Güteklasse D |
10CrMo910 | - | - | - | - | - |
| 12CR1MOV | - | 14MoV63 | - | - | - | - | - |
| 14Г2 | A414 Gr F, G A 515 Gr70 A516 Gr70 |
17 Mn4 | SB 46 SB 49 SG V 46 SG V 49 SP V 32 |
- | - | - | A 48CP |
| 15 | C1015 A 108 1015 A 512 1015 A 576 1015 |
C15 C15E Ck 15 |
S 15 C S 15 CK |
15 H15A ZG200−400 (ZG 15) |
- | - | C 18 RR XC 15 XC 18 |
| 15kp | A 621 FS Typ A A 621 FS Typ B |
DD 11 (StW 22) | SPHD | - | - | - | 1 C |
| 15Stück | A 29 1015 | QSt 38−3 | SWRCH15A SWRCH16R |
ML15 | - | CB 15 | - |
| 15H2M 15HM |
4615 | - | - | - | - | - | - |
| 15Х | - | 15Cr3 | - | - | - | - | - |
| 15X5M | A 182 Güteklasse F5 A 193 Güteklasse B5 |
- | - | - | - | - | - |
| 15X25T 15X28 |
A 268 TP446 | 10CrAl24 | - | - | - | - | - |
| 15XF | 6117 | - | - | - | - | - | - |
| 15CM | A 182 Güteklasse F12 A213 Güteklasse T12 A 335 Güteklasse P12 |
13CrMo-44 | - | - | - | - | - |
| 16К | A 414 Besoldungsgruppe E | H II St42−2 C22N ASt41 P 265 GH |
SG 295 SG 30 SM 53 B SM 53 C SPV 315 SPV 32 SPV 355 SPV 36 |
- | P 265 GH | Fe 410 KW P 265 GH |
- |
| 17GS | - | S355J2G3 / Fe 510 D1 St 52−3 St 52−3 / S355J2G3 St 52−3 G |
SM 490 A SM 520 C SM 53 C |
16Mn | - | Fe 510 Fe E 420 S 355 J 2 G 3 |
S 355 J 2 G 3 |
| 18CR | SA-29 Sorte 5115 | 16 MnCr 5 | - | 15CrMn 20CrMn |
527 M 17 590 H 17 590 M 17 |
16 MnCr 5 | 16 MC 5 16 MnCr 5 RR |
| 20 | C1020 A 105 Gr1 A 106 GrA, B A 659 CS Typ 1020 A 794 CS Typ 1020 |
C 22 C 22N C 22.3 Ck 22 St35.8 St45.8 |
S 20 C S 20CK |
- | 040A20 070 M 20 070 M 26 1 C 22 C 22 En3A En3B En3C En3D |
C 20 C 21 C 22 |
C 20 XC 25 |
| 20К | A 283-C A 285-A, B, c A 414 Klasse E A 515−5 A 515−60 A 515−70 |
H II P 265 GH |
SG 295 SG 30 SM 53 B SM 53 C SPV 315 SPV 32 SPV 355 SPV 36 |
- | P 265 GH | Fe 410 KW P 265 GH |
- |
| 20ps | A 29 1020 | - | SWRCH17R | ML20 | 0/4 | - | - |
| 20H2M 20HM |
4621 | - | - | - | - | - | - |
| 20X | 5120 | - | - | - | - | - | - |
| 20KHF | 6120 | 22CrV4 | - | - | - | - | - |
| 20Х13 | 420 A 276 420 A 580 420 |
X 20 Cr 13 | SUS 420J1 | 2Cr13 | 420 S 37 En56C |
X 20 Cr 13 | Z 20 C 13 |
| 20CR17NI2 | 431 A 493 431 A 580 431 SA-479 Typ 431 |
X17CrNi16−2 X17CrNi16−2 (X 20 CrNi 17 2) |
SUS 431 | 1Cr17Ni2 ML1Cr17Ni2 |
431 S 29 En57 |
X 16 CrNi 1 | Z 15 CN 16−02 Z 15 CN 16.02 CI |
| 20CR25NI20C2 | 310 314 |
X15CrNiSi25−20 X15CrNiSi25−21 |
SUS Y 310 | 2Cr25Ni20 | - | X 16 CrNiSi 25 20 | Z 15 CNS 25−20 |
| 20CRM | 4130 SA-29 Güte 4130 |
25 CrMo 4 GS-25 CrMo 4 |
SKM 420 SCM 430 |
ML30CrMo ML30CrMoA |
25 CrMo 4 | 25 CrMo 4 | 25 CrMo 4 |
| 20XH | 3120 | - | - | - | - | - | - |
| 22K | 1022 1518 |
20Mn5 | S Mn C 420 | - | 120M19 | - | 20M5 |
| 25 | C1025 | - | - | - | - | - | - |
| 25Г | 1025 A 108 1025 A 510 1025 A 512 1025 A 513 1025 A 576 1025 |
GS-Ck 25 | S 25 C | 25 25Z ZG230−450 (ZG 25) |
070 M 26 080 A 25 |
- | - |
| 25X1MF | A 193 B14 A 540 B21 |
24CrMoV55 | - | - | - | - | - |
| 30 | C1030 A 29 1030 SA-29 1030 |
- | SWRCH30K SWRCH33K |
ML25Mn ML30 |
1/1 | - | - |
| 30X | 5130 | - | - | - | - | - | - |
| 30XM | 4130 A 302 Gr B A 304 |
25CrMo4 | - | - | - | - | - |
| 30KH13 | 420F | X30Cr13 | SUS 420J2 | 3Cr13 | 420 S 45 En56D |
G X 30 Cr 13 X 30 Cr 13 |
Z 30 C 13 Z 33 C 13 |
| 30CRM | - | 34 CrMo 4 GS-34 CrMo 4 |
SCM 435 SCM 435 H |
35CrMo | 34 CrMo 4 | 34 CrMo 4 | 34 CrMo 4 |
| 30G2 | - | 36 Mn 5 | SCMn 3 SMn 438 SMn 438 H |
- | 150 M 36 En15 En15A |
- | 40 M 5 |
| 35 | C1035 C1034 A 107 |
C 35 Ck 35 |
S 35C | - | 080M36 | - | XC 38 |
| 35X | 5132 | 34Cr4 | - | - | - | - | - |
| 35XM | - | 34CrMo4 | - | - | - | - | - |
| 40 | 1040 | C40 Ck40 |
S 40C | - | 080A40 060A40 |
- | XC 42 |
| 40X | 5140 | 41 Cr 4 | S Gr 440 | - | 530A40 530M40 |
- | 42C4 |
| 40KH13 | - | X38Cr13 X39Cr13 X46Cr13 |
SUS 420J2 | - | 420S45 | X 40 Cr 14 X 46 Cr 13 |
Z 38 C 13 M Z 40 C 13 Z 40 C 14 Z 44 C 14 Z 50 C 14 |
| 40CR2H2MA | 4340 SA-29 Güte 4340 |
40 NiCrMo 6 | SNCM 439 STPT 38 |
40CrNiMoA ML40CrNiMoA |
818 M 40 | - | - |
| 40XH | 3135 3140 |
40Ni Cr 6 | - | - | 640M40 | - | - |
| 40CRNI2MA | 9840 | 36 CrNiMo 4 | - | - | 36 CrNiMo 4 | 36 CrNiMo 4 | 36 CrNiMo 4 40 NCD 3 |
| 45 | 1045 A 107 A 29 1044 SA-29 1044 |
C 45 Ck 45 Cq 45 |
S 45C SWRCH45K |
ML45 | 080M 080M46 |
- | XC48 |
| 45Г | 1045 A 108 1045 A 29 1045 A 311 1045 A 576 1045 SA-29 1045 SA-311 1045 |
C45E Ck 45 GS-Ck 45 |
S 45 C S 48 C |
45 ZG310−570 (ZG 45) |
C 45 E | C 45 E | C 45 E XC 45 |
| 45X | 5145 | - | - | - | - | - | - |
| 50 | С1050 A 108 1050 A 29 1050 A 311 1050 A 510 1050 A 576 1050 SA-29 1050 SA-311 1050 |
C 50 E Ck 50 |
- | 50 | 080 M 50 C 50 E |
C 50 E | C 50 E XC 50 |
| 50X | 5147 | - | - | - | - | - | - |
| 55 | С1055 A 29 1055 A 576 1055 SA-29 1055 |
C 55 Ck 53 |
S 55 C S 55 C-CSP |
- | 070 M 55 C 55 En9 En9K |
C 55 | AF 70 C 54 C 55 |
| 60 60Г |
C1060 A 29 1060 A 576 1060 SA-29 1060 |
C 60 | S 58 C S 60 C-CSP S 65 C-CSP |
- | 060 A 62 C 60 CS 60 HS 60 |
C 60 | C 60 |
| St0 St1kn |
A 283 Güteklasse A | S185 / Fe 310−0 St 33 |
SS 330 | Q195 Q195-F Q195-Z Q195-b |
HR 15 | S 185 | - |
| St2ps St2sp |
A53 Gr A A192 Gr A |
St 35 | - | Q215B Q215B-F Q215B-Z Q215B-b |
S360 | - | - |
| St3kn | A 107 A 283 Güteklasse C SA-283 C |
USt 37−2 USt 37−2 G RSt37−2 |
- | A3 Q235A Q235A-F Q235A-Z Q235A-b |
- | - | - |
| St3sp | A 414 Güteklasse A A 570 Sorte 36 |
S235J2G3 / Fe 360 D1 St 37−3 St 37−3 G UZSt 37−2 |
SS34 | - | HS 37/23 S 235 J 2 G 3 40C BS4360 |
S 235 J 2 G 3 | S 235 J 2 G 3 E 24−2NE |
| St5sp | A 570 Güteklasse 50 | St 50−2 | SS 50 | - | - | - | А 50−2 |
| St6ps St6sp |
A 572 Güteklasse 65 | E335 / Fe 590−2 St 60−2 St 60−2 G |
SM 570 SM 58 |
- | 55 C E 335 |
E 335 Fe 590 |
E 335 |
Quelle: gosts.org
| Stahlsorte GUS-Länder GOST | Euronorm-Stahlsorte | Stahlsorte Euronormen | US-Entsprechung |
|---|---|---|---|
| 10 | C10E | 1.1121 | 1010 |
| 10XHH1 | 10 XHN1 | 1.5805 | - |
| 14 CRH3 M | 14 NiCrMo1−3-4 | 1.6657 | 9310 |
| 15 | C15 E | 1.1141 | 1015 |
| 15 Г | C16 E | 1.1148 | 1016 |
| 16 CH | 16 MnCr5 | 1.7131 | 5115 |
| 16XGR | 16Mn CrB5 | 1.7160 | - |
| 16 CHN | 16NiCr4 | 1.5714 | - |
| 17 G1 C | S235J2G4 | 1.0117 | - |
| 17 CH3 | 15NiCr13 | 1.5752 | Е3310 |
| 18 CGM | 18CrMo4 | 1.7243 | 4120 |
| 18 X2 H2 M | 18CrNiMo7−6 | 1.6587 | - |
| 20 | C22E | 1.1151 | 1020 |
| 20 XM | 20MoCr3 | 1.7320 | 4118 |
| 20CRNIM | 20MoCr2−2 | 1.6523 | 8617 |
| 25 | C25E | 1.1158 | 1025 |
| 25 XM | 25CrMo4 | 1.7218 | 4130 |
| 28 Г | 28Mn6 | 1.1170 | 1330 |
| 30 | C30E | 1.1178 | 1030 |
| 34 Х | 34Cr4 | 1.7033 | 5130 |
| 34 X2 H2 M | 34CrNiMo6 | 1.6582 | 4340 |
| 35 | C35E | 1.1181 | 1035 |
| 36 CNM | 36CrNiMo4 | 1.6511 | 9840 |
| 36 X2 H4 MA | 36NiCrMo16 | 1.6773 | - |
| 40 | C40E | 1.1186 | 1040 |
| 42 XM | 42CrMo4 | 1.7225 | 4140 |
| 45 | C45E | 1.1191 | 1045 |
| 46 Х | 46Cr2 | 1.7006 | 5045 |
| 50 | C50E | 1.1206 | 1050 |
| 50 CGF | 50CrV4 | 1.8159 | 6150 |
Quelle: metaltrade.ru
| Stahlsorte GUS-Länder GOST | Stahlsorte Euronormen | Stahlsorte Euronormen | Analogien in US-Normen |
|---|---|---|---|
| 10 X2 M | 10CrMo9−10 | 1.7380 | F22 |
| 13 XM | 13CrMo4−4 | 1.7335 | F12 |
| 14 XMF | 14MoV6−3 | 1.7715 | - |
| 15 М | 15Mo3 | 1.5415 | F1 |
| 17 Г | 17Mn4 | 1.0481 | - |
| 20 | C22.8 | 1.0460 | - |
| 20 Г | 20Mn5 | 1.1133 | - |
| 20 X11 MNF | X20CrMoV12−1 | 1.4922 | - |
Quelle: metaltrade.ru
| GUS-Länder (GOST 1050−88) | Deutschland (DIN) Ausländische Entsprechungen | Deutschland (DIN) Ausländische Entsprechungen | USA (ASTM) |
|---|---|---|---|
| 10 | 1.0301 | C 10/Sc 10 | 1010 |
| 15 | 1.0401 | C15/Sc 15 | 1015 |
| 20 | 1.0402 | C 22/Sq 22 | 1020 |
| 30 | - | - | 1030 |
| 35 | 1.0501 | C 35/Ck 35 | 1035 |
| 40 | 1.0511 | C 40/Sk 40 | 1040 |
| 45 | 1.0503 | C 45/Sk 45 | 1045 |
| 50 | 1.0540 | C 50/Quadrat 50 | 1050 |
| 55 | 1.0535 | C 55/Quadrat 55 | 1055 |
| 60 | 1.0601 | C 60/Quadrat 60 | 1060 |
Quelle: metallopt.ru
| GUS-Länder (GOST, TU) | Deutschland (DIN) Ausländische Analoga | Deutschland (DIN) Ausländische Analoge | USA (ASTM) |
|---|---|---|---|
| 12XH3A | 1.5732 | 14NiCr10 | - |
| 12CR4A | Е3310 | ||
| 15CRM | 1.7335 | 13CrMo44 | - |
| 17G1S | 1.0570 | St52−3 | - |
| 18CR | 1.7131 | 16MnCr5 | 5120 |
| 20CR | 1.7218 | 25CrMo4 | 4130 |
| 27CRMO4 | 1.5526 | 30MnB4 | - |
| 30CR3MOV | 1.8519 | 31CrMoV9V | - |
| 30CR2H2M | 1.6580 | 30CrNiMo8V | - |
| 34CR2NIMO8V | 1.8550 | 34CrAlNi7V | - |
| 38CR2H2MA | 1.6582 | 34CrNiMo6 | 4330 |
| 40Х | 1.7045 | 42Cr4 | 5140 |
| 40CRM | 1.7225 | 42CrMo4 | 4140 |
| 40CRNI2MA | 1.6565 | 40NiCrMo6 | 4340 |
| 40CRNINM | 1.6546 | 40NiCrMo22 | 8640 |
| 45Г | 1.0912 | 46Mn7 | - |
Quelle: metallopt.ru
| Stahlsorte GUS-Länder GOST | Stahlsorte Euronormen | Stahlsorte Euronormen | Entsprechungen in US-Normen |
|---|---|---|---|
| SHC4 | 100Cr2 | 1.3501 | 50 100 |
| 30 30CR15 | 100Cr6 | 1.3505 | 52 100 |
| SHCR15 SG | 100CrMn6 | 1.3520 | A 485 (2) |
| 485 (2) Ø ØCR20 M | 100CrMo7 | 1.3537 | A 485 (3) |
Quelle: metaltrade.ru
| Stahlsorte GUS-Länder GOST | Euronorm-Stahlsorte | Euronorm-Stahlsorte | Entsprechungen in US-Normen |
|---|---|---|---|
| 38C2A | 38Si7 | 1.5023 | - |
| 50CRVA | 50CrV4 | 1.8159 | 6150 |
| 52 CGMFA | 51CrMoV4 | 1.7701 | - |
| 55 CR2A | 54SICr6 | 1.7102 | - |
| 55 CGA | 55Cr3 | 1.7176 | 5147 |
| 60 C2 CGA | 60SiCR7 | 1.7108 | 9262 |
Quelle: metaltrade.ru
| GUS-Länder (GOST, TU) | Deutschland (DIN) Ausländische Analoga | Deutschland (DIN) Ausländische Entsprechungen | USA (ASTM) |
|---|---|---|---|
| 70 | 1.1231 | Ck 67 | 1070 |
| 75 | 1.0605 | C 75 | 1074 |
| 85 | 1.1269 | Ck 85 | 1086 |
| 50CFA | 1.8159 | 50CrV4 | 6150 |
| 55С2 | 1.5026 | 55Si7 | - |
| 60Г | 1.0601 | С 60 | 1060 |
| 60C2 | 1.5027 | 60Si7 | 9260 |
| 60C2GH | 1.5092 | 60SiCr7 | 9262 |
| 70C2X | 1.5029 | 71Si 7 | - |
Quelle: metallopt.ru
| GUS-Länder (GOST, TU) | Deutschland (DIN) Ausländische Analoga | Deutschland (DIN) Ausländische Entsprechungen | USA (ASTM) |
|---|---|---|---|
| У 7 | 1.1620 | C 70W2 | - |
| U 7A | 1.1520 | C 70W1 | - |
| У 8 | 1.1625 | C 80W2 | - |
| U 8A | 1.1525 | C 80W1 | W 108 |
| У 10 | 1.1645 | C 105W2 | - |
| W 10A | 1.1545 | C 105W1 | W 110 |
| У 11 | 1.1654 | C 110W | - |
| У 13 | 1.1663 | C 125W | W 112 |
Quelle: metallopt.ru
| GUS-Länder (GOST, TU) | Deutschland (DIN/BOHLER) Ausländische Entsprechungen | Deutschland (DIN/BOHLER) Ausländische Entsprechungen | USA (AISI/ASTM) |
|---|---|---|---|
| Х12 | 1.2080 | X210Cr12 | D3 |
| X12B | 1.2436 | X210CrW12 | - |
| X12MF* | 1.2379 | X155CrVMo12−1 | D2 |
| X12MF4-MP | - | K190RM | - |
| 95CRF | 1.2210 | 115CrV 3 | L2 |
| 9X1F | 1.2067 | 102Cr 6 | L3 |
| 9G2F | 1.2842 | 90MnCrV 8 | O2 |
| 95CRVF | 1.2510 | 100MnCrW 4 | O1 |
| 3CR3B9F | 1.2581 | X30WCrV9−3 | H21 |
| 95CR5GM | 1.2363 | X100CrMoV5−1 | А2 |
| 95CRM | 1.2303 | 100CrMo 5 | L7 |
| 95Х18 | 1.4125 | X105CrMo17 | A473 (440C) |
| 5CRNIMO | 1.2713 | 55NiCrMoV 6 | L6 |
| 5CR2SF | 1.2550 | 60WCrV 7 | S1 |
| 5CR3MO2F | - | - | S7 |
| 5CRNI2MOV | 1.2714 | 56NiCrMoV 7 | - |
