| VT1-0 |
|
3.7035 |
R50400 |
|
Titan Grade 2 |
Titanmetall |
Band |
0,05х150mm |
in der Rolle |
35kg |
Ru020 |
|
| 15X25T |
EI439 |
1.4762 |
446 |
X10CrAl24 |
|
Hitzebeständige Stähle |
Rohr |
ф159х6mm |
GOST 9940-81 2-3M |
1445kg |
Ru020 |
|
| 15X25T |
EI439 |
1.4762 |
446 |
X10CrAl24 |
|
Hitzebeständige Stähle |
Rohr |
ф219х10mm |
GOST 9940-81 2-3M |
284kg |
Ru020 |
|
| 04Х17Н13М2 |
|
1.4404 |
316L |
X2CrNiMo17-12-2 |
|
Korrosionsbeständige Edelstahl |
Rohr |
ф6х1mm |
1620 Meter in der Bucht |
200 |
Ru020 |
|
| 08Х21Н6М2Т |
EP54 |
|
|
|
|
Edelstahl |
Rohr |
ф135х6mm |
4M GOST 9940-81 |
80kg |
Ru020 |
|
| 06HN28MDT |
EI943 |
1.4539 |
904L |
X3NiCrCuMoTi27-23 |
Cronifer 1925hMo |
Edelstahl |
Rohr |
ф102х18 |
GOST 9940-81 2-3M |
120kg |
Ru020 |
|
| 06HN28MDT |
EI943 |
1.4539 |
904L |
X3NiCrCuMoTi27-23 |
Cronifer 1925hMo |
Edelstahl |
Rohr |
ф108х4mm |
GOST 9940-81 |
76kg |
Ru020 |
|
| 06HN28MDT |
EI943 |
1.4539 |
904L |
X3NiCrCuMoTi27-23 |
Cronifer 1925hMo |
Edelstahl |
Rohr |
ф108х5mm |
VAT-Steuer GOST 9940-81 |
190kg |
Ru020 |
|
| 06HN28MDT |
EI943 |
1.4539 |
904L |
X3NiCrCuMoTi27-23 |
Cronifer 1925hMo |
Edelstahl |
Rohr |
ф108х7mm |
VAT-Steuer GOST 9940-81 |
354kg |
Ru020 |
|
| хн65мву |
EP760 |
2.4819 |
N10276 |
NiMo16Cr15W |
Hastelloy C276® |
Nickel-Molybdän-Legierung |
Kreis |
ф40mm |
xн65мв Alloy c-276 |
54kg |
Ru020 |
|
| XN45YU |
EP747 |
|
|
|
|
Hitzebeständige Legierung |
Blatt |
5х1200х2400mm |
|
233kg |
Ru020 |
|
| MA8M |
|
|
|
|
|
|
Blatt |
0,8х1200х4000mm |
magnesiahaltige |
62kg |
Ru020 |
|
| MA8M |
|
|
|
|
|
|
Blatt |
1х1200х4000mm |
magnesiahaltige |
8kg |
Ru020 |
|
| 40X13 |
EZH4 |
1.4034 |
420 |
X46Cr13 |
|
Edelstahl |
Blatt |
3х1000х2000mm |
Rostfrei , GOST 5582-75 |
235kg |
Ru020 |
|
| 40X13 |
EZH4 |
1.4034 |
420 |
X46Cr13 |
|
Edelstahl |
Blatt |
4х1000х2000mm |
Edelstahlblech , GOST 5582-75 |
252kg |
Ru020 |
|
| 40X13 |
EZH4 |
1.4034 |
420 |
X46Cr13 |
|
Edelstahl |
Blatt |
5х1500х3000mm |
rostfrei, GOST 5582-75 |
354kg |
Ru020 |
|
| 40X13 |
EZH4 |
1.4034 |
420 |
X46Cr13 |
|
Edelstahl |
Blatt |
6х1500х3000mm |
rostfrei, GOST 5582-75 |
426kg |
Ru020 |
|
| 12Х18Н10Т-Н |
EP2 |
1.4541 |
321 |
X12CrNiTi18-10 |
|
Edelstahl |
Band |
0,03х400mm |
GOST 4986-79, Авиатеxприемка |
8 |
Ru020 |
|
| 12X18H10T-M |
EP2 |
1.4541 |
321 |
X12CrNiTi18-10 |
|
Edelstahl |
Band |
0,1х400mm |
GOST 4986-79, Авиатеxприемка |
465 |
Ru020 |
|
| 12Х18Н10Т-Н |
