| VT1-0 |
|
3.7035 |
R50400 |
|
Titan Grade 2 |
Titanmetall |
Rohr |
45x2.5x |
|
97.5 |
Ru240 |
|
| OT4 |
|
|
|
|
Titanium gost OT4 |
Titanmetall |
Rohr |
45x3.5х3675-3875 |
2 Stück |
17 |
Ru240 |
|
| VT1-0 |
|
3.7035 |
R50400 |
|
Titan Grade 2 |
Titanmetall |
Rohr |
45x2 |
|
11,1 |
Ru250 |
|
| ХН78Т |
EI435 |
2.4630 |
N06075 |
NiCr20Ti |
Nimonic 75® |
Nickel-Legierung |
Blatt |
2,2 mm |
0,55x1м(9,8 kg); 0,44x0,9; 0,45x1; 0,44x1; 0,41x0,95; 0,45x1; 0,45x0,89; 0,45x0,9M nach 1piece |
63.0 |
Ua210 |
Ukraine |
| hn28mdt |
|
|
|
|
|
|
Blatt |
4 mm |
0,45x0,71м(30kg маркир) - 3st; 0,65x1,62m(36,1 kg); 0,68x1,65m(35,8 kg) |
101.7 |
Ua210 |
Ukraine |
| hn28mdt |
|
|
|
|
|
|
Blatt |
8 mm |
0,55x0,6M(20kg); 0,45x1,14m(32,4 kg) für 1pc |
52.4 |
Ua210 |
Ukraine |
| 12X18H10T |
EP2 |
1.4541 |
321 |
X12CrNiTi18-10 |
|
Edelstahl |
Blatt |
24 mm |
1,45x1,26m(338kg) - 1Stück Lager 2 |
338.0 |
Ua210 |
Ukraine |
| VT1-0 |
|
3.7035 |
R50400 |
|
Titan Grade 2 |
Titanmetall |
Blatt |
10mm |
1x1,41м(63kg); 0,9x2м(80,7 kg); 0,45x0,49m(10kg*); 0,55x1,2m(30,6 kg); 0,96x1,14m(49,7 kg) für 1pc |
234 |
Ua210 |
|
| LS-59 |
|
|
|
|
|
Messing |
Blatt |
4,0 mm |
Messing 0,45x0,83м(12,5 kg zu finden!!!!) 1Stück |
12.5 |
Ua210 |
|
| Techniker |
|
|
|
|
|
|
Blatt |
2mm |
1x2м 5er (152,7 kg) -2R; 1,045x1,6M(25kg); 0,64x0,39th(3,9 kg) -4j |
181.6 |
Ua220 |
Ukraine |
| 12X18H10T |
EP2 |
1.4541 |
321 |
X12CrNiTi18-10 |
|
Edelstahl |
Blatt |
3mm |
0,45x1м 10,8 kg; 0,29x0,45m-3,2 kg 3G |
14 |
Ua220 |
Ukraine |