| 3CR3M3F | 1.2365 | X32CrMoV3 3 | H10 |
| 4X5MFS | 1.2343 | X38CrMoV5−1 | H11 |
| 4X5MF1C | 1.2344 | X40CrMoV5−1 | H13 |
*mögliche Herstellung durch Pulvermetallurgieverfahren
Quelle: metallopt.ru
| Stahlsorte GUS-Länder GOST | Stahlsorte Euronormen | Stahlsorte Euronormen | Analogien in US-Normen |
|---|---|---|---|
| P0 M2 SF10-MP | - | - | А11 |
| R2 M9-MP | S2−9-2 | 1.3348 | М7 |
| R2 M10 K8-MP | S2−10−1-8 | 1.3247 | М42 |
| R6 M5-MP | S6−5-2 | 1.3343 | М2 |
| R6 M5 K5-MP | S6−5-2−5 | 1.3243 | - |
| R6 M5 F3-MP | S6−5-3 | 1.3344 | М3 |
| P6 M5 F4-MP | - | - | М4 |
| R6 M5 F3 K8-MP | - | - | М36 |
| R10 M4 F3 K10-PP | S10−4-3−10 | 1.3207 | - |
| R6 M5 F3 K9-MP | - | - | М48 |
| R12 M6 F5-MP | - | - | М61 |
| R12 F4 K5-MP | S12−1-4−5 | 1.3202 | - |
| R12 F5 K5-MP | - | - | Т15 |
| R18-MP | - | - | Т1 |
Quelle: metaltrade.ru
| GUS-Länder (GOST, TU) | Deutschland (DIN) | BOHLER (D-016) | USA (AISI/ASTM) |
|---|---|---|---|
| R18* | 1.3355 | S 200 | Т 1 |
| R6M5* | 1.3343 | S600/S601 | М 2 |
| R6M5K5* | 1.3243 | S 705 | - |
| R6M5F3-MP | 1.3342/1.3344 | S 790PM | М 3 |
| R6M5F4-MP | - | S 690PM | М 4 |
| R6M5F3K8-MP | - | S 590PM | М 36 |
| R10M2F5K8-MP | - | S 390PM | - |
| R10M3F4K8-MP | - | - | - |
| R12F3 | 1.3318 | - | - |
| R12MF4-MP | - | S 207PM | - |
| R12K5F4-MP | - | S 308PM | - |
| R12M6F5-MP | - | - | М 61 |
| R12MF5K5-MP | 1.3202 | - | Т 15 |
| R0M2SF10-MP | - | CPM 10V | А 11 |
* Herstellung nach dem pulvermetallurgischen Verfahren ist möglich
Quelle: metallopt.ru
| GUS-Länder (GOST) | Analog | Land Standard |
|---|---|---|
| 20GL | A352 Gr LCC | USA, ASTM A352 |
| 20GL | A757 Gr A2Q | USA, ASTM A757 |
| 20GL | A216 Gr WCC | USA, ASTM A216 |
| 30GSL | A304 (1330H) | USA, ASTM A304 |
| 30GSL | A322 (1330) | 1330H USA, ASTM A322 |
| 20Л | A732 (1A) | 1A USA, ASTM A732 |
| 25Л | A352 Gr LCA | 20L (1A) ASTM A732 (1A) USA, ASTM A352 |
| 25Л | A732 (2A) | 2A USA, ASTM A732 |
| 25Л | A216 Gr WCB | USA, ASTM A216 |
| 30Л | A352 Gr LCB | USA, ASTM A352 |
| 30Л | A216 Gr WCB | USA, ASTM A216 |
| 35Л | A356 Gr1 | USA, ASTM A356 |
| 40Л | A732 (3A) | USA, ASTM A732 |
Quelle: www. td-ksz.com
| GUS-Länder (GOST) | Analog | Land Norm |
|---|---|---|
| 20GL | 1.1120 | Deutschland, DIN 17 182 |
| 30GSL | 1.1165 | Deutschland, DIN 17 205 |
| 15Л | 1.0420 | Deutschland, DIN 1681 |
| 20Л | 1.0619 | Deutschland, DIN EN 10 213−2 |
| 25Л | 1.0446 | Deutschland, DIN 1681 |
| 35Л | 1.0552 | Deutschland, DIN 1681 |
| 45Л | 1.0558 | Deutschland, DIN 1681 |
Quelle: www. td-ksz.com
| GUS-Länder (GOST) | Kurzbezeichnung | Land Norm |
|---|---|---|
| 30GSL | AO35 MnSi5 | Ungarn, MSZ 8272 |
| 30GSL | 30 GSL | Bulgarien, BDS 6550 |
| 30GSL | T30 Si Mn12 | Rumänien, STAS 1773 |
| 15Л | 15LII | Bulgarien, BDS3492 |
| 15Л | AM1 | BRITANNIEN, B.S.3100 (91) |
| 15Л | Ao 400 FK | Ungarn, MSZ 8276 |
| 15Л | L II 400 | Polen, PN/H 83 152 |
| 15Л | OT 400−3 | Rumänien, STAS 600 |
| 15Л | 422 630 | Tschechische Republik, Slowakei, CSN 422 630 |
| 25Л | 161 Grad 430 | Großbritannien, B.S. 1504 (76) |
| 25Л | 25 LII | Bulgarien, BDS 3492 |
| 25Л | Ao 450 FK | Ungarn, MSZ 8276 |
| 25Л | OT 450−3 | Rumänien, STAS 600 |
| 25Л | 25LI | Bulgarien, BDS 3492 |
| 25Л | 422 640 | Tschechische Republik, Slowakei, CSN 422 640 |
| 25Л | L 450 | Polen, PN/H 83 152 |
| 30Л | 1505 | Schweden, SS |
| 35Л | 35LII | Bulgarien, BDS 3492 |
| 35Л | A2 | BRITANNIEN, B.S.3100 (91) |
| 35Л | Ao 500 FK | Ungarn, MSZ 8276 |
| 35Л | L500 | Polen, PN/H8 3152 |
| 35Л | OT 500−1 | Rumänien, STAS 600 |
| 35Л | 35LI | Bulgarien, BDS3492 |
| 35Л | 422 650 | Tschechische Republik, Slowakei, CSH 422 650 |
| 35Л | G-30−57 | Finnland, SFS 350 |
| 35Л | SCC | Japan, JIS G5111 (91) |
| 40Л | 35LI | Bulgarien, BDS 3492 |
| 40Л | OT 550−1 | Rumänien, STAS 600 |
| 40Л | CLA1 Klasse C | UK, B.S. 3146 Teil 1 (74) |
| 40Л | CLA8 Grad C | UK, B.S. 3146 Teil 1 (74) |
| 40Л | G-30−57 | Finnland, SFS 350 |
| 45Л | 45LI | Bulgarien, BDS 3492 |
| 45Л | A3 | BRITANNIEN, B.S.3100 (91) |
| 45Л | Ao550FK | Ungarn, MSZ 8276 |
Quelle: www. td-ksz.com
| Europa (EN) | Deutschland (DIN) | USA (AISI) | Japan (JIS) | GUS (GOST) |
|---|---|---|---|---|
| 1.4713 | X10CrAl7 | 10CR17CU | ||
| 1.4724 | X10CrAl13 | 405 | 10CR13CU | |
| 1.4742 | X10CrAl18 | 442 | ||
| 1.4762 | X10CrAl24 | 446 | ||
| 1.4878 | X12CrNiTi18−9 | 321 H | 12X18H10T | |
| 1.4828 | X15CrNiSi20−12 | 309 | 20X20H14C2 | |
| 1.4845 | X12CrNi25−21 | 310 S | 20CR23NI18 | |
| 1.4841 | X15CrNiSi25−20 | 314 | 20CR25H20C2 |
Quelle: www.uvis.ua
| Europa (EN) | Deutschland (DIN) | USA (AISI) | Japan (JIS) | GUS (GOST) |
|---|---|---|---|---|
| 1.4003 | X2CrNi12 | |||
| 1.4512 | X2CrTi12 | 409 | SUH 409 | |
| 1.4000 | X6Cr13 | 410S | SUS 410 S | 08KH13 |
| 1.4002 | X6CrAl13 | 405 | SUS 405 | |
| 1.4006 | X12CrN13 | 410 | SUS 410 | 12KH13 |
| 1.4024 | X15Cr13 | (410) | SUS 410 J1 | |
| 1.4021 | X20Cr13 | (420) | SUS 420 J1 | 20Х13 |
| 1.4028 | X30Cr13 | (420) | SUS 420 J2 | 30KH13 |
| 1.4031 | X39Cr13 | SUS 420 J2 | 40KH13 | |
| 1.4034 | X46Cr13 | (420) | 40KH13 | |
| 1.4016 | X6Cr17 | 430 | SUS 430 | 12Х17 |
| 1.4520 | X2CrTi17 | |||
| 1.4510 | X3CrTi17 | 439 | SUS 430 LX | 08CR17TI |
| 1.4113 | X6CrMo17−1 | 434 | SUS 434 | |
| 1.4509 | X2CrTiNb18 | 441 | ||
| 1.4521 | X2CrMoTi18−2 | 444 | SUS 444 | |
| 1.4589 | X5CrNiMoTi15−2 | |||
| 1.4310 | X10CrNi18−8 | (301) | SUS 301 | |
| 1.4318 | X2CrNiN18−7 | 301 LN | SUS 301 LN | |
| 1.4301 | X5CrNI18−10 | 304 | SUS 304 | 08CR18NI10 |
| 1.4303 | X4CrNi18−12 | (305) | SUS 305 | 12X18H12 |
| 1.4306 | X2CrNi19−11 | 304 L | SUS 304 L | 03CR18NI11 |
| 1.4541 | X6CrNiTi18−10 | 321 | SUS 321 | 08CR18NITI10T |
| 1.4550 | X6CrNiNb18−10 | 347 | SUS 347 | |
| 1.4401 | X5CrNiMo17−12−2 | 316 | SUS 316 | |
| 1.4404 | X2CrNiMo17−12−2 | 316 L | SUS 316 L | |
| 1.4571 | X6CrNiMoTi17−12−2 | 316 Ti | SUS 316 Ti | 10X17H13M2T |
| 1.4561 | X1CrNiMoTi18−13−2 | |||
| 1.4435 | X2CrNiMo18−14−3 | 316 L | SUS 316 L | 03CR17H14M2 |
| 1.4439 | X2CrNiMoN17−13−5 | S 31 726 | SUS 317 | |
| 1.4539 | X1NiCrMoCu25−20−5 | N 8 904 | ||
| 1.4565 | X3CrNiMnMoNbN 23−17−5-3 | S 34 565 | ||
| 1.4462 | X2CrNiMoN22−5-3 | S 31 803 | SUS 329 J3L | |
| Europa (EN) | Deutschland (DIN) | USA (AISI) | Japan (JIS) | GUS (GOST) |
Quelle: www.uvis.ua
| GUS (GOST) | Euronormen (EN) | Deutschland (DIN) | USA (AISI) |
|---|---|---|---|
| 03 X17 H13 M2 | 1.4404 | X2 CrNiMo 17−12−2 | 316 L |
| 03 X17 H14 M3 | 1.4435 | X2 CrNiMo 18−4-3 | - |
| 03 X18 H11 | 1.4306 | X2 CrNi 19−11 | 304 L |
| 03 X18 H10 T-U | 1.4541-MOD | - | - |
| 06 CHN28-MDT | 1.4503 | X3 NiCrCuMoTi 27−23 | - |
| 06 X18 H11 | 1.4303 | X4 CrNi 18−11 | 305 L |
| 08 X12 T1 | 1.4512 | X6 CrTi 12 | 409 |
| 08 Х13 | 1.4000 | X6 Cr 13 | 410S |
| 08 CR17 H13 M2 | 1.4436 | X5CrNiMo 17−13−3 | 316 |
| 08 X17 H13 M2 T | 1.4571 | X6 CrNiMoTi 17−12−2 | 316Ti |
| 08 CR17 T | 1.4510 | X6 CrTi 17 | 430Ti |
| 08 X18 H10 | 1.4301 | X5 CrNi 18−10 | 304 |
| 08 CR18 H12 T | 1.4541 | X6 CrNiTi 18−10 | 321 |
| 10 X23 H18 | 1.4842 | X12 CrNi 25−20 | 310S |
| 10X13 | 1.4006 | X10 Cr13 | 410 |
| 12 X18 H10 T | 1.4878 | X12 CrNiTi 18−9 | - |
| 12 X18 H9 | - | - | 302 |
| 15 X5 M | 1.7362 | X12 CrCo 5 | 501 |
| 15 X25 T | 1.4746 | X8 CrTi 25 | - |
| 20X13 | 1.4021 | X20 Cr 13 | 420 |
| 20 X17 H2 | 1.4057 | X20 CrNi 17−2 | 431 |
| 20 X23 H13 | 1.4833 | X7 CrNi 23−14 | 309 |
| 20 X23 H18 | 1.4843 | X16 CrNi 25−20 | 310 |
| 20 X25 H20 C2 | 1.4841 | X56 CrNiSi 25−20 | 314 |
| 03 X18 AH11 | 1.4311 | X2 CrNiN 18−10 | 304LN |
| 03 X19 H13 M3 | 1.4438 | X2 18−5-4 | 317L |
| 03 X23 H6 | 1.4362 | X2 CrNiN 23−4 | - |
| 02 X18 M2 BT | 1.4521 | X2 CrMoTi 18−2 | 444 |
| 02 X28 H30 MDB | 1.4563 | X1 NiCrMoCu 31−27−4 | - |
| 03 X17 H13 AM3 | 1.4429 | X2 CrNiMoN 17−13−3 | 316LN |
| 03 X22 H5 AM2 | 1.4462 | X2 CrNiMoN 22−5-3 | - |
| 03 X24 N13 G2 C | 1.4332 | X2 CrNi 24−12 | 309L |
| 08 X16 N13 M2 B | 1.4580 | X1 CrNiMoNb 17−12−2 | 316 Cd |
| 08 CR18 H12 B | 1.4550 | X6 CrNiNb 18−10 | 347 |
| 08 CRNINB 18−10 347 CD 08 X18 H12 B 1 4550 X6 CRNINB 18−10 347 | 1.4583 X10 CrNiMoNb | X10 CrNiMoNb 18−12 | 318 |
| 08X19AH9 | - | - | 304N |
| 08X19H13M3 | 1.4449 | X5 CrNiMo 17−13 | 317 |
| 08X20H11 | 1.4331 | X2 CrNi 21−10 | 308 |
| 08X20H20TU | 1.4847 | X8 CrNiAlTi 20−20 | 334 |
| 08X25H4M2 | 1.4460 | X3 CrnImOn 27−5-2 | 329 |
| 08X23H13 | - | - | 309S |
| 09X17H7U | 1.4568 | X7 CrNiAl 17−7 | 631 |
| 1X16H13M2 B | 1.4580 | X6 CrNiMoNb 17−12−2 | 316Cd |
| 10X13 EDELSTAHL | 1.4724 | X10 CrAlSi 13 | 405 |
| 12X15 | 1.4001 | X7 Cr 14 | 429 |
| 12X17 | 1.4016 | X6 Cr17 | 430 |
| 12X17M | 1.4113 | X6 CrMo 17−1 | 434 |
| 12X17MB | 1.4522 | X2 CrMoNb | 436 |
| 12X18H12 | 1.3955 | GX12 CrNi 18−11 | 305 |
| 12X17 G9 AH4 | 1.4373 | X12 CrMnNiN 18−9-5 | 202 |
| 15X9M | 1.7386 | X12 CrMo 9−1 | 504 |
| 15X12 | - | - | 403 |
| 15X13H2 | - | - | 414 |
| 15X17H7 | 1.4310 | X12 CrNi 17−7 | 301 |
| Legierungssorte nach GOST 1583−93 | Europäische Norm | USA | Japan | Frankreich | Italien | Vereinigtes Königreich |
|---|---|---|---|---|---|---|
| EN 1676 | ASTM, B179, B26, B85, AA, SAE | JIS, H5202, H2211, H2118 | NFA57−702 | UN14514 | BS14 | |
| AK8 (AL34) |
ENAB-42 100 (ENAB AlSi7Mg0,3) |
358.0 356.2 (A03562) |
AC4C.1 | A-S7G | - | - |
| AK7 | ENAB-42 000 (ENAB AlSi7Mg) |
357.0 356.1 (A03561) |
AC4C.1 | - | AlSi7Mg | - |
| AK7h (AL9) |
ENAB-42 000 (ENAB AlSi7Mg) |
356.0 356.1 (A03561) SG70A |
AC4C.1 | A-S7GU3 | AlSi7MgTi | LM2 |
| AK7pch (AL9−1) |
ENAB-42 100 (ENAB AlSi7Mg0,3) |
356.2 (A03562) |
AC4C.2 | A-S7G | AlSi7Mg | - |
| AK12 (AL2) |
ENAB-44 100 (ENAB AlSi12 (b)) |
A413.1 (A4131) |
AC3C.1 | A-S12G A-S13 |
G-Al-Si13 | LM6 |
Quelle: www. aluminium-union.ru
| GUS, GOST | USA AISI, ASTM, ASME |
Deutschland DIN |
Japan JIS |
China GB UK |
UK B.S. |
Italien UNI |
Frankreich AFNOR NF |
|---|---|---|---|---|---|---|---|
| 03CR17H14M3 | 316L SA-240TP316L |
X2CrNiMo18−14−3 | SUS 316L | 00Cr17Ni14Mo2 00Cr17Ni14Mo3 |
316S13 LW 22 |
X2CrNiMo 18−14−3 X2CrNiMo1713KG |
Z 3 CND 17−12−03 |
| 03X18H11 | 304 L SA-240TP304L |
X2 Cr Ni 19−11 GX2 Cr Ni 19−11 |
SUS304 L | - | 304S11 LW 20 LWCF 20 S 536 304 C12 (LT 196) 305 S 11 |
X2 CrNi 18 11 X 3 CrNi 18 11 GX 2 CrNi 19 10 |
Z 1 CN 18−12 Z 2 CN 18−10 Z 3 CN 19−10M Z 3 CN 18−10 Z 3 CN 19−11 Z 3 CN 19−11FF |
| 03CRNI28MDT 06CR28MDT |
- | X3NiCrCuMoTi2730 | - | - | - | - | - |
| 06X18H11 | 305 3008 |
X4CrNi18−12 | SUS 305 SUS 305J1 |
- | 305S17 305S19 |
X7 CrNi18 10 X8 CrNi 19 10 |
Z 5 CN 18−11FF |
| 07C16H6 | 301 A 167 301 A 240 301 A 666 301 |
X12CrNi17−7 X10CrNi18−8 |
SUS 301 | - | 301 S 21 301 S 22 Cr Ni 17/7 |
X10CrNi18−8 X12CrNi17−07 |
Z 11 CN 17−08 Z 11 CN 18−08 Z 12 CN 18−09 |
| 08kp | A 622 | St 50−2 | SPHE | - | BS 1449 1 HR |
- | 3C |
| 08X13 | 403 409 410 S 429 SA-240 TP 410S |
X6 Cr 13 X7 Cr 14 |
SUS 403 SUS 410S SUS429 |
- | 403 S17 | X6 Cr 13 | Z6 C13 Z8 C12 Z8 C13FF |
