Die Preisliste
Lager
Zusätzliche Felder
| Markierung | W. Nr. | Titel | Stahl Typ | Form | Größe | Kommentar | Die Balance |
|---|---|---|---|---|---|---|---|
| 36NKhTYU-N-O | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,45х115mm | GOST 14117-85 | 18.7 |
| 36NKhTYU-N-O | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,5х100mm | GOST 14117-85 | 38.4 |
| 36NKhTYU-N-O | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,5х160mm | GOST 14117-85 | 30.4 |
| 36NKhTYU-N-O | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,5х200mm | GOST 14117-85 | 62.3 |
| 36NKhTYu-SH-N-O | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,5х200mm | TU 14-131-504-81 | 76.1 |
| 36NKhTYu-SH-N-O | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,5х200mm | TU 14-131-504-81 | 70 |
| 36NKhTYU-N-O | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,75h100mm | GOST 14117-85 | 20.2 |
| 36NKhTYU-N-O | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,8х160mm | GOST 14117-85 | 50.1 |
| 36NKhTYU-N-O | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,8х200mm | GOST 14117-85 | 87.5 |
| 36NKhTYU-N-O | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 1х200mm | GOST 14117-85 | 38.8 |
| 36NKhTYU-N-O | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 1,25х250mm | GOST 14117-85 | 59.8 |
| 36NKhTYU-N-O | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 1,5х250mm | GOST 14117-85 | 250.2 |
| 36NKhTYU-N-O | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,12х100mm | GOST 14117-85 | 36.1 |
| 36NKhTYU-N-O | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,15х115mm | GOST 14117-85 | 37 |
| 36NKhTYU-N-O | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,15х150mm | GOST 14117-85 | 60.8 |
| 36NKhTYU-N-O | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,15х93mm | GOST 14117-85 | 13.9 |
| 36NKhTYU-N-O | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,15х93mm | GOST 14117-85 | 41.5 |
| 36NKhTYU-N-O | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,15х93mm | GOST 14117-85 | 34.4 |
| 36NKhTYU-N-O | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,15х93mm | GOST 14117-85 | 46.4 |
| 36NKhTYU-N-O | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,15х93mm | GOST 14117-85 | 48.8 |
| 36NKhTYU-N-O | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,15х93mm | GOST 14117-85 | 50.5 |
| 36NKhTYU-N-O | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,1х200mm | GOST 14117-85 | 29.8 |
| 36NKhTYU-N-O | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,1х250mm | GOST 14117-85 | 36.4 |
| 36NKhTYU-N-O | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,25х150mm | GOST 14117-85 | 50.9 |
| 36NKhTYU-N-O | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,25х150mm | GOST 14117-85 | 60 |
| 36NKhTYU-N-O | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,25х250mm | GOST 14117-85 | 17.1 |
| 36NKhTYU-N-O | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,25х250mm | GOST 14117-85 | 32 |