| 08X17H13M2T 10X17H13M2T |
316 Ti A 167 316Ti A 213 F316H A 240 316Ti A 368 316Ti SA-240 TP 316Ti SA-479 316Ti |
X6CrNiMoTi 12 122 X 10 CrNiMoTi 18−12 |
SUS 316Ti | 0Cr18Ni12Mo3Ti 1Cr18Ni12Mo3Ti |
320 S 33 CrNiMo 17/12/2 ¼ Ti |
X 6 CrNiMoTi 17 13 | Z6 CNDT 17.12 |
| 08CRNI17TI | 430Ti 439 |
X 6 CrTi 17 X3CrTi 17 |
SUS 430LX | - | - | X 3 CrTi 17 X 6 CrTi 17 |
Z 4 CT 17 |
| 08X18H10 | 304 304 H SA-240 TP 304 |
X5 Cr Ni 18 10 | SUS 304 | - | 304S11 304S15 304S16 304S17 304S31 LW21 LWCF 21 |
X 5 Cr Ni 18 10 | Z4 CN 19−10 FF Z5 CN 17−06 Z6CN 18.09 Z7 CN 18−09 |
| 08CR18NI12B | 347 A 167 347 A 240 347 A 313 347 A 580 347 |
X 6 CrNiNb 18 10 X6CrNiNb 18−10 |
SUS 347 | 0Cr18Ni11Nb 1Cr18Ni11Nb 1Cr19Ni11Nb |
347 S 20 347 S 31 ANC 3 Güteklasse B CrNi 18/9/Nb CrNi 18/9 0,10C/Nb |
X 6 CrNiNb 18 11 | Z 6 CNNb 18−10 |
| 08 SA | A 620 | DC 04 DC04 + ZE Fe P04 / St 14 St 14 St 4 |
SPCE | - | DC 04 / FeP 04 HR 1 HR 2 |
DC 04 / FeP 04 | DC 04 / FeP 04 |
| 09G2S | A 516−55 A 516−60 A 516−65 A 561 Gr70 |
- | SM41B SB49 |
- | - | - | - |
| 09CR17NI7U | - | X 7 CrNiAl 17 7 X7CrNiAl17−7 |
SUS 631 | 0Cr17Ni7Al | 301 S 81 | - | Z 9 CNA 17−07 |
| 10 | C1010 A 108 1010 A 29 M1010 A 510 1010 A 575 M1010 SA-29 M1010 |
C 10 C10E Ck 10 |
S 10 C S 9 CK SACM 1 |
10 | 040 A 10 045 M 10 En2A En32A HS 10 |
1 C 10 2 C 10 2 C 15 C 10 |
C 10 RR XC 10 |
| 10C13CU | A 268 TP405 | X10CrAl13 X10CrAlSi13 |
- | - | - | X 10 CrAl 12 | Z 13 C 13 |
| 10X23H18 20X23H18 |
SA-240 TP 310S | - | - | - | - | - | - |
| 12К | A 201 Gr AFx | ASt 35 | - | - | - | - | - |
| 12X13 15X13L |
410 430 A 183 F6 A 193 B6 A 479 410 |
X 10 Cr 13 X12 Cr13 GX 12 Cr 12 |
SUS 410 | - | 410C21 410S21 ANC 1A |
X 10 Cr13 X 12 Cr13 |
Z10C13 Z12C13 |
| 12Х17 | 430 A 182 F 430 A 240 430 SA-182 Güteklasse F 430 SA-240 Typ 430 |
X6Cr17 | SUS 430 | 1Cr15 1Cr17 ML1Cr17 |
17Cr 430S17 430S18 |
X 6 Cr 17 X 8 Cr 17 |
Z 8 C 17 |
| 12X18H10T 06X18H10T 08X18H10T 09CR18NI10T |
321 A 213 TP321H SA-240 TP 321 |
X6 Cr Ni Ti 18 10 X10 Cr Ni Ti 189 |
SUS 321 | - | 321S12 | - | Z6 CNT 18.10 |
| 12XM | A 182 Güteklasse F12 A213 Güteklasse T12 A 335 Güteklasse P12 A 387A, B, C |
13CrMo-44 | - | - | - | - | - |
| 12X2M | A 182 Güteklasse F22 A335 Güteklasse P22 387 Güteklasse D |
10CrMo910 | - | - | - | - | - |
| 12CR1MOV | - | 14MoV63 | - | - | - | - | - |
| 14Г2 | A414 Gr F, G A 515 Gr70 A516 Gr70 |
17 Mn4 | SB 46 SB 49 SG V 46 SG V 49 SP V 32 |
- | - | - | A 48CP |
| 15 | C1015 A 108 1015 A 512 1015 A 576 1015 |
C15 C15E Ck 15 |
S 15 C S 15 CK |
15 H15A ZG200−400 (ZG 15) |
- | - | C 18 RR XC 15 XC 18 |
| 15kp | A 621 FS Typ A A 621 FS Typ B |
DD 11 (StW 22) | SPHD | - | - | - | 1 C |
| 15Stück | A 29 1015 | QSt 38−3 | SWRCH15A SWRCH16R |
ML15 | - | CB 15 | - |
| 15H2M 15HM |
4615 | - | - | - | - | - | - |
| 15Х | - | 15Cr3 | - | - | - | - | - |
| 15X5M | A 182 Güteklasse F5 A 193 Güteklasse B5 |
- | - | - | - | - | - |
| 15X25T 15X28 |
A 268 TP446 | 10CrAl24 | - | - | - | - | - |
| 15XF | 6117 | - | - | - | - | - | - |
| 15CM | A 182 Güteklasse F12 A213 Güteklasse T12 A 335 Güteklasse P12 |
13CrMo-44 | - | - | - | - | - |
| 16К | A 414 Besoldungsgruppe E | H II St42−2 C22N ASt41 P 265 GH |
SG 295 SG 30 SM 53 B SM 53 C SPV 315 SPV 32 SPV 355 SPV 36 |
- | P 265 GH | Fe 410 KW P 265 GH |
- |
| 17GS | - | S355J2G3 / Fe 510 D1 St 52−3 St 52−3 / S355J2G3 St 52−3 G |
SM 490 A SM 520 C SM 53 C |
16Mn | - | Fe 510 Fe E 420 S 355 J 2 G 3 |
S 355 J 2 G 3 |
| 18CR | SA-29 Güte 5115 | 16 MnCr 5 | - | 15CrMn 20CrMn |
527 M 17 590 H 17 590 M 17 |
16 MnCr 5 | 16 MC 5 16 MnCr 5 RR |
| 20 | C1020 A 105 Gr1 A 106 GrA, B A 659 CS Typ 1020 A 794 CS Typ 1020 |
C 22 C 22N C 22.3 Ck 22 St35.8 St45.8 |
S 20 C S 20CK |
- | 040A20 070 M 20 070 M 26 1 C 22 C 22 En3A En3B En3C En3D |
C 20 C 21 C 22 |
C 20 XC 25 |
| 20К | A 283-C A 285-A, B, c A 414 Klasse E A 515−5 A 515−60 A 515−70 |
H II P 265 GH |
SG 295 SG 30 SM 53 B SM 53 C SPV 315 SPV 32 SPV 355 SPV 36 |
- | P 265 GH | Fe 410 KW P 265 GH |
- |
| 20ps | A 29 1020 | - | SWRCH17R | ML20 | 0/4 | - | - |
| 20H2M 20HM |
4621 | - | - | - | - | - | - |
| 20X | 5120 | - | - | - | - | - | - |
| 20KHF | 6120 | 22CrV4 | - | - | - | - | - |
| 20Х13 | 420 A 276 420 A 580 420 |
X 20 Cr 13 | SUS 420J1 | 2Cr13 | 420 S 37 En56C |
X 20 Cr 13 | Z 20 C 13 |
| 20CR17NI2 | 431 A 493 431 A 580 431 SA-479 Typ 431 |
X17CrNi16−2 X17CrNi16−2 (X 20 CrNi 17 2) |
SUS 431 | 1Cr17Ni2 ML1Cr17Ni2 |
431 S 29 En57 |
X 16 CrNi 1 | Z 15 CN 16−02 Z 15 CN 16.02 CI |
| 20CR25NI20C2 | 310 314 |
X15CrNiSi25−20 X15CrNiSi25−21 |
SUS Y 310 | 2Cr25Ni20 | - | X 16 CrNiSi 25 20 | Z 15 CNS 25−20 |
| 20CRM | 4130 SA-29 Güte 4130 |
25 CrMo 4 GS-25 CrMo 4 |
SKM 420 SCM 430 |
ML30CrMo ML30CrMoA |
25 CrMo 4 | 25 CrMo 4 | 25 CrMo 4 |
| 20XH | 3120 | - | - | - | - | - | - |
| 22K | 1022 1518 |
20Mn5 | S Mn C 420 | - | 120M19 | - | 20M5 |
| 25 | C1025 | - | - | - | - | - | - |
| 25Г | 1025 A 108 1025 A 510 1025 A 512 1025 A 513 1025 A 576 1025 |
GS-Ck 25 | S 25 C | 25 25Z ZG230−450 (ZG 25) |
070 M 26 080 A 25 |
- | - |
| 25X1MF | A 193 B14 A 540 B21 |
24CrMoV55 | - | - | - | - | - |
| 30 | C1030 A 29 1030 SA-29 1030 |
- | SWRCH30K SWRCH33K |
ML25Mn ML30 |
1/1 | - | - |
| 30X | 5130 | - | - | - | - | - | - |
| 30XM | 4130 A 302 Gr B A 304 |
25CrMo4 | - | - | - | - | - |
| 30KH13 | 420F | X30Cr13 | SUS 420J2 | 3Cr13 | 420 S 45 En56D |
G X 30 Cr 13 X 30 Cr 13 |
Z 30 C 13 Z 33 C 13 |
| 30CRM | - | 34 CrMo 4 GS-34 CrMo 4 |
SCM 435 SCM 435 H |
35CrMo | 34 CrMo 4 | 34 CrMo 4 | 34 CrMo 4 |
| 30G2 | - | 36 Mn 5 | SCMn 3 SMn 438 SMn 438 H |
- | 150 M 36 En15 En15A |
- | 40 M 5 |
| 35 | C1035 C1034 A 107 |
C 35 Ck 35 |
S 35C | - | 080M36 | - | XC 38 |
| 35X | 5132 | 34Cr4 | - | - | - | - | - |
| 35XM | - | 34CrMo4 | - | - | - | - | - |
| 40 | 1040 | C40 Ck40 |
S 40C | - | 080A40 060A40 |
- | XC 42 |
| 40X | 5140 | 41 Cr 4 | S Gr 440 | - | 530A40 530M40 |
- | 42C4 |
| 40KH13 | - | X38Cr13 X39Cr13 X46Cr13 |
SUS 420J2 | - | 420S45 | X 40 Cr 14 X 46 Cr 13 |
Z 38 C 13 M Z 40 C 13 Z 40 C 14 Z 44 C 14 Z 50 C 14 |
| 40CR2H2MA | 4340 SA-29 Güte 4340 |
40 NiCrMo 6 | SNCM 439 STPT 38 |
40CrNiMoA ML40CrNiMoA |
818 M 40 | - | - |
| 40XH | 3135 3140 |
40Ni Cr 6 | - | - | 640M40 | - | - |
| 40CRNI2MA | 9840 | 36 CrNiMo 4 | - | - | 36 CrNiMo 4 | 36 CrNiMo 4 | 36 CrNiMo 4 40 NCD 3 |
| 45 | 1045 A 107 A 29 1044 SA-29 1044 |
C 45 Ck 45 Cq 45 |
S 45C SWRCH45K |
ML45 | 080M 080M46 |
- | XC48 |
| 45Г | 1045 A 108 1045 A 29 1045 A 311 1045 A 576 1045 SA-29 1045 SA-311 1045 |
C45E Ck 45 GS-Ck 45 |
S 45 C S 48 C |
45 ZG310−570 (ZG 45) |
C 45 E | C 45 E | C 45 E XC 45 |
| 45X | 5145 | - | - | - | - | - | - |
| 50 | С1050 A 108 1050 A 29 1050 A 311 1050 A 510 1050 A 576 1050 SA-29 1050 SA-311 1050 |
C 50 E Ck 50 |
- | 50 | 080 M 50 C 50 E |
C 50 E | C 50 E XC 50 |
| 50X | 5147 | - | - | - | - | - | - |
| 55 | С1055 A 29 1055 A 576 1055 SA-29 1055 |
C 55 Ck 53 |
S 55 C S 55 C-CSP |
- | 070 M 55 C 55 En9 En9K |
C 55 | AF 70 C 54 C 55 |
| 60 60Г |
C1060 A 29 1060 A 576 1060 SA-29 1060 |
C 60 | S 58 C S 60 C-CSP S 65 C-CSP |
- | 060 A 62 C 60 CS 60 HS 60 |
C 60 | C 60 |
| St0 St1kn |
A 283 Güteklasse A | S185 / Fe 310−0 St 33 |
SS 330 | Q195 Q195-F Q195-Z Q195-b |
HR 15 | S 185 | - |
| St2ps St2sp |
A53 Gr A A192 Gr A |
St 35 | - | Q215B Q215B-F Q215B-Z Q215B-b |
S360 | - | - |
| St3kn | A 107 A 283 Güteklasse C SA-283 C |
USt 37−2 USt 37−2 G RSt37−2 |
- | A3 Q235A Q235A-F Q235A-Z Q235A-b |
- | - | - |
| St3sp | A 414 Güteklasse A A 570 Sorte 36 |
S235J2G3 / Fe 360 D1 St 37−3 St 37−3 G UZSt 37−2 |
SS34 | - | HS 37/23 S 235 J 2 G 3 40C BS4360 |
S 235 J 2 G 3 | S 235 J 2 G 3 E 24−2NE |
| St5sp | A 570 Güteklasse 50 | St 50−2 | SS 50 | - | - | - | А 50−2 |
| St6ps St6sp |
A 572 Güteklasse 65 | E335 / Fe 590−2 St 60−2 St 60−2 G |
SM 570 SM 58 |
- | 55 C E 335 |
E 335 Fe 590 |
E 335 |
Quelle: gosts.org
| Stahlsorte GUS-Länder GOST | Euronorm-Stahlsorte | Stahlsorte Euronormen | US-Entsprechung |
|---|---|---|---|
| 10 | C10E | 1.1121 | 1010 |
| 10XHH1 | 10 XHN1 | 1.5805 | - |
| 14 CRH3 M | 14 NiCrMo1−3-4 | 1.6657 | 9310 |
| 15 | C15 E | 1.1141 | 1015 |
| 15 Г | C16 E | 1.1148 | 1016 |
| 16 CH | 16 MnCr5 | 1.7131 | 5115 |
| 16XGR | 16Mn CrB5 | 1.7160 | - |
| 16 CHN | 16NiCr4 | 1.5714 | - |
| 17 G1 C | S235J2G4 | 1.0117 | - |
| 17 CH3 | 15NiCr13 | 1.5752 | Е3310 |
| 18 CGM | 18CrMo4 | 1.7243 | 4120 |
| 18 X2 H2 M | 18CrNiMo7−6 | 1.6587 | - |
| 20 | C22E | 1.1151 | 1020 |
| 20 XM | 20MoCr3 | 1.7320 | 4118 |
| 20CRNIM | 20MoCr2−2 | 1.6523 | 8617 |
| 25 | C25E | 1.1158 | 1025 |
| 25 XM | 25CrMo4 | 1.7218 | 4130 |
| 28 Г | 28Mn6 | 1.1170 | 1330 |
| 30 | C30E | 1.1178 | 1030 |
| 34 Х | 34Cr4 | 1.7033 | 5130 |
| 34 X2 H2 M | 34CrNiMo6 | 1.6582 | 4340 |
| 35 | C35E | 1.1181 | 1035 |
| 36 CNM | 36CrNiMo4 | 1.6511 | 9840 |
| 36 X2 H4 MA | 36NiCrMo16 | 1.6773 | - |
| 40 | C40E | 1.1186 | 1040 |
| 42 XM | 42CrMo4 | 1.7225 | 4140 |
| 45 | C45E | 1.1191 | 1045 |
| 46 Х | 46Cr2 | 1.7006 | 5045 |
| 50 | C50E | 1.1206 | 1050 |
| 50 CGF | 50CrV4 | 1.8159 | 6150 |
Quelle: metaltrade.ru
| Stahlsorte GUS-Länder GOST | Stahlsorte Euronormen | Stahlsorte Euronormen | Analogien in US-Normen |
|---|---|---|---|
| 10 X2 M | 10CrMo9−10 | 1.7380 | F22 |
| 13 XM | 13CrMo4−4 | 1.7335 | F12 |
| 14 XMF | 14MoV6−3 | 1.7715 | - |
| 15 М | 15Mo3 | 1.5415 | F1 |
| 17 Г | 17Mn4 | 1.0481 | - |
| 20 | C22.8 | 1.0460 | - |
| 20 Г | 20Mn5 | 1.1133 | - |
| 20 X11 MNF | X20CrMoV12−1 | 1.4922 | - |
Quelle: metaltrade.ru
| GUS-Länder (GOST 1050−88) | Deutschland (DIN) Ausländische Entsprechungen | Deutschland (DIN) Ausländische Entsprechungen | USA (ASTM) |
|---|---|---|---|
| 10 | 1.0301 | C 10/Sc 10 | 1010 |
| 15 | 1.0401 | C15/Sc 15 | 1015 |
| 20 | 1.0402 | C 22/Sq 22 | 1020 |
| 30 | - | - | 1030 |
| 35 | 1.0501 | C 35/Ck 35 | 1035 |
| 40 | 1.0511 | C 40/Sk 40 | 1040 |
| 45 | 1.0503 | C 45/Sk 45 | 1045 |
| 50 | 1.0540 | C 50/Quadrat 50 | 1050 |
| 55 | 1.0535 | C 55/Quadrat 55 | 1055 |
| 60 | 1.0601 | C 60/Quadrat 60 | 1060 |
Quelle: metallopt.ru
| GUS-Länder (GOST, TU) | Deutschland (DIN) Ausländische Analoga | Deutschland (DIN) Ausländische Analoge | USA (ASTM) |
|---|---|---|---|
| 12XH3A | 1.5732 | 14NiCr10 | - |
| 12CR4A | Е3310 | ||
| 15CRM | 1.7335 | 13CrMo44 | - |
| 17G1S | 1.0570 | St52−3 | - |
| 18CR | 1.7131 | 16MnCr5 | 5120 |
| 20CR | 1.7218 | 25CrMo4 | 4130 |
| 27CRMO4 | 1.5526 | 30MnB4 | - |
| 30CR3MOV | 1.8519 | 31CrMoV9V | - |
| 30CR2H2M | 1.6580 | 30CrNiMo8V | - |
| 34CR2NIMO8V | 1.8550 | 34CrAlNi7V | - |
| 38CR2H2MA | 1.6582 | 34CrNiMo6 | 4330 |
| 40Х | 1.7045 | 42Cr4 | 5140 |
| 40CRM | 1.7225 | 42CrMo4 | 4140 |
| 40CRNI2MA | 1.6565 | 40NiCrMo6 | 4340 |
| 40CRNINM | 1.6546 | 40NiCrMo22 | 8640 |
| 45Г | 1.0912 | 46Mn7 | - |
Quelle: metallopt.ru
| Stahlsorte GUS-Länder GOST | Stahlsorte Euronormen | Stahlsorte Euronormen | Entsprechungen in US-Normen |
|---|---|---|---|
| SHCR4 | 100Cr2 | 1.3501 | 50 100 |
| 30 30CR15 | 100Cr6 | 1.3505 | 52 100 |
| SHCR15 SG | 100CrMn6 | 1.3520 | A 485 (2) |
| 485 (2) Ø ØCR20 M | 100CrMo7 | 1.3537 | A 485 (3) |
Quelle: metaltrade.ru
| Stahlsorte GUS-Länder GOST | Euronorm-Stahlsorte | Euronorm-Stahlsorte | Entsprechungen in US-Normen |
|---|---|---|---|
| 38C2A | 38Si7 | 1.5023 | - |
| 50CRVA | 50CrV4 | 1.8159 | 6150 |
| 52 CGMFA | 51CrMoV4 | 1.7701 | - |
| 55 CR2A | 54SICr6 | 1.7102 | - |
| 55 CGA | 55Cr3 | 1.7176 | 5147 |
| 60 C2 CGA | 60SiCR7 | 1.7108 | 9262 |
Quelle: metaltrade.ru
| GUS-Länder (GOST, TU) | Deutschland (DIN) Ausländische Analoga | Deutschland (DIN) Ausländische Entsprechungen | USA (ASTM) |
|---|---|---|---|
| 70 | 1.1231 | Ck 67 | 1070 |
| 75 | 1.0605 | C 75 | 1074 |
| 85 | 1.1269 | Ck 85 | 1086 |
| 50CFA | 1.8159 | 50CrV4 | 6150 |
| 55С2 | 1.5026 | 55Si7 | - |
| 60Г | 1.0601 | С 60 | 1060 |
| 60C2 | 1.5027 | 60Si7 | 9260 |
| 60C2GH | 1.5092 | 60SiCr7 | 9262 |
| 70C2X | 1.5029 | 71Si 7 | - |
Quelle: metallopt.ru
| GUS-Länder (GOST, TU) | Deutschland (DIN) Ausländische Analoga | Deutschland (DIN) Ausländische Entsprechungen | USA (ASTM) |
|---|---|---|---|
| У 7 | 1.1620 | C 70W2 | - |
| U 7A | 1.1520 | C 70W1 | - |
| У 8 | 1.1625 | C 80W2 | - |
| U 8A | 1.1525 | C 80W1 | W 108 |
| У 10 | 1.1645 | C 105W2 | - |
| W 10A | 1.1545 | C 105W1 | W 110 |
| У 11 | 1.1654 | C 110W | - |
| У 13 | 1.1663 | C 125W | W 112 |
Quelle: metallopt.ru
| GUS-Länder (GOST, TU) | Deutschland (DIN/BOHLER) Ausländische Entsprechungen | Deutschland (DIN/BOHLER) Ausländische Entsprechungen | USA (AISI/ASTM) |
|---|---|---|---|
| Х12 | 1.2080 | X210Cr12 | D3 |
| X12B | 1.2436 | X210CrW12 | - |
| X12MF* | 1.2379 | X155CrVMo12−1 | D2 |
| X12MF4-MP | - | K190RM | - |
| 95CRF | 1.2210 | 115CrV 3 | L2 |
| 9X1F | 1.2067 | 102Cr 6 | L3 |
| 9G2F | 1.2842 | 90MnCrV 8 | O2 |
| 95CRVF | 1.2510 | 100MnCrW 4 | O1 |
| 3CR3B9F | 1.2581 | X30WCrV9−3 | H21 |
| 95CR5GM | 1.2363 | X100CrMoV5−1 | А2 |
| 95CRM | 1.2303 | 100CrMo 5 | L7 |
| 95Х18 | 1.4125 | X105CrMo17 | A473 (440C) |
| 5CRNIMO | 1.2713 | 55NiCrMoV 6 | L6 |
| 5CR2SF | 1.2550 | 60WCrV 7 | S1 |
| 5CR3MO2F | - | - | S7 |
| 5CRNI2MOV | 1.2714 | 56NiCrMoV 7 | - |
| 3CR3M3F | 1.2365 | X32CrMoV3 3 | H10 |
| 4X5MFS | 1.2343 | X38CrMoV5−1 | H11 |
| 4X5MF1C | 1.2344 | X40CrMoV5−1 | H13 |
*mögliche Herstellung durch Pulvermetallurgieverfahren
Quelle: metallopt.ru
| Stahlsorte GUS-Länder GOST | Stahlsorte Euronormen | Stahlsorte Euronormen | Analogien in US-Normen |
|---|---|---|---|
| P0 M2 SF10-MP | - | - | А11 |
| R2 M9-MP | S2−9-2 | 1.3348 | М7 |
| R2 M10 K8-MP | S2−10−1-8 | 1.3247 | М42 |
| R6 M5-MP | S6−5-2 | 1.3343 | М2 |
| R6 M5 K5-MP | S6−5-2−5 | 1.3243 | - |
| R6 M5 F3-MP | S6−5-3 | 1.3344 | М3 |
| P6 M5 F4-MP | - | - | М4 |
| R6 M5 F3 K8-MP | - | - | М36 |
| R10 M4 F3 K10-PP | S10−4-3−10 | 1.3207 | - |
| R6 M5 F3 K9-MP | - | - | М48 |
| R12 M6 F5-MP | - | - | М61 |
| R12 F4 K5-MP | S12−1-4−5 | 1.3202 | - |
| R12 F5 K5-MP | - | - | Т15 |
| R18-MP | - | - | Т1 |
Quelle: metaltrade.ru
| GUS-Länder (GOST, TU) | Deutschland (DIN) | BOHLER (D-016) | USA (AISI/ASTM) |
|---|---|---|---|
| R18* | 1.3355 | S 200 | Т 1 |
| R6M5* | 1.3343 | S600/S601 | М 2 |
| R6M5K5* | 1.3243 | S 705 | - |
| R6M5F3-MP | 1.3342/1.3344 | S 790PM | М 3 |
| R6M5F4-MP | - | S 690PM | М 4 |
| R6M5F3K8-MP | - | S 590PM | М 36 |
| R10M2F5K8-MP | - | S 390PM | - |
| R10M3F4K8-MP | - | - | - |
| R12F3 | 1.3318 | - | - |
| R12MF4-MP | - | S 207PM | - |
| R12K5F4-MP | - | S 308PM | - |
| R12M6F5-MP | - | - | М 61 |
| R12MF5K5-MP | 1.3202 | - | Т 15 |
| R0M2SF10-MP | - | CPM 10V | А 11 |
* Herstellung nach dem pulvermetallurgischen Verfahren ist möglich
Quelle: metallopt.ru
| GUS-Länder (GOST) | Analog | Land Standard |
|---|---|---|
| 20GL | A352 Gr LCC | USA, ASTM A352 |
| 20GL | A757 Gr A2Q | USA, ASTM A757 |
| 20GL | A216 Gr WCC | USA, ASTM A216 |
| 30GSL | A304 (1330H) | USA, ASTM A304 |
| 30GSL | A322 (1330) | 1330H USA, ASTM A322 |
| 20Л | A732 (1A) | 1A USA, ASTM A732 |
| 25Л | A352 Gr LCA | 20L (1A) ASTM A732 (1A) USA, ASTM A352 |
| 25Л | A732 (2A) | 2A USA, ASTM A732 |
| 25Л | A216 Gr WCB | USA, ASTM A216 |
| 30Л | A352 Gr LCB | USA, ASTM A352 |
| 30Л | A216 Gr WCB | USA, ASTM A216 |
| 35Л | A356 Gr1 | USA, ASTM A356 |
| 40Л | A732 (3A) | USA, ASTM A732 |
Quelle: www. td-ksz.com
| GUS-Länder (GOST) | Analog | Land Norm |
|---|---|---|
| 20GL | 1.1120 | Deutschland, DIN 17 182 |
| 30GSL | 1.1165 | Deutschland, DIN 17 205 |
| 15Л | 1.0420 | Deutschland, DIN 1681 |
| 20Л | 1.0619 | Deutschland, DIN EN 10 213−2 |
| 25Л | 1.0446 | Deutschland, DIN 1681 |
| 35Л | 1.0552 | Deutschland, DIN 1681 |
| 45Л | 1.0558 | Deutschland, DIN 1681 |
Quelle: www. td-ksz.com
| GUS-Länder (GOST) | Kurzbezeichnung | Land Norm |
|---|---|---|
| 30GSL | AO35 MnSi5 | Ungarn, MSZ 8272 |
| 30GSL | 30 GSL | Bulgarien, BDS 6550 |
| 30GSL | T30 Si Mn12 | Rumänien, STAS 1773 |
| 15Л | 15LII | Bulgarien, BDS3492 |
| 15Л | AM1 | BRITANNIEN, B.S.3100 (91) |
| 15Л | Ao 400 FK | Ungarn, MSZ 8276 |
| 15Л | L II 400 | Polen, PN/H 83 152 |
| 15Л | OT 400−3 | Rumänien, STAS 600 |
| 15Л | 422 630 | Tschechische Republik, Slowakei, CSN 422 630 |
| 25Л | 161 Grad 430 | Großbritannien, B.S. 1504 (76) |
| 25Л | 25 LII | Bulgarien, BDS 3492 |
| 25Л | Ao 450 FK | Ungarn, MSZ 8276 |
| 25Л | OT 450−3 | Rumänien, STAS 600 |
| 25Л | 25LI | Bulgarien, BDS 3492 |
| 25Л | 422 640 | Tschechische Republik, Slowakei, CSN 422 640 |
| 25Л | L 450 | Polen, PN/H 83 152 |
| 30Л | 1505 | Schweden, SS |
| 35Л | 35LII | Bulgarien, BDS 3492 |
| 35Л | A2 | BRITANNIEN, B.S.3100 (91) |
| 35Л | Ao 500 FK | Ungarn, MSZ 8276 |
| 35Л | L500 | Polen, PN/H8 3152 |
| 35Л | OT 500−1 | Rumänien, STAS 600 |
| 35Л | 35LI | Bulgarien, BDS3492 |
| 35Л | 422 650 | Tschechische Republik, Slowakei, CSH 422 650 |
| 35Л | G-30−57 | Finnland, SFS 350 |
| 35Л | SCC | Japan, JIS G5111 (91) |
| 40Л | 35LI | Bulgarien, BDS 3492 |
| 40Л | OT 550−1 | Rumänien, STAS 600 |
| 40Л | CLA1 Klasse C | UK, B.S. 3146 Teil 1 (74) |
| 40Л | CLA8 Grad C | UK, B.S. 3146 Teil 1 (74) |
| 40Л | G-30−57 | Finnland, SFS 350 |
| 45Л | 45LI | Bulgarien, BDS 3492 |
| 45Л | A3 | BRITANNIEN, B.S.3100 (91) |
| 45Л | Ao550FK | Ungarn, MSZ 8276 |
Quelle: www. td-ksz.com
| Europa (EN) | Deutschland (DIN) | USA (AISI) | Japan (JIS) | GUS (GOST) |
|---|---|---|---|---|
| 1.4713 | X10CrAl7 | 10CR17CU | ||
| 1.4724 | X10CrAl13 | 405 | 10CR13CU | |
| 1.4742 | X10CrAl18 | 442 | ||
| 1.4762 | X10CrAl24 | 446 | ||
| 1.4878 | X12CrNiTi18−9 | 321 H | 12X18H10T | |
| 1.4828 | X15CrNiSi20−12 | 309 | 20X20H14C2 | |
| 1.4845 | X12CrNi25−21 | 310 S | 20CR23NI18 | |
| 1.4841 | X15CrNiSi25−20 | 314 | 20CR25H20C2 |
Quelle: www.uvis.ua
| Europa (EN) | Deutschland (DIN) | USA (AISI) | Japan (JIS) | GUS (GOST) |
|---|---|---|---|---|
| 1.4003 | X2CrNi12 | |||
| 1.4512 | X2CrTi12 | 409 | SUH 409 | |
| 1.4000 | X6Cr13 | 410S | SUS 410 S | 08KH13 |
| 1.4002 | X6CrAl13 | 405 | SUS 405 | |
| 1.4006 | X12CrN13 | 410 | SUS 410 | 12KH13 |
| 1.4024 | X15Cr13 | (410) | SUS 410 J1 | |
| 1.4021 | X20Cr13 | (420) | SUS 420 J1 | 20Х13 |
| 1.4028 | X30Cr13 | (420) | SUS 420 J2 | 30KH13 |
| 1.4031 | X39Cr13 | SUS 420 J2 | 40KH13 | |
| 1.4034 | X46Cr13 | (420) | 40KH13 | |
| 1.4016 | X6Cr17 | 430 | SUS 430 | 12Х17 |
| 1.4520 | X2CrTi17 | |||
| 1.4510 | X3CrTi17 | 439 | SUS 430 LX | 08CR17TI |
| 1.4113 | X6CrMo17−1 | 434 | SUS 434 | |
| 1.4509 | X2CrTiNb18 | 441 | ||
| 1.4521 | X2CrMoTi18−2 | 444 | SUS 444 | |
| 1.4589 | X5CrNiMoTi15−2 | |||
| 1.4310 | X10CrNi18−8 | (301) | SUS 301 | |
| 1.4318 | X2CrNiN18−7 | 301 LN | SUS 301 LN | |
| 1.4301 | X5CrNI18−10 | 304 | SUS 304 | 08CR18NI10 |
| 1.4303 | X4CrNi18−12 | (305) | SUS 305 | 12X18H12 |
| 1.4306 | X2CrNi19−11 | 304 L | SUS 304 L | 03CR18NI11 |
| 1.4541 | X6CrNiTi18−10 | 321 | SUS 321 | 08CR18NITI10T |
| 1.4550 | X6CrNiNb18−10 | 347 | SUS 347 | |
| 1.4401 | X5CrNiMo17−12−2 | 316 | SUS 316 | |
| 1.4404 | X2CrNiMo17−12−2 | 316 L | SUS 316 L | |
| 1.4571 | X6CrNiMoTi17−12−2 | 316 Ti | SUS 316 Ti | 10X17H13M2T |
| 1.4561 | X1CrNiMoTi18−13−2 | |||
| 1.4435 | X2CrNiMo18−14−3 | 316 L | SUS 316 L | 03CR17H14M2 |
| 1.4439 | X2CrNiMoN17−13−5 | S 31 726 | SUS 317 | |
| 1.4539 | X1NiCrMoCu25−20−5 | N 8 904 | ||
| 1.4565 | X3CrNiMnMoNbN 23−17−5-3 | S 34 565 | ||
| 1.4462 | X2CrNiMoN22−5-3 | S 31 803 | SUS 329 J3L | |
| Europa (EN) | Deutschland (DIN) | USA (AISI) | Japan (JIS) | GUS (GOST) |
Quelle: www.uvis.ua
| GUS (GOST) | Euronormen (EN) | Deutschland (DIN) | USA (AISI) |
|---|---|---|---|
| 03 X17 H13 M2 | 1.4404 | X2 CrNiMo 17−12−2 | 316 L |
| 03 X17 H14 M3 | 1.4435 | X2 CrNiMo 18−4-3 | - |
| 03 X18 H11 | 1.4306 | X2 CrNi 19−11 | 304 L |
| 03 X18 H10 T-U | 1.4541-MOD | - | - |
| 06 CHN28-MDT | 1.4503 | X3 NiCrCuMoTi 27−23 | - |
| 06 X18 H11 | 1.4303 | X4 CrNi 18−11 | 305 L |
| 08 X12 T1 | 1.4512 | X6 CrTi 12 | 409 |
| 08 Х13 | 1.4000 | X6 Cr 13 | 410S |
| 08 CR17 H13 M2 | 1.4436 | X5CrNiMo 17−13−3 | 316 |
| 08 X17 H13 M2 T | 1.4571 | X6 CrNiMoTi 17−12−2 | 316Ti |
| 08 CR17 T | 1.4510 | X6 CrTi 17 | 430Ti |
| 08 X18 H10 | 1.4301 | X5 CrNi 18−10 | 304 |
| 08 CR18 H12 T | 1.4541 | X6 CrNiTi 18−10 | 321 |
| 10 X23 H18 | 1.4842 | X12 CrNi 25−20 | 310S |
| 10X13 | 1.4006 | X10 Cr13 | 410 |
| 12 X18 H10 T | 1.4878 | X12 CrNiTi 18−9 | - |
| 12 X18 H9 | - | - | 302 |
| 15 X5 M | 1.7362 | X12 CrCo 5 | 501 |
| 15 X25 T | 1.4746 | X8 CrTi 25 | - |
| 20X13 | 1.4021 | X20 Cr 13 | 420 |
| 20 X17 H2 | 1.4057 | X20 CrNi 17−2 | 431 |
| 20 X23 H13 | 1.4833 | X7 CrNi 23−14 | 309 |
| 20 X23 H18 | 1.4843 | X16 CrNi 25−20 | 310 |
| 20 X25 H20 C2 | 1.4841 | X56 CrNiSi 25−20 | 314 |
| 03 X18 AH11 | 1.4311 | X2 CrNiN 18−10 | 304LN |
| 03 X19 H13 M3 | 1.4438 | X2 18−5-4 | 317L |
| 03 X23 H6 | 1.4362 | X2 CrNiN 23−4 | - |
| 02 X18 M2 BT | 1.4521 | X2 CrMoTi 18−2 | 444 |
| 02 X28 H30 MDB | 1.4563 | X1 NiCrMoCu 31−27−4 | - |
| 03 X17 H13 AM3 | 1.4429 | X2 CrNiMoN 17−13−3 | 316LN |
| 03 X22 H5 AM2 | 1.4462 | X2 CrNiMoN 22−5-3 | - |
| 03 X24 N13 G2 C | 1.4332 | X2 CrNi 24−12 | 309L |
| 08 X16 N13 M2 B | 1.4580 | X1 CrNiMoNb 17−12−2 | 316 Cd |
| 08 CR18 H12 B | 1.4550 | X6 CrNiNb 18−10 | 347 |
| 08 CRNINB 18−10 347 CD 08 X18 H12 B 1 4550 X6 CRNINB 18−10 347 | 1.4583 X10 CrNiMoNb | X10 CrNiMoNb 18−12 | 318 |
| 08X19AH9 | - | - | 304N |
| 08X19H13M3 | 1.4449 | X5 CrNiMo 17−13 | 317 |
| 08X20H11 | 1.4331 | X2 CrNi 21−10 | 308 |
| 08X20H20TU | 1.4847 | X8 CrNiAlTi 20−20 | 334 |
| 08X25H4M2 | 1.4460 | X3 CrnImOn 27−5-2 | 329 |
| 08X23H13 | - | - | 309S |
| 09X17H7U | 1.4568 | X7 CrNiAl 17−7 | 631 |
| 1X16H13M2 B | 1.4580 | X6 CrNiMoNb 17−12−2 | 316Cd |
| 10X13 EDELSTAHL | 1.4724 | X10 CrAlSi 13 | 405 |
| 12X15 | 1.4001 | X7 Cr 14 | 429 |
| 12X17 | 1.4016 | X6 Cr17 | 430 |
| 12X17M | 1.4113 | X6 CrMo 17−1 | 434 |