| 36NKhTYU-N-O | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,2х150mm | GOST 14117-85 | 84.6 |
| 36NKhTYu-M-N-O | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,2х200mm | GOST 14117-85 | - |
| 36NKhTYU-N-O | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,2х200mm | GOST 14117-85 | 16.8 |
| 36NKhTYU-N-O | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,2х200mm | GOST 14117-85 | 12.2 |
| 36NKhTYU-N-O | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,35х150mm | GOST 14117-85 | 59.3 |
| 36NKhTYU-N-O | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,35х200mm | GOST 14117-85 | 16.8 |
| 36NKhTYU-N-O | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,35х200mm | GOST 14117-85 | 52.1 |
| 36НХТЮ | 1.3918 | Elinvar® | Ni-SpanC902 | Kreis | ф6mm | GOST 14119-85 | 39kg |
| 36НХТЮ | 1.3918 | Elinvar® | Ni-SpanC902 | Kreis | ф9mm | GOST 14119-85 | 74kg |
| 36НХТЮ | 1.3918 | Elinvar® | Ni-SpanC902 | Kreis | ф10mm | GOST 14119-85 | 132kg |
| 36НХТЮ | 1.3918 | Elinvar® | Ni-SpanC902 | Kreis | ф15mm | GOST 14119-85 | 47kg |
| 36НХТЮ | 1.3918 | Elinvar® | Ni-SpanC902 | Kreis | ф16mm | GOST 14119-85 | 65kg |
| 36НХТЮ | 1.3918 | Elinvar® | Ni-SpanC902 | Kreis | ф20mm | GOST 14119-85 | 84kg |
| 36НХТЮ | 1.3918 | Elinvar® | Ni-SpanC902 | Kreis | ф25mm | GOST 14119-85 | 72kg |
| 36НХТЮ | 1.3918 | Elinvar® | Ni-SpanC902 | Kreis | ф32mm | GOST 14119-85 | 65kg |
| 36НХТЮ | 1.3918 | Elinvar® | Ni-SpanC902 | Kreis | ф40mm | GOST 14119-85 | 27kg |
| 36НХТЮ | 1.3918 | Elinvar® | Ni-SpanC902 | Kreis | ф55mm | GOST 14119-85 | 43kg |
| 36НХТЮ | 1.3918 | Elinvar® | Ni-SpanC902 | Kreis | ф60mm | GOST 14119-85 | 57kg |
| 36НХТЮ | 1.3918 | Elinvar® | Ni-SpanC902 | Kreis | ф80mm | GOST 14119-85 | 162kg |
| VT1-00 | 3.7025 | Titan Grade 1 | Titanmetall | Band | 0,05х150mm | 37 | |
| VT1-00 | 3.7025 | Titan Grade 1 | Titanmetall | Rohr | 2H0,5 | 14 | |
| 36НХТЮ | 1.3918 | Elinvar® | Ni-SpanC902 | Draht | 1,80 | 3 | |
| 36НХТЮ | 1.3918 | Elinvar® | Ni-SpanC902 | Draht | 0,1х200 | 18 | |
| 36НХТЮ | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,4 x 400 mm | ≈ 70 kg | |
| VT1-00-св | 3.7025 | Titan Grade 1 | Titanmetall | Draht | 1.2 x | 2B | 11.6 |
| VT1-00-св | 3.7025 | Titan Grade 1 | Titanmetall | Draht | 1.5 x | 1B | 28 |
| VT1-00-св | 3.7025 | Titan Grade 1 | Titanmetall | Draht | 2x | 5B | 171.4 |
| VT1-00-св | 3.7025 | Titan Grade 1 | Titanmetall | Draht | 2.5 x | 1B | 11.8 |
| VT1-00-св | 3.7025 | Titan Grade 1 | Titanmetall | Draht | 3h | 2B | 15.4 |
| VT1-00-св | 3.7025 | Titan Grade 1 | Titanmetall | Draht | 4x | 2B | 7 |
| VT1-00-св | 3.7025 | Titan Grade 1 | Titanmetall | Draht | 4x | 5B | 177.6 |
| VT1-00-св | 3.7025 | Titan Grade 1 | Titanmetall | Draht | 6x | 1B | 3 |
| VT1-00 | 3.7025 | Titan Grade 1 | Titanmetall | Kreis | 25х1200-1400 | m/O | 220,5 |
| VT1-00 | 3.7025 | Titan Grade 1 | Titanmetall | Draht | 1 | ВИЛС, Umbau | 28 |
| VT1-00 | 3.7025 | Titan Grade 1 | Titanmetall | Draht | 1.21 | Stück | 34,3 |
| VT1-00 | 3.7025 | Titan Grade 1 | Titanmetall | Draht | 1.2 | 41,6 | |