| 12X17MB | 1.4522 | X2 CrMoNb | 436 |
| 12X18H12 | 1.3955 | GX12 CrNi 18−11 | 305 |
| 12X17 G9 AH4 | 1.4373 | X12 CrMnNiN 18−9-5 | 202 |
| 15X9M | 1.7386 | X12 CrMo 9−1 | 504 |
| 15X12 | - | - | 403 |
| 15X13H2 | - | - | 414 |
| 15X17H7 | 1.4310 | X12 CrNi 17−7 | 301 |
| Legierungssorte nach GOST 1583−93 | Europäische Norm | USA | Japan | Frankreich | Italien | Vereinigtes Königreich |
|---|---|---|---|---|---|---|
| EN 1676 | ASTM, B179, B26, B85, AA, SAE | JIS, H5202, H2211, H2118 | NFA57−702 | UN14514 | BS14 | |
| AK8 (AL34) |
ENAB-42 100 (ENAB AlSi7Mg0,3) |
358.0 356.2 (A03562) |
AC4C.1 | A-S7G | - | - |
| AK7 | ENAB-42 000 (ENAB AlSi7Mg) |
357.0 356.1 (A03561) |
AC4C.1 | - | AlSi7Mg | - |
| AK7h (AL9) |
ENAB-42 000 (ENAB AlSi7Mg) |
356.0 356.1 (A03561) SG70A |
AC4C.1 | A-S7GU3 | AlSi7MgTi | LM2 |
| AK7pch (AL9−1) |
ENAB-42 100 (ENAB AlSi7Mg0,3) |
356.2 (A03562) |
AC4C.2 | A-S7G | AlSi7Mg | - |
| AK12 (AL2) |
ENAB-44 100 (ENAB AlSi12 (b)) |
A413.1 (A4131) |
AC3C.1 | A-S12G A-S13 |
G-Al-Si13 | LM6 |
Quelle: www. aluminium-union.ru
| GUS, GOST | USA AISI, ASTM, ASME |
Deutschland DIN |
Japan JIS |
China GB VEREINIGTES KÖNIGREICH |
UK B.S. |
Italien UNI |
Frankreich AFNOR NF |
|---|---|---|---|---|---|---|---|
| 03CR17H14M3 | 316L SA-240TP316L |
X2CrNiMo18−14−3 | SUS 316L | 00Cr17Ni14Mo2 00Cr17Ni14Mo3 |
316S13 LW 22 |
X2CrNiMo 18−14−3 X2CrNiMo1713KG |
Z 3 CND 17−12−03 |
| 03X18H11 | 304 L SA-240TP304L |
X2 Cr Ni 19−11 GX2 Cr Ni 19−11 |
SUS304 L | - | 304S11 LW 20 LWCF 20 S 536 304 C12 (LT 196) 305 S 11 |
X2 CrNi 18 11 X 3 CrNi 18 11 GX 2 CrNi 19 10 |
Z 1 CN 18−12 Z 2 CN 18−10 Z 3 CN 19−10M Z 3 CN 18−10 Z 3 CN 19−11 Z 3 CN 19−11FF |
| 03CRNI28MDT 06CR28MDT |
- | X3NiCrCuMoTi2730 | - | - | - | - | - |
| 06X18H11 | 305 3008 |
X4CrNi18−12 | SUS 305 SUS 305J1 |
- | 305S17 305S19 |
X7 CrNi18 10 X8 CrNi 19 10 |
Z 5 CN 18−11FF |
| 07C16H6 | 301 A 167 301 A 240 301 A 666 301 |
X12CrNi17−7 X10CrNi18−8 |
SUS 301 | - | 301 S 21 301 S 22 Cr Ni 17/7 |
X10CrNi18−8 X12CrNi17−07 |
Z 11 CN 17−08 Z 11 CN 18−08 Z 12 CN 18−09 |
| 08kp | A 622 | St 50−2 | SPHE | - | BS 1449 1 HR |
- | 3C |
| 08X13 | 403 409 410 S 429 SA-240 TP 410S |
X6 Cr 13 X7 Cr 14 |
SUS 403 SUS 410S SUS429 |
- | 403 S17 | X6 Cr 13 | Z6 C13 Z8 C12 Z8 C13FF |
| 08X17H13M2T 10X17H13M2T |
316 Ti A 167 316Ti A 213 F316H A 240 316Ti A 368 316Ti SA-240 TP 316Ti SA-479 316Ti |
X6CrNiMoTi 12 122 X 10 CrNiMoTi 18−12 |
SUS 316Ti | 0Cr18Ni12Mo3Ti 1Cr18Ni12Mo3Ti |
320 S 33 CrNiMo 17/12/2 ¼ Ti |
X 6 CrNiMoTi 17 13 | Z6 CNDT 17.12 |
| 08CRNI17TI | 430Ti 439 |
X 6 CrTi 17 X3CrTi 17 |
SUS 430LX | - | - | X 3 CrTi 17 X 6 CrTi 17 |
Z 4 CT 17 |
| 08X18H10 | 304 304 H SA-240 TP 304 |
X5 Cr Ni 18 10 | SUS 304 | - | 304S11 304S15 304S16 304S17 304S31 LW21 LWCF 21 |
X 5 Cr Ni 18 10 | Z4 CN 19−10 FF Z5 CN 17−06 Z6CN 18.09 Z7 CN 18−09 |
| 08CR18NI12B | 347 A 167 347 A 240 347 A 313 347 A 580 347 |
X 6 CrNiNb 18 10 X6CrNiNb 18−10 |
SUS 347 | 0Cr18Ni11Nb 1Cr18Ni11Nb 1Cr19Ni11Nb |
347 S 20 347 S 31 ANC 3 Güteklasse B CrNi 18/9/Nb CrNi 18/9 0,10C/Nb |
X 6 CrNiNb 18 11 | Z 6 CNNb 18−10 |
| 08 SA | A 620 | DC 04 DC04 + ZE Fe P04 / St 14 St 14 St 4 |
SPCE | - | DC 04 / FeP 04 HR 1 HR 2 |
DC 04 / FeP 04 | DC 04 / FeP 04 |
| 09G2S | A 516−55 A 516−60 A 516−65 A 561 Gr70 |
- | SM41B SB49 |
- | - | - | - |
| 09CR17NI7U | - | X 7 CrNiAl 17 7 X7CrNiAl17−7 |
SUS 631 | 0Cr17Ni7Al | 301 S 81 | - | Z 9 CNA 17−07 |
| 10 | C1010 A 108 1010 A 29 M1010 A 510 1010 A 575 M1010 SA-29 M1010 |
C 10 C10E Ck 10 |
S 10 C S 9 CK SACM 1 |
10 | 040 A 10 045 M 10 En2A En32A HS 10 |
1 C 10 2 C 10 2 C 15 C 10 |
C 10 RR XC 10 |
| 10C13CU | A 268 TP405 | X10CrAl13 X10CrAlSi13 |
- | - | - | X 10 CrAl 12 | Z 13 C 13 |
| 10X23H18 20X23H18 |
SA-240 TP 310S | - | - | - | - | - | - |
| 12К | A 201 Gr AFx | ASt 35 | - | - | - | - | - |
| 12X13 15X13L |
410 430 A 183 F6 A 193 B6 A 479 410 |
X 10 Cr 13 X12 Cr13 GX 12 Cr 12 |
SUS 410 | - | 410C21 410S21 ANC 1A |
X 10 Cr13 X 12 Cr13 |
Z10C13 Z12C13 |
| 12Х17 | 430 A 182 F 430 A 240 430 SA-182 Güteklasse F 430 SA-240 Typ 430 |
X6Cr17 | SUS 430 | 1Cr15 1Cr17 ML1Cr17 |
17Cr 430S17 430S18 |
X 6 Cr 17 X 8 Cr 17 |
Z 8 C 17 |
| 12X18H10T 06X18H10T 08X18H10T 09CR18NI10T |
321 A 213 TP321H SA-240 TP 321 |
X6 Cr Ni Ti 18 10 X10 Cr Ni Ti 189 |
SUS 321 | - | 321S12 | - | Z6 CNT 18.10 |
| 12XM | A 182 Güteklasse F12 A213 Güteklasse T12 A 335 Güteklasse P12 A 387A, B, C |
13CrMo-44 | - | - | - | - | - |
| 12X2M | A 182 Güteklasse F22 A335 Güteklasse P22 387 Güteklasse D |
10CrMo910 | - | - | - | - | - |
| 12CR1MOV | - | 14MoV63 | - | - | - | - | - |
| 14Г2 | A414 Gr F, G A 515 Gr70 A516 Gr70 |
17 Mn4 | SB 46 SB 49 SG V 46 SG V 49 SP V 32 |
- | - | - | A 48CP |
| 15 | C1015 A 108 1015 A 512 1015 A 576 1015 |
C15 C15E Ck 15 |
S 15 C S 15 CK |
15 H15A ZG200−400 (ZG 15) |
- | - | C 18 RR XC 15 XC 18 |
| 15kp | A 621 FS Typ A A 621 FS Typ B |
DD 11 (StW 22) | SPHD | - | - | - | 1 C |
| 15Stück | A 29 1015 | QSt 38−3 | SWRCH15A SWRCH16R |
ML15 | - | CB 15 | - |
| 15H2M 15HM |
4615 | - | - | - | - | - | - |
| 15Х | - | 15Cr3 | - | - | - | - | - |
| 15X5M | A 182 Güteklasse F5 A 193 Güteklasse B5 |
- | - | - | - | - | - |
| 15X25T 15X28 |
A 268 TP446 | 10CrAl24 | - | - | - | - | - |
| 15XF | 6117 | - | - | - | - | - | - |
| 15CM | A 182 Güteklasse F12 A213 Güteklasse T12 A 335 Güteklasse P12 |
13CrMo-44 | - | - | - | - | - |
| 16К | A 414 Besoldungsgruppe E | H II St42−2 C22N ASt41 P 265 GH |
SG 295 SG 30 SM 53 B SM 53 C SPV 315 SPV 32 SPV 355 SPV 36 |
- | P 265 GH | Fe 410 KW P 265 GH |
- |
| 17GS | - | S355J2G3 / Fe 510 D1 St 52−3 St 52−3 / S355J2G3 St 52−3 G |
SM 490 A SM 520 C SM 53 C |
16Mn | - | Fe 510 Fe E 420 S 355 J 2 G 3 |
S 355 J 2 G 3 |
| 18CR | SA-29 Sorte 5115 | 16 MnCr 5 | - | 15CrMn 20CrMn |
527 M 17 590 H 17 590 M 17 |
16 MnCr 5 | 16 MC 5 16 MnCr 5 RR |
| 20 | C1020 A 105 Gr1 A 106 GrA, B A 659 CS Typ 1020 A 794 CS Typ 1020 |
C 22 C 22N C 22.3 Ck 22 St35.8 St45.8 |
S 20 C S 20CK |
- | 040A20 070 M 20 070 M 26 1 C 22 C 22 En3A En3B En3C En3D |
C 20 C 21 C 22 |
C 20 XC 25 |
| 20К | A 283-C A 285-A, B, c A 414 Klasse E A 515−5 A 515−60 A 515−70 |
H II P 265 GH |
SG 295 SG 30 SM 53 B SM 53 C SPV 315 SPV 32 SPV 355 SPV 36 |
- | P 265 GH | Fe 410 KW P 265 GH |
- |
| 20ps | A 29 1020 | - | SWRCH17R | ML20 | 0/4 | - | - |
| 20H2M 20HM |
4621 | - | - | - | - | - | - |
| 20X | 5120 | - | - | - | - | - | - |
| 20KHF | 6120 | 22CrV4 | - | - | - | - | - |
| 20Х13 | 420 A 276 420 A 580 420 |
X 20 Cr 13 | SUS 420J1 | 2Cr13 | 420 S 37 En56C |
X 20 Cr 13 | Z 20 C 13 |
| 20CR17NI2 | 431 A 493 431 A 580 431 SA-479 Typ 431 |
X17CrNi16−2 X17CrNi16−2 (X 20 CrNi 17 2) |
SUS 431 | 1Cr17Ni2 ML1Cr17Ni2 |
431 S 29 En57 |
X 16 CrNi 1 | Z 15 CN 16−02 Z 15 CN 16.02 CI |
| 20CR25NI20C2 | 310 314 |
X15CrNiSi25−20 X15CrNiSi25−21 |
SUS Y 310 | 2Cr25Ni20 | - | X 16 CrNiSi 25 20 | Z 15 CNS 25−20 |
| 20CRM | 4130 SA-29 Güte 4130 |
25 CrMo 4 GS-25 CrMo 4 |
SKM 420 SCM 430 |
ML30CrMo ML30CrMoA |
25 CrMo 4 | 25 CrMo 4 | 25 CrMo 4 |
| 20XH | 3120 | - | - | - | - | - | - |
| 22K | 1022 1518 |
20Mn5 | S Mn C 420 | - | 120M19 | - | 20M5 |
| 25 | C1025 | - | - | - | - | - | - |
| 25Г | 1025 A 108 1025 A 510 1025 A 512 1025 A 513 1025 A 576 1025 |
GS-Ck 25 | S 25 C | 25 25Z ZG230−450 (ZG 25) |
070 M 26 080 A 25 |
- | - |
| 25X1MF | A 193 B14 A 540 B21 |
24CrMoV55 | - | - | - | - | - |
| 30 | C1030 A 29 1030 SA-29 1030 |
- | SWRCH30K SWRCH33K |
ML25Mn ML30 |
1/1 | - | - |
| 30X | 5130 | - | - | - | - | - | - |
| 30XM | 4130 A 302 Gr B A 304 |
25CrMo4 | - | - | - | - | - |
| 30KH13 | 420F | X30Cr13 | SUS 420J2 | 3Cr13 | 420 S 45 En56D |
G X 30 Cr 13 X 30 Cr 13 |
Z 30 C 13 Z 33 C 13 |
| 30CRM | - | 34 CrMo 4 GS-34 CrMo 4 |
SCM 435 SCM 435 H |
35CrMo | 34 CrMo 4 | 34 CrMo 4 | 34 CrMo 4 |
| 30G2 | - | 36 Mn 5 | SCMn 3 SMn 438 SMn 438 H |
- | 150 M 36 En15 En15A |
- | 40 M 5 |
| 35 | C1035 C1034 A 107 |
C 35 Ck 35 |
S 35C | - | 080M36 | - | XC 38 |
| 35X | 5132 | 34Cr4 | - | - | - | - | - |
| 35XM | - | 34CrMo4 | - | - | - | - | - |
| 40 | 1040 | C40 Ck40 |
S 40C | - | 080A40 060A40 |
- | XC 42 |
| 40X | 5140 | 41 Cr 4 | S Gr 440 | - | 530A40 530M40 |
- | 42C4 |
| 40KH13 | - | X38Cr13 X39Cr13 X46Cr13 |
SUS 420J2 | - | 420S45 | X 40 Cr 14 X 46 Cr 13 |
Z 38 C 13 M Z 40 C 13 Z 40 C 14 Z 44 C 14 Z 50 C 14 |
| 40CR2H2MA | 4340 SA-29 Güte 4340 |
40 NiCrMo 6 | SNCM 439 STPT 38 |
40CrNiMoA ML40CrNiMoA |
818 M 40 | - | - |
| 40XH | 3135 3140 |
40Ni Cr 6 | - | - | 640M40 | - | - |
| 40CRNI2MA | 9840 | 36 CrNiMo 4 | - | - | 36 CrNiMo 4 | 36 CrNiMo 4 | 36 CrNiMo 4 40 NCD 3 |
| 45 | 1045 A 107 A 29 1044 SA-29 1044 |
C 45 Ck 45 Cq 45 |
S 45C SWRCH45K |
ML45 | 080M 080M46 |
- | XC48 |
| 45Г | 1045 A 108 1045 A 29 1045 A 311 1045 A 576 1045 SA-29 1045 SA-311 1045 |
C45E Ck 45 GS-Ck 45 |
S 45 C S 48 C |
45 ZG310−570 (ZG 45) |
C 45 E | C 45 E | C 45 E XC 45 |
| 45X | 5145 | - | - | - | - | - | - |
| 50 | С1050 A 108 1050 A 29 1050 A 311 1050 A 510 1050 A 576 1050 SA-29 1050 SA-311 1050 |
C 50 E Ck 50 |
- | 50 | 080 M 50 C 50 E |
C 50 E | C 50 E XC 50 |
| 50X | 5147 | - | - | - | - | - | - |
| 55 | С1055 A 29 1055 A 576 1055 SA-29 1055 |
C 55 Ck 53 |
S 55 C S 55 C-CSP |
- | 070 M 55 C 55 En9 En9K |
C 55 | AF 70 C 54 C 55 |
| 60 60Г |
C1060 A 29 1060 A 576 1060 SA-29 1060 |
C 60 | S 58 C S 60 C-CSP S 65 C-CSP |
- | 060 A 62 C 60 CS 60 HS 60 |
C 60 | C 60 |
| St0 St1kn |
A 283 Güteklasse A | S185 / Fe 310−0 St 33 |
SS 330 | Q195 Q195-F Q195-Z Q195-b |
HR 15 | S 185 | - |
| St2ps St2sp |
A53 Gr A A192 Gr A |
St 35 | - | Q215B Q215B-F Q215B-Z Q215B-b |
S360 | - | - |
| St3kn | A 107 A 283 Güteklasse C SA-283 C |
USt 37−2 USt 37−2 G RSt37−2 |
- | A3 Q235A Q235A-F Q235A-Z Q235A-b |
- | - | - |
| St3sp | A 414 Güteklasse A A 570 Sorte 36 |
S235J2G3 / Fe 360 D1 St 37−3 St 37−3 G UZSt 37−2 |
SS34 | - | HS 37/23 S 235 J 2 G 3 40C BS4360 |
S 235 J 2 G 3 | S 235 J 2 G 3 E 24−2NE |
| St5sp | A 570 Güteklasse 50 | St 50−2 | SS 50 | - | - | - | А 50−2 |
| St6ps St6sp |
A 572 Güteklasse 65 | E335 / Fe 590−2 St 60−2 St 60−2 G |
SM 570 SM 58 |
- | 55 C E 335 |
E 335 Fe 590 |
E 335 |
Quelle: gosts.org
| Stahlsorte GUS-Länder GOST | Euronorm-Stahlsorte | Stahlsorte Euronormen | US-Entsprechung |
|---|---|---|---|
| 10 | C10E | 1.1121 | 1010 |
| 10XHH1 | 10 XHN1 | 1.5805 | - |
| 14 CRH3 M | 14 NiCrMo1−3-4 | 1.6657 | 9310 |
| 15 | C15 E | 1.1141 | 1015 |
| 15 Г | C16 E | 1.1148 | 1016 |
| 16 CH | 16 MnCr5 | 1.7131 | 5115 |
| 16XGR | 16Mn CrB5 | 1.7160 | - |
| 16 CHN | 16NiCr4 | 1.5714 | - |
| 17 G1 C | S235J2G4 | 1.0117 | - |
| 17 CH3 | 15NiCr13 | 1.5752 | Е3310 |
| 18 CGM | 18CrMo4 | 1.7243 | 4120 |
| 18 X2 H2 M | 18CrNiMo7−6 | 1.6587 | - |
| 20 | C22E | 1.1151 | 1020 |
| 20 XM | 20MoCr3 | 1.7320 | 4118 |
| 20CRNIM | 20MoCr2−2 | 1.6523 | 8617 |
| 25 | C25E | 1.1158 | 1025 |
| 25 XM | 25CrMo4 | 1.7218 | 4130 |
| 28 Г | 28Mn6 | 1.1170 | 1330 |
| 30 | C30E | 1.1178 | 1030 |
| 34 Х | 34Cr4 | 1.7033 | 5130 |
| 34 X2 H2 M | 34CrNiMo6 | 1.6582 | 4340 |
| 35 | C35E | 1.1181 | 1035 |
| 36 CNM | 36CrNiMo4 | 1.6511 | 9840 |
| 36 X2 H4 MA | 36NiCrMo16 | 1.6773 | - |
| 40 | C40E | 1.1186 | 1040 |
| 42 XM | 42CrMo4 | 1.7225 | 4140 |
| 45 | C45E | 1.1191 | 1045 |
| 46 Х | 46Cr2 | 1.7006 | 5045 |
| 50 | C50E | 1.1206 | 1050 |
| 50 CGF | 50CrV4 | 1.8159 | 6150 |
Quelle: metaltrade.ru
| Stahlsorte GUS-Länder GOST | Stahlsorte Euronormen | Stahlsorte Euronormen | Entsprechungen in US-Normen |
|---|---|---|---|
| 10 X2 M | 10CrMo9−10 | 1.7380 | F22 |
| 13 XM | 13CrMo4−4 | 1.7335 | F12 |
| 14 XMF | 14MoV6−3 | 1.7715 | - |
| 15 М | 15Mo3 | 1.5415 | F1 |
| 17 Г | 17Mn4 | 1.0481 | - |
| 20 | C22.8 | 1.0460 | - |
| 20 Г | 20Mn5 | 1.1133 | - |
| 20 X11 MNF | X20CrMoV12−1 | 1.4922 | - |
Quelle: metaltrade.ru
| GUS-Länder (GOST 1050−88) | Deutschland (DIN) Ausländische Entsprechungen | Deutschland (DIN) Ausländische Entsprechungen | USA (ASTM) |
|---|---|---|---|
| 10 | 1.0301 | C 10/Sc 10 | 1010 |
| 15 | 1.0401 | C15/Sc 15 | 1015 |
| 20 | 1.0402 | C 22/Sq 22 | 1020 |
| 30 | - | - | 1030 |
| 35 | 1.0501 | C 35/Ck 35 | 1035 |
| 40 | 1.0511 | C 40/Sk 40 | 1040 |
| 45 | 1.0503 | C 45/Sk 45 | 1045 |
| 50 | 1.0540 | C 50/Quadrat 50 | 1050 |
| 55 | 1.0535 | C 55/Quadrat 55 | 1055 |
| 60 | 1.0601 | C 60/Quadrat 60 | 1060 |
Quelle: metallopt.ru
| GUS-Länder (GOST, TU) | Deutschland (DIN) Ausländische Analoga | Deutschland (DIN) Ausländische Analoge | USA (ASTM) |
|---|---|---|---|
| 12XH3A | 1.5732 | 14NiCr10 | - |
| 12CR4A | Е3310 | ||
| 15CRM | 1.7335 | 13CrMo44 | - |
| 17G1S | 1.0570 | St52−3 | - |
| 18CR | 1.7131 | 16MnCr5 | 5120 |
| 20CR | 1.7218 | 25CrMo4 | 4130 |
| 27CRMO4 | 1.5526 | 30MnB4 | - |
| 30CR3MOV | 1.8519 | 31CrMoV9V | - |
| 30CR2H2M | 1.6580 | 30CrNiMo8V | - |
| 34CR2NIMO8V | 1.8550 | 34CrAlNi7V | - |
| 38CR2H2MA | 1.6582 | 34CrNiMo6 | 4330 |
| 40Х | 1.7045 | 42Cr4 | 5140 |
| 40CRM | 1.7225 | 42CrMo4 | 4140 |
| 40CRNI2MA | 1.6565 | 40NiCrMo6 | 4340 |
| 40CRNINM | 1.6546 | 40NiCrMo22 | 8640 |
| 45Г | 1.0912 | 46Mn7 | - |
Quelle: metallopt.ru
| Stahlsorte GUS-Länder GOST | Stahlsorte Euronormen | Stahlsorte Euronormen | Entsprechungen in US-Normen |
|---|---|---|---|
| SHC4 | 100Cr2 | 1.3501 | 50 100 |
| 30 30CR15 | 100Cr6 | 1.3505 | 52 100 |
| SHCR15 SG | 100CrMn6 | 1.3520 | A 485 (2) |
| 485 (2) Ø ØCR20 M | 100CrMo7 | 1.3537 | A 485 (3) |
Quelle: metaltrade.ru
| Stahlsorte GUS-Länder GOST | Euronorm-Stahlsorte | Stahlsorte Euronormen | Entsprechungen in US-Normen |
|---|---|---|---|
| 38C2A | 38Si7 | 1.5023 | - |
| 50CRVA | 50CrV4 | 1.8159 | 6150 |
| 52 CGMFA | 51CrMoV4 | 1.7701 | - |
| 55 CR2A | 54SICr6 | 1.7102 | - |
| 55 CGA | 55Cr3 | 1.7176 | 5147 |
| 60 C2 CGA | 60SiCR7 | 1.7108 | 9262 |
Quelle: metaltrade.ru
| GUS-Länder (GOST, TU) | Deutschland (DIN) Ausländische Analoga | Deutschland (DIN) Ausländische Entsprechungen | USA (ASTM) |
|---|---|---|---|
| 70 | 1.1231 | Ck 67 | 1070 |
| 75 | 1.0605 | C 75 | 1074 |
| 85 | 1.1269 | Ck 85 | 1086 |
| 50CFA | 1.8159 | 50CrV4 | 6150 |
| 55С2 | 1.5026 | 55Si7 | - |
| 60Г | 1.0601 | С 60 | 1060 |
| 60C2 | 1.5027 | 60Si7 | 9260 |
| 60C2GH | 1.5092 | 60SiCr7 | 9262 |
| 70C2X | 1.5029 | 71Si 7 | - |
Quelle: metallopt.ru
| GUS-Länder (GOST, TU) | Deutschland (DIN) Ausländische Analoga | Deutschland (DIN) Ausländische Entsprechungen | USA (ASTM) |
|---|---|---|---|
| У 7 | 1.1620 | C 70W2 | - |
| U 7A | 1.1520 | C 70W1 | - |
| У 8 | 1.1625 | C 80W2 | - |
| U 8A | 1.1525 | C 80W1 | W 108 |
| У 10 | 1.1645 | C 105W2 | - |
| W 10A | 1.1545 | C 105W1 | W 110 |
| У 11 | 1.1654 | C 110W | - |
| У 13 | 1.1663 | C 125W | W 112 |
Quelle: metallopt.ru
| GUS-Länder (GOST, TU) | Deutschland (DIN/BOHLER) Ausländische Entsprechungen | Deutschland (DIN/BOHLER) Ausländische Entsprechungen | USA (AISI/ASTM) |
|---|---|---|---|
| Х12 | 1.2080 | X210Cr12 | D3 |
| X12B | 1.2436 | X210CrW12 | - |
| X12MF* | 1.2379 | X155CrVMo12−1 | D2 |
| X12MF4-MP | - | K190RM | - |
| 95CRF | 1.2210 | 115CrV 3 | L2 |
| 9X1F | 1.2067 | 102Cr 6 | L3 |
| 9G2F | 1.2842 | 90MnCrV 8 | O2 |
| 95CRVF | 1.2510 | 100MnCrW 4 | O1 |
| 3CR3B9F | 1.2581 | X30WCrV9−3 | H21 |
| 95CR5GM | 1.2363 | X100CrMoV5−1 | А2 |
| 95CRM | 1.2303 | 100CrMo 5 | L7 |
| 95Х18 | 1.4125 | X105CrMo17 | A473 (440C) |
| 5CRNIMO | 1.2713 | 55NiCrMoV 6 | L6 |
| 5CR2SF | 1.2550 | 60WCrV 7 | S1 |
| 5CR3MO2F | - | - | S7 |
| 5CRNI2MOV | 1.2714 | 56NiCrMoV 7 | - |
| 3CR3M3F | 1.2365 | X32CrMoV3 3 | H10 |
| 4X5MFS | 1.2343 | X38CrMoV5−1 | H11 |
| 4X5MF1C | 1.2344 | X40CrMoV5−1 | H13 |
*mögliche Herstellung durch Pulvermetallurgieverfahren
Quelle: metallopt.ru
| Stahlsorte GUS-Länder GOST | Stahlsorte Euronormen | Stahlsorte Euronormen | Analogien in US-Normen |
|---|---|---|---|
| P0 M2 SF10-MP | - | - | А11 |
| R2 M9-MP | S2−9-2 | 1.3348 | М7 |
| R2 M10 K8-MP | S2−10−1-8 | 1.3247 | М42 |
| R6 M5-MP | S6−5-2 | 1.3343 | М2 |
| R6 M5 K5-MP | S6−5-2−5 | 1.3243 | - |
| R6 M5 F3-MP | S6−5-3 | 1.3344 | М3 |
| P6 M5 F4-MP | - | - | М4 |
| R6 M5 F3 K8-MP | - | - | М36 |
| R10 M4 F3 K10-PP | S10−4-3−10 | 1.3207 | - |
| R6 M5 F3 K9-MP | - | - | М48 |
| R12 M6 F5-MP | - | - | М61 |
| R12 F4 K5-MP | S12−1-4−5 | 1.3202 | - |
| R12 F5 K5-MP | - | - | Т15 |
| R18-MP | - | - | Т1 |
Quelle: metaltrade.ru
| GUS-Länder (GOST, TU) | Deutschland (DIN) | BOHLER (D-016) | USA (AISI/ASTM) |
|---|---|---|---|
| R18* | 1.3355 | S 200 | Т 1 |
| R6M5* | 1.3343 | S600/S601 | М 2 |
| R6M5K5* | 1.3243 | S 705 | - |
| R6M5F3-MP | 1.3342/1.3344 | S 790PM | М 3 |
| R6M5F4-MP | - | S 690PM | М 4 |
| R6M5F3K8-MP | - | S 590PM | М 36 |
| R10M2F5K8-MP | - | S 390PM | - |
| R10M3F4K8-MP | - | - | - |
| R12F3 | 1.3318 | - | - |
| R12MF4-MP | - | S 207PM | - |
| R12K5F4-MP | - | S 308PM | - |
| R12M6F5-MP | - | - | М 61 |
| R12MF5K5-MP | 1.3202 | - | Т 15 |
| R0M2SF10-MP | - | CPM 10V | А 11 |
* Herstellung nach dem pulvermetallurgischen Verfahren ist möglich
Quelle: metallopt.ru
| GUS-Länder (GOST) | Analog | Land Standard |
|---|---|---|
| 20GL | A352 Gr LCC | USA, ASTM A352 |
| 20GL | A757 Gr A2Q | USA, ASTM A757 |
| 20GL | A216 Gr WCC | USA, ASTM A216 |
| 30GSL | A304 (1330H) | USA, ASTM A304 |
| 30GSL | A322 (1330) | 1330H USA, ASTM A322 |
| 20Л | A732 (1A) | 1A USA, ASTM A732 |
| 25Л | A352 Gr LCA | 20L (1A) ASTM A732 (1A) USA, ASTM A352 |
| 25Л | A732 (2A) | 2A USA, ASTM A732 |
| 25Л | A216 Gr WCB | USA, ASTM A216 |
| 30Л | A352 Gr LCB | USA, ASTM A352 |
| 30Л | A216 Gr WCB | USA, ASTM A216 |
| 35Л | A356 Gr1 | USA, ASTM A356 |
| 40Л | A732 (3A) | USA, ASTM A732 |
Quelle: www. td-ksz.com
| GUS-Länder (GOST) | Analog | Land Norm |
|---|---|---|
| 20GL | 1.1120 | Deutschland, DIN 17 182 |
| 30GSL | 1.1165 | Deutschland, DIN 17 205 |
| 15Л | 1.0420 | Deutschland, DIN 1681 |
| 20Л | 1.0619 | Deutschland, DIN EN 10 213−2 |
| 25Л | 1.0446 | Deutschland, DIN 1681 |
| 35Л | 1.0552 | Deutschland, DIN 1681 |
| 45Л | 1.0558 | Deutschland, DIN 1681 |
Quelle: www. td-ksz.com
| GUS-Länder (GOST) | Kurzbezeichnung | Land Norm |
|---|---|---|
| 30GSL | AO35 MnSi5 | Ungarn, MSZ 8272 |
| 30GSL | 30 GSL | Bulgarien, BDS 6550 |
| 30GSL | T30 Si Mn12 | Rumänien, STAS 1773 |
| 15Л | 15LII | Bulgarien, BDS3492 |
| 15Л | AM1 | BRITANNIEN, B.S.3100 (91) |
| 15Л | Ao 400 FK | Ungarn, MSZ 8276 |
| 15Л | L II 400 | Polen, PN/H 83 152 |
| 15Л | OT 400−3 | Rumänien, STAS 600 |
| 15Л | 422 630 | Tschechische Republik, Slowakei, CSN 422 630 |
| 25Л | 161 Grad 430 | Großbritannien, B.S. 1504 (76) |
| 25Л | 25 LII | Bulgarien, BDS 3492 |
| 25Л | Ao 450 FK | Ungarn, MSZ 8276 |
| 25Л | OT 450−3 | Rumänien, STAS 600 |
| 25Л | 25LI | Bulgarien, BDS 3492 |
| 25Л | 422 640 | Tschechische Republik, Slowakei, CSN 422 640 |
| 25Л | L 450 | Polen, PN/H 83 152 |
| 30Л | 1505 | Schweden, SS |
| 35Л | 35LII | Bulgarien, BDS 3492 |
| 35Л | A2 | BRITANNIEN, B.S.3100 (91) |
| 35Л | Ao 500 FK | Ungarn, MSZ 8276 |
| 35Л | L500 | Polen, PN/H8 3152 |
| 35Л | OT 500−1 | Rumänien, STAS 600 |
| 35Л | 35LI | Bulgarien, BDS3492 |
| 35Л | 422 650 | Tschechische Republik, Slowakei, CSH 422 650 |
| 35Л | G-30−57 | Finnland, SFS 350 |
| 35Л | SCC | Japan, JIS G5111 (91) |
| 40Л | 35LI | Bulgarien, BDS 3492 |
| 40Л | OT 550−1 | Rumänien, STAS 600 |
| 40Л | CLA1 Klasse C | UK, B.S. 3146 Teil 1 (74) |
| 40Л | CLA8 Grad C | UK, B.S. 3146 Teil 1 (74) |
| 40Л | G-30−57 | Finnland, SFS 350 |
| 45Л | 45LI | Bulgarien, BDS 3492 |
| 45Л | A3 | BRITANNIEN, B.S.3100 (91) |
| 45Л | Ao550FK | Ungarn, MSZ 8276 |
Quelle: www. td-ksz.com
| Europa (EN) | Deutschland (DIN) | USA (AISI) | Japan (JIS) | GUS (GOST) |
|---|---|---|---|---|
| 1.4713 | X10CrAl7 | 10CR17CU | ||
| 1.4724 | X10CrAl13 | 405 | 10CR13CU | |
| 1.4742 | X10CrAl18 | 442 | ||
| 1.4762 | X10CrAl24 | 446 | ||
| 1.4878 | X12CrNiTi18−9 | 321 H | 12X18H10T | |
| 1.4828 | X15CrNiSi20−12 | 309 | 20X20H14C2 | |
| 1.4845 | X12CrNi25−21 | 310 S | 20CR23NI18 | |
| 1.4841 | X15CrNiSi25−20 | 314 | 20CR25H20C2 |
Quelle: www.uvis.ua
| Europa (EN) | Deutschland (DIN) | USA (AISI) | Japan (JIS) | GUS (GOST) |
|---|---|---|---|---|
| 1.4003 | X2CrNi12 | |||
| 1.4512 | X2CrTi12 | 409 | SUH 409 | |
| 1.4000 | X6Cr13 | 410S | SUS 410 S | 08KH13 |
| 1.4002 | X6CrAl13 | 405 | SUS 405 | |
| 1.4006 | X12CrN13 | 410 | SUS 410 | 12KH13 |
| 1.4024 | X15Cr13 | (410) | SUS 410 J1 | |
| 1.4021 | X20Cr13 | (420) | SUS 420 J1 | 20Х13 |
| 1.4028 | X30Cr13 | (420) | SUS 420 J2 | 30KH13 |
| 1.4031 | X39Cr13 | SUS 420 J2 | 40KH13 | |
| 1.4034 | X46Cr13 | (420) | 40KH13 | |
| 1.4016 | X6Cr17 | 430 | SUS 430 | 12Х17 |
| 1.4520 | X2CrTi17 | |||
| 1.4510 | X3CrTi17 | 439 | SUS 430 LX | 08CR17TI |
| 1.4113 | X6CrMo17−1 | 434 | SUS 434 | |
| 1.4509 | X2CrTiNb18 | 441 | ||
| 1.4521 | X2CrMoTi18−2 | 444 | SUS 444 | |
| 1.4589 | X5CrNiMoTi15−2 | |||
| 1.4310 | X10CrNi18−8 | (301) | SUS 301 | |
| 1.4318 | X2CrNiN18−7 | 301 LN | SUS 301 LN | |
| 1.4301 | X5CrNI18−10 | 304 | SUS 304 | 08CR18NI10 |
| 1.4303 | X4CrNi18−12 | (305) | SUS 305 | 12X18H12 |
| 1.4306 | X2CrNi19−11 | 304 L | SUS 304 L | 03CR18NI11 |
| 1.4541 | X6CrNiTi18−10 | 321 | SUS 321 | 08CR18NITI10T |
| 1.4550 | X6CrNiNb18−10 | 347 | SUS 347 | |
| 1.4401 | X5CrNiMo17−12−2 | 316 | SUS 316 | |
| 1.4404 | X2CrNiMo17−12−2 | 316 L | SUS 316 L | |
| 1.4571 | X6CrNiMoTi17−12−2 | 316 Ti | SUS 316 Ti | 10X17H13M2T |
| 1.4561 | X1CrNiMoTi18−13−2 | |||
| 1.4435 | X2CrNiMo18−14−3 | 316 L | SUS 316 L | 03CR17H14M2 |
| 1.4439 | X2CrNiMoN17−13−5 | S 31 726 | SUS 317 | |
| 1.4539 | X1NiCrMoCu25−20−5 | N 8 904 | ||
| 1.4565 | X3CrNiMnMoNbN 23−17−5-3 | S 34 565 | ||
| 1.4462 | X2CrNiMoN22−5-3 | S 31 803 | SUS 329 J3L | |
| Europa (EN) | Deutschland (DIN) | USA (AISI) | Japan (JIS) | GUS (GOST) |
Quelle: www.uvis.ua
| GUS (GOST) | Euronormen (EN) | Deutschland (DIN) | USA (AISI) |