| VT1-00 | 3.7025 | Titan Grade 1 | Titanmetall | Draht | 1.5 | 39,4 | |
| VT1-00 | 3.7025 | Titan Grade 1 | Titanmetall | Draht | 1.61 | Stück ВИЛС, Umbau | 43 |
| VT1-00 | 3.7025 | Titan Grade 1 | Titanmetall | Draht | 1.6 | 79,1 | |
| VT1-00 | 3.7025 | Titan Grade 1 | Titanmetall | Draht | 2 | 216,8 | |
| VT1-00 | 3.7025 | Titan Grade 1 | Titanmetall | Draht | 2.3 | 6,8 | |
| VT1-00 | 3.7025 | Titan Grade 1 | Titanmetall | Draht | 2.5 | 10,6 | |
| VT1-00 | 3.7025 | Titan Grade 1 | Titanmetall | Draht | 3 | 42,6 | |
| VT1-00 | 3.7025 | Titan Grade 1 | Titanmetall | Draht | 3.3 | 10,8 | |
| VT1-00 | 3.7025 | Titan Grade 1 | Titanmetall | Draht | 4 | 97 | |
| VT1-00 | 3.7025 | Titan Grade 1 | Titanmetall | Draht | 5 | 28,3 | |
| VT1-00 | 3.7025 | Titan Grade 1 | Titanmetall | Draht | 8 | 31,1 kg+42,2 kg | 73,3 |
| VT1-00 | 3.7025 | Titan Grade 1 | Titanmetall | Kreis | 12 | 6kg | |
| VT1-00 | 3.7025 | Titan Grade 1 | Titanmetall | Rohr | 25x1.5 | 80 | |
| VT1-00 | 3.7025 | Titan Grade 1 | Titanmetall | Draht | 2х530 | kg | unter die Bestellung |
| VT1-00-св | 3.7025 | Titan Grade 1 | Titanmetall | Draht | 0.8 | 50 | |
| VT1-00-св | 3.7025 | Titan Grade 1 | Titanmetall | Draht | 2.5 | 68 | |
| VT1-00-св | 3.7025 | Titan Grade 1 | Titanmetall | Draht | 3 | 890 | |
| VT1-00-св | 3.7025 | Titan Grade 1 | Titanmetall | Draht | 4 | 144 | |
| 36НХТЮ | 1.3918 | Elinvar® | Ni-SpanC902 | Kreis | Ø 55 x 1560 mm mm | 28,9 kg | |
| 36НХТЮ | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,15х90 mm | 45,5 kg | |
| 36НХТЮ | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,15х100 mm | 54,2 kg | |
| 36НХТЮ | 1.3918 | Elinvar® | Ni-SpanC902 | Kreis | Ø 52 | 25,7 kg | |
| 36НХТЮ | 1.3918 | Elinvar® | Ni-SpanC902 | Kreis | Ø 90 | 67,5 kg | |
| 36НХТЮ | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,2h200 | 5,3 kg | |
| 36НХТЮ | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,2h200 mm | 23,3 kg | |
| 36НХТЮ | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,3х200 mm | 50 kg | |
| 36НХТЮ | 1.3918 | Elinvar® | Ni-SpanC902 | Band | ø3 mm | 6,6 kg | |
| 36НХТЮ | 1.3918 | Elinvar® | Ni-SpanC902 | Band | ø3,5 mm | 8,2 kg | |
| 36НХТЮ | 1.3918 | Elinvar® | Ni-SpanC902 | Band | ø3,5 mm | 14,4 kg | |
| 36НХТЮ | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,4х200 | 8 kg | |
| 36НХТЮ | 1.3918 | Elinvar® | Ni-SpanC902 | Band | 0,35*250mm | 6 | |
| 36НХТЮ | 1.3918 | Elinvar® | Ni-SpanC902 | Blatt | 1*720*1430mm | 8.3 | |
| 36НХТЮ | 1.3918 | Elinvar® | Ni-SpanC902 | Blatt | 0,5H100 | Band 36НХТЮ 1 Stück. | 41.50 |
| 36НХТЮ | 1.3918 | Elinvar® | Ni-SpanC902 | Kreis | F-16 | Kreis 36НХТЮ 1 | 5.00 |
| 36НХТЮ | 1.3918 | Elinvar® | Ni-SpanC902 | Kreis | f-40+1; | F-40 Kreis 36НХТЮ 3 | 65 |
| 36НХТЮ | 1.3918 | Elinvar® | Ni-SpanC902 | Kreis | 180 mm | 0,08 m(21,2 kg засверл) 1Stück Stigma эи702 | 21.2 |
| 36НХТЮ | 1.3918 | Elinvar® | Ni-SpanC902 | Kreis | 27mm | 2,632,7 m(60,2 kg) 5er; 2,13 m(9,5 kg); 1,15 m(5,2 kg) für 1pc N\O | 75 |