|---|---|---|---|
| 03 X17 H13 M2 | 1.4404 | X2 CrNiMo 17−12−2 | 316 L |
| 03 X17 H14 M3 | 1.4435 | X2 CrNiMo 18−4-3 | - |
| 03 X18 H11 | 1.4306 | X2 CrNi 19−11 | 304 L |
| 03 X18 H10 T-U | 1.4541-MOD | - | - |
| 06 CHN28-MDT | 1.4503 | X3 NiCrCuMoTi 27−23 | - |
| 06 X18 H11 | 1.4303 | X4 CrNi 18−11 | 305 L |
| 08 X12 T1 | 1.4512 | X6 CrTi 12 | 409 |
| 08 Х13 | 1.4000 | X6 Cr 13 | 410S |
| 08 CR17 H13 M2 | 1.4436 | X5CrNiMo 17−13−3 | 316 |
| 08 X17 H13 M2 T | 1.4571 | X6 CrNiMoTi 17−12−2 | 316Ti |
| 08 CR17 T | 1.4510 | X6 CrTi 17 | 430Ti |
| 08 X18 H10 | 1.4301 | X5 CrNi 18−10 | 304 |
| 08 CR18 H12 T | 1.4541 | X6 CrNiTi 18−10 | 321 |
| 10 X23 H18 | 1.4842 | X12 CrNi 25−20 | 310S |
| 10X13 | 1.4006 | X10 Cr13 | 410 |
| 12 X18 H10 T | 1.4878 | X12 CrNiTi 18−9 | - |
| 12 X18 H9 | - | - | 302 |
| 15 X5 M | 1.7362 | X12 CrCo 5 | 501 |
| 15 X25 T | 1.4746 | X8 CrTi 25 | - |
| 20X13 | 1.4021 | X20 Cr 13 | 420 |
| 20 X17 H2 | 1.4057 | X20 CrNi 17−2 | 431 |
| 20 X23 H13 | 1.4833 | X7 CrNi 23−14 | 309 |
| 20 X23 H18 | 1.4843 | X16 CrNi 25−20 | 310 |
| 20 X25 H20 C2 | 1.4841 | X56 CrNiSi 25−20 | 314 |
| 03 X18 AH11 | 1.4311 | X2 CrNiN 18−10 | 304LN |
| 03 X19 H13 M3 | 1.4438 | X2 18−5-4 | 317L |
| 03 X23 H6 | 1.4362 | X2 CrNiN 23−4 | - |
| 02 X18 M2 BT | 1.4521 | X2 CrMoTi 18−2 | 444 |
| 02 X28 H30 MDB | 1.4563 | X1 NiCrMoCu 31−27−4 | - |
| 03 X17 H13 AM3 | 1.4429 | X2 CrNiMoN 17−13−3 | 316LN |
| 03 X22 H5 AM2 | 1.4462 | X2 CrNiMoN 22−5-3 | - |
| 03 X24 N13 G2 C | 1.4332 | X2 CrNi 24−12 | 309L |
| 08 X16 N13 M2 B | 1.4580 | X1 CrNiMoNb 17−12−2 | 316 Cd |
| 08 CR18 H12 B | 1.4550 | X6 CrNiNb 18−10 | 347 |
| 08 CRNINB 18−10 347 CD 08 X18 H12 B 1 4550 X6 CRNINB 18−10 347 | 1.4583 X10 CrNiMoNb | X10 CrNiMoNb 18−12 | 318 |
| 08X19AH9 | - | - | 304N |
| 08X19H13M3 | 1.4449 | X5 CrNiMo 17−13 | 317 |
| 08X20H11 | 1.4331 | X2 CrNi 21−10 | 308 |
| 08X20H20TU | 1.4847 | X8 CrNiAlTi 20−20 | 334 |
| 08X25H4M2 | 1.4460 | X3 CrnImOn 27−5-2 | 329 |
| 08X23H13 | - | - | 309S |
| 09X17H7U | 1.4568 | X7 CrNiAl 17−7 | 631 |
| 1X16H13M2 B | 1.4580 | X6 CrNiMoNb 17−12−2 | 316Cd |
| 10X13 EDELSTAHL | 1.4724 | X10 CrAlSi 13 | 405 |
| 12X15 | 1.4001 | X7 Cr 14 | 429 |
| 12X17 | 1.4016 | X6 Cr17 | 430 |
| 12X17M | 1.4113 | X6 CrMo 17−1 | 434 |
| 12X17MB | 1.4522 | X2 CrMoNb | 436 |
| 12X18H12 | 1.3955 | GX12 CrNi 18−11 | 305 |
| 12X17 G9 AH4 | 1.4373 | X12 CrMnNiN 18−9-5 | 202 |
| 15X9M | 1.7386 | X12 CrMo 9−1 | 504 |
| 15X12 | - | - | 403 |
| 15X13H2 | - | - | 414 |
| 15X17H7 | 1.4310 | X12 CrNi 17−7 | 301 |
| Legierungssorte nach GOST 1583−93 | Europäische Norm | USA | Japan | Frankreich | Italien | Vereinigtes Königreich |
|---|---|---|---|---|---|---|
| EN 1676 | ASTM, B179, B26, B85, AA, SAE | JIS, H5202, H2211, H2118 | NFA57−702 | UN14514 | BS14 | |
| AK8 (AL34) |
ENAB-42 100 (ENAB AlSi7Mg0,3) |
358.0 356.2 (A03562) |
AC4C.1 | A-S7G | - | - |
| AK7 | ENAB-42 000 (ENAB AlSi7Mg) |
357.0 356.1 (A03561) |
AC4C.1 | - | AlSi7Mg | - |
| AK7h (AL9) |
ENAB-42 000 (ENAB AlSi7Mg) |
356.0 356.1 (A03561) SG70A |
AC4C.1 | A-S7GU3 | AlSi7MgTi | LM2 |
| AK7pch (AL9−1) |
ENAB-42 100 (ENAB AlSi7Mg0,3) |
356.2 (A03562) |
AC4C.2 | A-S7G | AlSi7Mg | - |
| AK12 (AL2) |
ENAB-44 100 (ENAB AlSi12 (b)) |
A413.1 (A4131) |
AC3C.1 | A-S12G A-S13 |
G-Al-Si13 | LM6 |
Quelle: www. aluminium-union.ru
| GUS, GOST | USA AISI, ASTM, ASME |
Deutschland DIN |
Japan JIS |
China GB UK |
UK B.S. |
Italien UNI |
Frankreich AFNOR NF |
|---|---|---|---|---|---|---|---|
| 03CR17H14M3 | 316L SA-240TP316L |
X2CrNiMo18−14−3 | SUS 316L | 00Cr17Ni14Mo2 00Cr17Ni14Mo3 |
316S13 LW 22 |
X2CrNiMo 18−14−3 X2CrNiMo1713KG |
Z 3 CND 17−12−03 |
| 03X18H11 | 304 L SA-240TP304L |
X2 Cr Ni 19−11 GX2 Cr Ni 19−11 |
SUS304 L | - | 304S11 LW 20 LWCF 20 S 536 304 C12 (LT 196) 305 S 11 |
X2 CrNi 18 11 X 3 CrNi 18 11 GX 2 CrNi 19 10 |
Z 1 CN 18−12 Z 2 CN 18−10 Z 3 CN 19−10M Z 3 CN 18−10 Z 3 CN 19−11 Z 3 CN 19−11FF |
| 03CRNI28MDT 06CR28MDT |
- | X3NiCrCuMoTi2730 | - | - | - | - | - |
| 06X18H11 | 305 3008 |
X4CrNi18−12 | SUS 305 SUS 305J1 |
- | 305S17 305S19 |
X7 CrNi18 10 X8 CrNi 19 10 |
Z 5 CN 18−11FF |
| 07C16H6 | 301 A 167 301 A 240 301 A 666 301 |
X12CrNi17−7 X10CrNi18−8 |
SUS 301 | - | 301 S 21 301 S 22 Cr Ni 17/7 |
X10CrNi18−8 X12CrNi17−07 |
Z 11 CN 17−08 Z 11 CN 18−08 Z 12 CN 18−09 |
| 08kp | A 622 | St 50−2 | SPHE | - | BS 1449 1 HR |
- | 3C |
| 08X13 | 403 409 410 S 429 SA-240 TP 410S |
X6 Cr 13 X7 Cr 14 |
SUS 403 SUS 410S SUS429 |
- | 403 S17 | X6 Cr 13 | Z6 C13 Z8 C12 Z8 C13FF |
| 08X17H13M2T 10X17H13M2T |
316 Ti A 167 316Ti A 213 F316H A 240 316Ti A 368 316Ti SA-240 TP 316Ti SA-479 316Ti |
X6CrNiMoTi 12 122 X 10 CrNiMoTi 18−12 |
SUS 316Ti | 0Cr18Ni12Mo3Ti 1Cr18Ni12Mo3Ti |
320 S 33 CrNiMo 17/12/2 ¼ Ti |
X 6 CrNiMoTi 17 13 | Z6 CNDT 17.12 |
| 08CRNI17TI | 430Ti 439 |
X 6 CrTi 17 X3CrTi 17 |
SUS 430LX | - | - | X 3 CrTi 17 X 6 CrTi 17 |
Z 4 CT 17 |
| 08X18H10 | 304 304 H SA-240 TP 304 |
X5 Cr Ni 18 10 | SUS 304 | - | 304S11 304S15 304S16 304S17 304S31 LW21 LWCF 21 |
X 5 Cr Ni 18 10 | Z4 CN 19−10 FF Z5 CN 17−06 Z6CN 18.09 Z7 CN 18−09 |
| 08CR18NI12B | 347 A 167 347 A 240 347 A 313 347 A 580 347 |
X 6 CrNiNb 18 10 X6CrNiNb 18−10 |
SUS 347 | 0Cr18Ni11Nb 1Cr18Ni11Nb 1Cr19Ni11Nb |
347 S 20 347 S 31 ANC 3 Güteklasse B CrNi 18/9/Nb CrNi 18/9 0,10C/Nb |
X 6 CrNiNb 18 11 | Z 6 CNNb 18−10 |
| 08 SA | A 620 | DC 04 DC04 + ZE Fe P04 / St 14 St 14 St 4 |
SPCE | - | DC 04 / FeP 04 HR 1 HR 2 |
DC 04 / FeP 04 | DC 04 / FeP 04 |
| 09G2S | A 516−55 A 516−60 A 516−65 A 561 Gr70 |
- | SM41B SB49 |
- | - | - | - |
| 09CR17NI7U | - | X 7 CrNiAl 17 7 X7CrNiAl17−7 |
SUS 631 | 0Cr17Ni7Al | 301 S 81 | - | Z 9 CNA 17−07 |
| 10 | C1010 A 108 1010 A 29 M1010 A 510 1010 A 575 M1010 SA-29 M1010 |
C 10 C10E Ck 10 |
S 10 C S 9 CK SACM 1 |
10 | 040 A 10 045 M 10 En2A En32A HS 10 |
1 C 10 2 C 10 2 C 15 C 10 |
C 10 RR XC 10 |
| 10C13CU | A 268 TP405 | X10CrAl13 X10CrAlSi13 |
- | - | - | X 10 CrAl 12 | Z 13 C 13 |
| 10X23H18 20X23H18 |
SA-240 TP 310S | - | - | - | - | - | - |
| 12К | A 201 Gr AFx | ASt 35 | - | - | - | - | - |
| 12X13 15X13L |
410 430 A 183 F6 A 193 B6 A 479 410 |
X 10 Cr 13 X12 Cr13 GX 12 Cr 12 |
SUS 410 | - | 410C21 410S21 ANC 1A |
X 10 Cr13 X 12 Cr13 |
Z10C13 Z12C13 |
| 12Х17 | 430 A 182 F 430 A 240 430 SA-182 Güteklasse F 430 SA-240 Typ 430 |
X6Cr17 | SUS 430 | 1Cr15 1Cr17 ML1Cr17 |
17Cr 430S17 430S18 |
X 6 Cr 17 X 8 Cr 17 |
Z 8 C 17 |
| 12X18H10T 06X18H10T 08X18H10T 09CR18NI10T |
321 A 213 TP321H SA-240 TP 321 |
X6 Cr Ni Ti 18 10 X10 Cr Ni Ti 189 |
SUS 321 | - | 321S12 | - | Z6 CNT 18.10 |
| 12XM | A 182 Güteklasse F12 A213 Güteklasse T12 A 335 Güteklasse P12 A 387A, B, C |
13CrMo-44 | - | - | - | - | - |
| 12X2M | A 182 Güteklasse F22 A335 Güteklasse P22 387 Güteklasse D |
10CrMo910 | - | - | - | - | - |
| 12CR1MOV | - | 14MoV63 | - | - | - | - | - |
| 14Г2 | A414 Gr F, G A 515 Gr70 A516 Gr70 |
17 Mn4 | SB 46 SB 49 SG V 46 SG V 49 SP V 32 |
- | - | - | A 48CP |
| 15 | C1015 A 108 1015 A 512 1015 A 576 1015 |
C15 C15E Ck 15 |
S 15 C S 15 CK |
15 H15A ZG200−400 (ZG 15) |
- | - | C 18 RR XC 15 XC 18 |
| 15kp | A 621 FS Typ A A 621 FS Typ B |
DD 11 (StW 22) | SPHD | - | - | - | 1 C |
| 15Stück | A 29 1015 | QSt 38−3 | SWRCH15A SWRCH16R |
ML15 | - | CB 15 | - |
| 15H2M 15HM |
4615 | - | - | - | - | - | - |
| 15Х | - | 15Cr3 | - | - | - | - | - |
| 15X5M | A 182 Güteklasse F5 A 193 Güteklasse B5 |
- | - | - | - | - | - |
| 15X25T 15X28 |
A 268 TP446 | 10CrAl24 | - | - | - | - | - |
| 15XF | 6117 | - | - | - | - | - | - |
| 15CM | A 182 Güteklasse F12 A213 Güteklasse T12 A 335 Güteklasse P12 |
13CrMo-44 | - | - | - | - | - |
| 16К | A 414 Besoldungsgruppe E | H II St42−2 C22N ASt41 P 265 GH |
SG 295 SG 30 SM 53 B SM 53 C SPV 315 SPV 32 SPV 355 SPV 36 |
- | P 265 GH | Fe 410 KW P 265 GH |
- |
| 17GS | - | S355J2G3 / Fe 510 D1 St 52−3 St 52−3 / S355J2G3 St 52−3 G |
SM 490 A SM 520 C SM 53 C |
16Mn | - | Fe 510 Fe E 420 S 355 J 2 G 3 |
S 355 J 2 G 3 |
| 18CR | SA-29 Güte 5115 | 16 MnCr 5 | - | 15CrMn 20CrMn |
527 M 17 590 H 17 590 M 17 |
16 MnCr 5 | 16 MC 5 16 MnCr 5 RR |
| 20 | C1020 A 105 Gr1 A 106 GrA, B A 659 CS Typ 1020 A 794 CS Typ 1020 |
C 22 C 22N C 22.3 Ck 22 St35.8 St45.8 |
S 20 C S 20CK |
- | 040A20 070 M 20 070 M 26 1 C 22 C 22 En3A En3B En3C En3D |
C 20 C 21 C 22 |
C 20 XC 25 |
| 20К | A 283-C A 285-A, B, c A 414 Klasse E A 515−5 A 515−60 A 515−70 |
H II P 265 GH |
SG 295 SG 30 SM 53 B SM 53 C SPV 315 SPV 32 SPV 355 SPV 36 |
- | P 265 GH | Fe 410 KW P 265 GH |
- |
| 20ps | A 29 1020 | - | SWRCH17R | ML20 | 0/4 | - | - |
| 20H2M 20HM |
4621 | - | - | - | - | - | - |
| 20X | 5120 | - | - | - | - | - | - |
| 20KHF | 6120 | 22CrV4 | - | - | - | - | - |
| 20Х13 | 420 A 276 420 A 580 420 |
X 20 Cr 13 | SUS 420J1 | 2Cr13 | 420 S 37 En56C |
X 20 Cr 13 | Z 20 C 13 |
| 20CR17NI2 | 431 A 493 431 A 580 431 SA-479 Typ 431 |
X17CrNi16−2 X17CrNi16−2 (X 20 CrNi 17 2) |
SUS 431 | 1Cr17Ni2 ML1Cr17Ni2 |
431 S 29 En57 |
X 16 CrNi 1 | Z 15 CN 16−02 Z 15 CN 16.02 CI |
| 20CR25NI20C2 | 310 314 |
X15CrNiSi25−20 X15CrNiSi25−21 |
SUS Y 310 | 2Cr25Ni20 | - | X 16 CrNiSi 25 20 | Z 15 CNS 25−20 |
| 20CRM | 4130 SA-29 Güte 4130 |
25 CrMo 4 GS-25 CrMo 4 |
SKM 420 SCM 430 |
ML30CrMo ML30CrMoA |
25 CrMo 4 | 25 CrMo 4 | 25 CrMo 4 |
| 20XH | 3120 | - | - | - | - | - | - |
| 22K | 1022 1518 |
20Mn5 | S Mn C 420 | - | 120M19 | - | 20M5 |
| 25 | C1025 | - | - | - | - | - | - |
| 25Г | 1025 A 108 1025 A 510 1025 A 512 1025 A 513 1025 A 576 1025 |
GS-Ck 25 | S 25 C | 25 25Z ZG230−450 (ZG 25) |
070 M 26 080 A 25 |
- | - |
| 25X1MF | A 193 B14 A 540 B21 |
24CrMoV55 | - | - | - | - | - |
| 30 | C1030 A 29 1030 SA-29 1030 |
- | SWRCH30K SWRCH33K |
ML25Mn ML30 |
1/1 | - | - |
| 30X | 5130 | - | - | - | - | - | - |
| 30XM | 4130 A 302 Gr B A 304 |
25CrMo4 | - | - | - | - | - |
| 30KH13 | 420F | X30Cr13 | SUS 420J2 | 3Cr13 | 420 S 45 En56D |
G X 30 Cr 13 X 30 Cr 13 |
Z 30 C 13 Z 33 C 13 |
| 30CRM | - | 34 CrMo 4 GS-34 CrMo 4 |
SCM 435 SCM 435 H |
35CrMo | 34 CrMo 4 | 34 CrMo 4 | 34 CrMo 4 |
| 30G2 | - | 36 Mn 5 | SCMn 3 SMn 438 SMn 438 H |
- | 150 M 36 En15 En15A |
- | 40 M 5 |
| 35 | C1035 C1034 A 107 |
C 35 Ck 35 |
S 35C | - | 080M36 | - | XC 38 |
| 35X | 5132 | 34Cr4 | - | - | - | - | - |
| 35XM | - | 34CrMo4 | - | - | - | - | - |
| 40 | 1040 | C40 Ck40 |
S 40C | - | 080A40 060A40 |
- | XC 42 |
| 40X | 5140 | 41 Cr 4 | S Gr 440 | - | 530A40 530M40 |
- | 42C4 |
| 40KH13 | - | X38Cr13 X39Cr13 X46Cr13 |
SUS 420J2 | - | 420S45 | X 40 Cr 14 X 46 Cr 13 |
Z 38 C 13 M Z 40 C 13 Z 40 C 14 Z 44 C 14 Z 50 C 14 |
| 40CR2H2MA | 4340 SA-29 Güte 4340 |
40 NiCrMo 6 | SNCM 439 STPT 38 |
40CrNiMoA ML40CrNiMoA |
818 M 40 | - | - |
| 40XH | 3135 3140 |
40Ni Cr 6 | - | - | 640M40 | - | - |
| 40CRNI2MA | 9840 | 36 CrNiMo 4 | - | - | 36 CrNiMo 4 | 36 CrNiMo 4 | 36 CrNiMo 4 40 NCD 3 |
| 45 | 1045 A 107 A 29 1044 SA-29 1044 |
C 45 Ck 45 Cq 45 |
S 45C SWRCH45K |
ML45 | 080M 080M46 |
- | XC48 |
| 45Г | 1045 A 108 1045 A 29 1045 A 311 1045 A 576 1045 SA-29 1045 SA-311 1045 |
C45E Ck 45 GS-Ck 45 |
S 45 C S 48 C |
45 ZG310−570 (ZG 45) |
C 45 E | C 45 E | C 45 E XC 45 |
| 45X | 5145 | - | - | - | - | - | - |
| 50 | С1050 A 108 1050 A 29 1050 A 311 1050 A 510 1050 A 576 1050 SA-29 1050 SA-311 1050 |
C 50 E Ck 50 |
- | 50 | 080 M 50 C 50 E |
C 50 E | C 50 E XC 50 |
| 50X | 5147 | - | - | - | - | - | - |
| 55 | С1055 A 29 1055 A 576 1055 SA-29 1055 |
C 55 Ck 53 |
S 55 C S 55 C-CSP |
- | 070 M 55 C 55 En9 En9K |
C 55 | AF 70 C 54 C 55 |
| 60 60Г |
C1060 A 29 1060 A 576 1060 SA-29 1060 |
C 60 | S 58 C S 60 C-CSP S 65 C-CSP |
- | 060 A 62 C 60 CS 60 HS 60 |
C 60 | C 60 |
| St0 St1kn |
A 283 Güteklasse A | S185 / Fe 310−0 St 33 |
SS 330 | Q195 Q195-F Q195-Z Q195-b |
HR 15 | S 185 | - |
| St2ps St2sp |
A53 Gr A A192 Gr A |
St 35 | - | Q215B Q215B-F Q215B-Z Q215B-b |
S360 | - | - |
| St3kn | A 107 A 283 Güteklasse C SA-283 C |
USt 37−2 USt 37−2 G RSt37−2 |
- | A3 Q235A Q235A-F Q235A-Z Q235A-b |
- | - | - |
| St3sp | A 414 Güteklasse A A 570 Sorte 36 |
S235J2G3 / Fe 360 D1 St 37−3 St 37−3 G UZSt 37−2 |
SS34 | - | HS 37/23 S 235 J 2 G 3 40C BS4360 |
S 235 J 2 G 3 | S 235 J 2 G 3 E 24−2NE |
| St5sp | A 570 Güteklasse 50 | St 50−2 | SS 50 | - | - | - | А 50−2 |
| St6ps St6sp |
A 572 Güteklasse 65 | E335 / Fe 590−2 St 60−2 St 60−2 G |
SM 570 SM 58 |
- | 55 C E 335 |
E 335 Fe 590 |
E 335 |
Quelle: gosts.org
| Stahlsorte GUS-Länder GOST | Euronorm-Stahlsorte | Stahlsorte Euronormen | US-Entsprechung |
|---|---|---|---|
| 10 | C10E | 1.1121 | 1010 |
| 10XHH1 | 10 XHN1 | 1.5805 | - |
| 14 CRH3 M | 14 NiCrMo1−3-4 | 1.6657 | 9310 |
| 15 | C15 E | 1.1141 | 1015 |
| 15 Г | C16 E | 1.1148 | 1016 |
| 16 CH | 16 MnCr5 | 1.7131 | 5115 |
| 16XGR | 16Mn CrB5 | 1.7160 | - |
| 16 CHN | 16NiCr4 | 1.5714 | - |
| 17 G1 C | S235J2G4 | 1.0117 | - |
| 17 CH3 | 15NiCr13 | 1.5752 | Е3310 |
| 18 CGM | 18CrMo4 | 1.7243 | 4120 |
| 18 X2 H2 M | 18CrNiMo7−6 | 1.6587 | - |
| 20 | C22E | 1.1151 | 1020 |
| 20 XM | 20MoCr3 | 1.7320 | 4118 |
| 20CRNIM | 20MoCr2−2 | 1.6523 | 8617 |
| 25 | C25E | 1.1158 | 1025 |
| 25 XM | 25CrMo4 | 1.7218 | 4130 |
| 28 Г | 28Mn6 | 1.1170 | 1330 |
| 30 | C30E | 1.1178 | 1030 |
| 34 Х | 34Cr4 | 1.7033 | 5130 |
| 34 X2 H2 M | 34CrNiMo6 | 1.6582 | 4340 |
| 35 | C35E | 1.1181 | 1035 |
| 36 CNM | 36CrNiMo4 | 1.6511 | 9840 |
| 36 X2 H4 MA | 36NiCrMo16 | 1.6773 | - |
| 40 | C40E | 1.1186 | 1040 |
| 42 XM | 42CrMo4 | 1.7225 | 4140 |
| 45 | C45E | 1.1191 | 1045 |
| 46 Х | 46Cr2 | 1.7006 | 5045 |
| 50 | C50E | 1.1206 | 1050 |
| 50 CGF | 50CrV4 | 1.8159 | 6150 |
Quelle: metaltrade.ru
| Stahlsorte GUS-Länder GOST | Stahlsorte Euronormen | Stahlsorte Euronormen | Analogien in US-Normen |
|---|---|---|---|
| 10 X2 M | 10CrMo9−10 | 1.7380 | F22 |
| 13 XM | 13CrMo4−4 | 1.7335 | F12 |
| 14 XMF | 14MoV6−3 | 1.7715 | - |
| 15 М | 15Mo3 | 1.5415 | F1 |
| 17 Г | 17Mn4 | 1.0481 | - |
| 20 | C22.8 | 1.0460 | - |
| 20 Г | 20Mn5 | 1.1133 | - |
| 20 X11 MNF | X20CrMoV12−1 | 1.4922 | - |
Quelle: metaltrade.ru
| GUS-Länder (GOST 1050−88) | Deutschland (DIN) Ausländische Entsprechungen | Deutschland (DIN) Ausländische Entsprechungen | USA (ASTM) |
|---|---|---|---|
| 10 | 1.0301 | C 10/Sc 10 | 1010 |
| 15 | 1.0401 | C15/Sc 15 | 1015 |
| 20 | 1.0402 | C 22/Sq 22 | 1020 |
| 30 | - | - | 1030 |
| 35 | 1.0501 | C 35/Ck 35 | 1035 |
| 40 | 1.0511 | C 40/Sk 40 | 1040 |
| 45 | 1.0503 | C 45/Sk 45 | 1045 |
| 50 | 1.0540 | C 50/Quadrat 50 | 1050 |
| 55 | 1.0535 | C 55/Quadrat 55 | 1055 |
| 60 | 1.0601 | C 60/Quadrat 60 | 1060 |
Quelle: metallopt.ru
| GUS-Länder (GOST, TU) | Deutschland (DIN) Ausländische Analoga | Deutschland (DIN) Ausländische Analoge | USA (ASTM) |
|---|---|---|---|
| 12XH3A | 1.5732 | 14NiCr10 | - |
| 12CR4A | Е3310 | ||
| 15CRM | 1.7335 | 13CrMo44 | - |
| 17G1S | 1.0570 | St52−3 | - |
| 18CR | 1.7131 | 16MnCr5 | 5120 |
| 20CR | 1.7218 | 25CrMo4 | 4130 |
| 27CRMO4 | 1.5526 | 30MnB4 | - |
| 30CR3MOV | 1.8519 | 31CrMoV9V | - |
| 30CR2H2M | 1.6580 | 30CrNiMo8V | - |
| 34CR2NIMO8V | 1.8550 | 34CrAlNi7V | - |
| 38CR2H2MA | 1.6582 | 34CrNiMo6 | 4330 |
| 40Х | 1.7045 | 42Cr4 | 5140 |
| 40CRM | 1.7225 | 42CrMo4 | 4140 |
| 40CRNI2MA | 1.6565 | 40NiCrMo6 | 4340 |
| 40CRNINM | 1.6546 | 40NiCrMo22 | 8640 |
| 45Г | 1.0912 | 46Mn7 | - |
Quelle: metallopt.ru
| Stahlsorte GUS-Länder GOST | Stahlsorte Euronormen | Stahlsorte Euronormen | Entsprechungen in US-Normen |
|---|---|---|---|
| SHCR4 | 100Cr2 | 1.3501 | 50 100 |
| 30 30CR15 | 100Cr6 | 1.3505 | 52 100 |
| SHCR15 SG | 100CrMn6 | 1.3520 | A 485 (2) |
| 485 (2) Ø ØCR20 M | 100CrMo7 | 1.3537 | A 485 (3) |
Quelle: metaltrade.ru
| Stahlsorte GUS-Länder GOST | Euronorm-Stahlsorte | Euronorm-Stahlsorte | Entsprechungen in US-Normen |
|---|---|---|---|
| 38C2A | 38Si7 | 1.5023 | - |
| 50CRVA | 50CrV4 | 1.8159 | 6150 |
| 52 CGMFA | 51CrMoV4 | 1.7701 | - |
| 55 CR2A | 54SICr6 | 1.7102 | - |
| 55 CGA | 55Cr3 | 1.7176 | 5147 |
| 60 C2 CGA | 60SiCR7 | 1.7108 | 9262 |
Quelle: metaltrade.ru
| GUS-Länder (GOST, TU) | Deutschland (DIN) Ausländische Analoga | Deutschland (DIN) Ausländische Entsprechungen | USA (ASTM) |
|---|---|---|---|
| 70 | 1.1231 | Ck 67 | 1070 |
| 75 | 1.0605 | C 75 | 1074 |
| 85 | 1.1269 | Ck 85 | 1086 |
| 50CFA | 1.8159 | 50CrV4 | 6150 |
| 55С2 | 1.5026 | 55Si7 | - |
| 60Г | 1.0601 | С 60 | 1060 |
| 60C2 | 1.5027 | 60Si7 | 9260 |
| 60C2GH | 1.5092 | 60SiCr7 | 9262 |
| 70C2X | 1.5029 | 71Si 7 | - |
Quelle: metallopt.ru
| GUS-Länder (GOST, TU) | Deutschland (DIN) Ausländische Analoga | Deutschland (DIN) Ausländische Entsprechungen | USA (ASTM) |
|---|---|---|---|
| У 7 | 1.1620 | C 70W2 | - |
| U 7A | 1.1520 | C 70W1 | - |
| У 8 | 1.1625 | C 80W2 | - |
| U 8A | 1.1525 | C 80W1 | W 108 |
| У 10 | 1.1645 | C 105W2 | - |
| W 10A | 1.1545 | C 105W1 | W 110 |
| У 11 | 1.1654 | C 110W | - |
| У 13 | 1.1663 | C 125W | W 112 |
Quelle: metallopt.ru
| GUS-Länder (GOST, TU) | Deutschland (DIN/BOHLER) Ausländische Entsprechungen | Deutschland (DIN/BOHLER) Ausländische Entsprechungen | USA (AISI/ASTM) |
|---|---|---|---|
| Х12 | 1.2080 | X210Cr12 | D3 |
| X12B | 1.2436 | X210CrW12 | - |
| X12MF* | 1.2379 | X155CrVMo12−1 | D2 |
| X12MF4-MP | - | K190RM | - |
| 95CRF | 1.2210 | 115CrV 3 | L2 |
| 9X1F | 1.2067 | 102Cr 6 | L3 |
| 9G2F | 1.2842 | 90MnCrV 8 | O2 |
| 95CRVF | 1.2510 | 100MnCrW 4 | O1 |
| 3CR3B9F | 1.2581 | X30WCrV9−3 | H21 |
| 95CR5GM | 1.2363 | X100CrMoV5−1 | А2 |
| 95CRM | 1.2303 | 100CrMo 5 | L7 |
| 95Х18 | 1.4125 | X105CrMo17 | A473 (440C) |
| 5CRNIMO | 1.2713 | 55NiCrMoV 6 | L6 |
| 5CR2SF | 1.2550 | 60WCrV 7 | S1 |
| 5CR3MO2F | - | - | S7 |
| 5CRNI2MOV | 1.2714 | 56NiCrMoV 7 | - |
| 3CR3M3F | 1.2365 | X32CrMoV3 3 | H10 |
| 4X5MFS | 1.2343 | X38CrMoV5−1 | H11 |
| 4X5MF1C | 1.2344 | X40CrMoV5−1 | H13 |
*mögliche Herstellung durch Pulvermetallurgieverfahren
Quelle: metallopt.ru
| Stahlsorte GUS-Länder GOST | Stahlsorte Euronormen | Stahlsorte Euronormen | Analogien in US-Normen |
|---|---|---|---|
| P0 M2 SF10-MP | - | - | А11 |
| R2 M9-MP | S2−9-2 | 1.3348 | М7 |
| R2 M10 K8-MP | S2−10−1-8 | 1.3247 | М42 |
| R6 M5-MP | S6−5-2 | 1.3343 | М2 |
| R6 M5 K5-MP | S6−5-2−5 | 1.3243 | - |
| R6 M5 F3-MP | S6−5-3 | 1.3344 | М3 |
| P6 M5 F4-MP | - | - | М4 |
| R6 M5 F3 K8-MP | - | - | М36 |
| R10 M4 F3 K10-PP | S10−4-3−10 | 1.3207 | - |
| R6 M5 F3 K9-MP | - | - | М48 |
| R12 M6 F5-MP | - | - | М61 |
| R12 F4 K5-MP | S12−1-4−5 | 1.3202 | - |
| R12 F5 K5-MP | - | - | Т15 |
| R18-MP | - | - | Т1 |
Quelle: metaltrade.ru
| GUS-Länder (GOST, TU) | Deutschland (DIN) | BOHLER (D-016) | USA (AISI/ASTM) |
|---|---|---|---|
| R18* | 1.3355 | S 200 | Т 1 |
| R6M5* | 1.3343 | S600/S601 | М 2 |
| R6M5K5* | 1.3243 | S 705 | - |
| R6M5F3-MP | 1.3342/1.3344 | S 790PM | М 3 |
| R6M5F4-MP | - | S 690PM | М 4 |
| R6M5F3K8-MP | - | S 590PM | М 36 |
| R10M2F5K8-MP | - | S 390PM | - |
| R10M3F4K8-MP | - | - | - |
| R12F3 | 1.3318 | - | - |
| R12MF4-MP | - | S 207PM | - |
| R12K5F4-MP | - | S 308PM | - |
| R12M6F5-MP | - | - | М 61 |
| R12MF5K5-MP | 1.3202 | - | Т 15 |
| R0M2SF10-MP | - | CPM 10V | А 11 |
* Herstellung nach dem pulvermetallurgischen Verfahren ist möglich
Quelle: metallopt.ru
| GUS-Länder (GOST) | Analog | Land Standard |
|---|---|---|
| 20GL | A352 Gr LCC | USA, ASTM A352 |
| 20GL | A757 Gr A2Q | USA, ASTM A757 |
| 20GL | A216 Gr WCC | USA, ASTM A216 |
| 30GSL | A304 (1330H) | USA, ASTM A304 |
| 30GSL | A322 (1330) | 1330H USA, ASTM A322 |
| 20Л | A732 (1A) | 1A USA, ASTM A732 |
| 25Л | A352 Gr LCA | 20L (1A) ASTM A732 (1A) USA, ASTM A352 |
| 25Л | A732 (2A) | 2A USA, ASTM A732 |
| 25Л | A216 Gr WCB | USA, ASTM A216 |
| 30Л | A352 Gr LCB | USA, ASTM A352 |
| 30Л | A216 Gr WCB | USA, ASTM A216 |
| 35Л | A356 Gr1 | USA, ASTM A356 |
| 40Л | A732 (3A) | USA, ASTM A732 |
Quelle: www. td-ksz.com
| GUS-Länder (GOST) | Analog | Land Norm |
|---|---|---|
| 20GL | 1.1120 | Deutschland, DIN 17 182 |
| 30GSL | 1.1165 | Deutschland, DIN 17 205 |
| 15Л | 1.0420 | Deutschland, DIN 1681 |
| 20Л | 1.0619 | Deutschland, DIN EN 10 213−2 |
| 25Л | 1.0446 | Deutschland, DIN 1681 |
| 35Л | 1.0552 | Deutschland, DIN 1681 |
| 45Л | 1.0558 | Deutschland, DIN 1681 |
Quelle: www. td-ksz.com
| GUS-Länder (GOST) | Kurzbezeichnung | Land Norm |
|---|---|---|
| 30GSL | AO35 MnSi5 | Ungarn, MSZ 8272 |
| 30GSL | 30 GSL | Bulgarien, BDS 6550 |
| 30GSL | T30 Si Mn12 | Rumänien, STAS 1773 |
| 15Л | 15LII | Bulgarien, BDS3492 |
| 15Л | AM1 | BRITANNIEN, B.S.3100 (91) |
| 15Л | Ao 400 FK | Ungarn, MSZ 8276 |
| 15Л | L II 400 | Polen, PN/H 83 152 |
| 15Л | OT 400−3 | Rumänien, STAS 600 |
| 15Л | 422 630 | Tschechische Republik, Slowakei, CSN 422 630 |
| 25Л | 161 Grad 430 | Großbritannien, B.S. 1504 (76) |
| 25Л | 25 LII | Bulgarien, BDS 3492 |
| 25Л | Ao 450 FK | Ungarn, MSZ 8276 |
| 25Л | OT 450−3 | Rumänien, STAS 600 |
| 25Л | 25LI | Bulgarien, BDS 3492 |
| 25Л | 422 640 | Tschechische Republik, Slowakei, CSN 422 640 |
| 25Л | L 450 | Polen, PN/H 83 152 |
| 30Л | 1505 | Schweden, SS |
| 35Л | 35LII | Bulgarien, BDS 3492 |
| 35Л | A2 | BRITANNIEN, B.S.3100 (91) |
| 35Л | Ao 500 FK | Ungarn, MSZ 8276 |
| 35Л | L500 | Polen, PN/H8 3152 |
| 35Л | OT 500−1 | Rumänien, STAS 600 |
| 35Л | 35LI | Bulgarien, BDS3492 |
| 35Л | 422 650 | Tschechische Republik, Slowakei, CSH 422 650 |
| 35Л | G-30−57 | Finnland, SFS 350 |
| 35Л | SCC | Japan, JIS G5111 (91) |
| 40Л | 35LI | Bulgarien, BDS 3492 |
| 40Л | OT 550−1 | Rumänien, STAS 600 |
| 40Л | CLA1 Klasse C | UK, B.S. 3146 Teil 1 (74) |
| 40Л | CLA8 Grad C | UK, B.S. 3146 Teil 1 (74) |
| 40Л | G-30−57 | Finnland, SFS 350 |
| 45Л | 45LI | Bulgarien, BDS 3492 |
| 45Л | A3 | BRITANNIEN, B.S.3100 (91) |
| 45Л | Ao550FK | Ungarn, MSZ 8276 |
Quelle: www. td-ksz.com