EP2 |
1.4541 |
321 |
X12CrNiTi18-10 |
|
Edelstahl |
Band |
0,18х400mm |
GOST 4986-79, Авиатеxприемка |
119 |
Ru020 |
|
| 12X18H10T-M |
EP2 |
1.4541 |
321 |
X12CrNiTi18-10 |
|
Edelstahl |
Band |
0,2х400mm |
GOST 4986-79, Авиатеxприемка |
96 |
Ru020 |
|
| 12Х18Н10Т-Н |
EP2 |
1.4541 |
321 |
X12CrNiTi18-10 |
|
Edelstahl |
Band |
0,3х400mm |
GOST 4986-79, Авиатеxприемка |
32 |
Ru020 |
|
| 12X18H10T-M |
EP2 |
1.4541 |
321 |
X12CrNiTi18-10 |
|
Edelstahl |
Band |
0,4х400mm |
GOST 4986-79, Авиатеxприемка |
26 |
Ru020 |
|
| 12X18H10T-M |
EP2 |
1.4541 |
321 |
X12CrNiTi18-10 |
|
Edelstahl |
Band |
0,5х400mm |
GOST 4986-79, Авиатеxприемка |
44 |
Ru020 |
|
| 36NKhTYU5M-N-O |
EP51 |
EP51 |
|
|
Elinvar + 5Mo® |
Nickel-Legierung |
Band |
0,3х140mm |
GOST 14117-85 |
34.9 |
Ru020 |
|
| 36НХТЮ |
EI702 |
1.3918 |
N09902 |
|
Elinvar® |
Ni-SpanC902 |
Kreis |
ф40mm |
GOST 14119-85 |
27kg |
Ru020 |
|
| 50N |
EI467 |
1.3922 |
K94840 |
NiFe50 |
Permalloy® |
Präzisions-Legierung |
Draht |
ф8mm |
|
11,2 kg |
Ru020 |
|
| BrB2 |
|
2.1447 |
|
CuBe2 |
CB2 |
Berylliumbronze |
Kreis |
40mm |
Feste |
auf Anfrage |
Ru020 |
|
| BrB2 |
|
2.1447 |
|
CuBe2 |
CB2 |
Berylliumbronze |
Kreis |
40mm |
Feste |
auf Anfrage |
Ru020 |
|
| BrB2 |
|
2.1447 |
|
CuBe2 |
CB2 |
Berylliumbronze |
Kreis |
40mm |
solide gezogene Stangen |
auf Anfrage |
Ru020 |
|
| XN65MV |
EP567 |
2.4819 |
N10276 |
NiMo16Cr15W |
Hastelloy C276® |
Nickel-Molybdän-Legierung |
Kreis |
ф40mm |
TU 14-1-377-72/2590-2006, Авиатеxприемка |
139kg |
Ru020 |
|
| 29NK |
|
1.3981 |
K94610 |
NiCo29-18 |
Kovar® |
Nilo |
Kreis |
ф6mm |
GOST 14082-78 |
62kg |
Ru020 |
|
| 29NK |
|
1.3981 |
K94610 |
NiCo29-18 |
Kovar® |
Nilo |
Kreis |
ф9mm |
GOST 14082-78 |
58kg |
Ru020 |
|
| 29NK |
|
1.3981 |
K94610 |
NiCo29-18 |
Kovar® |
Nilo |
Kreis |
ф20mm |
GOST 14082-78 |
61kg |
Ru020 |
|
| 29NK |
|
1.3981 |
K94610 |
NiCo29-18 |
Kovar® |
Nilo |
Kreis |
ф25mm |
GOST 14082-78 |
84kg |
Ru020 |
|
| 29NK |
|
1.3981 |
K94610 |
NiCo29-18 |
Kovar® |
Nilo |
Kreis |
ф35mm |
GOST 14082-78 |
27kg |
Ru020 |
|
| 29NK |
|
1.3981 |
K94610 |
NiCo29-18 |
Kovar® |
Nilo |
Kreis |
ф40mm |
GOST 14082-78 |
87kg |
Ru020 |
|
| 29NK |
|
1.3981 |
K94610 |
NiCo29-18 |
Kovar® |
Nilo |
Kreis |
ф50mm |
GOST 14082-78 |
65kg |
Ru020 |
|
| 29NK |
|
1.3981 |
K94610 |
NiCo29-18 |
Kovar® |
Nilo |
Kreis |
ф55mm |
GOST 14082-78 |
121kg |
Ru020 |
|
| 29NK |
|
1.3981 |
K94610 |
NiCo29-18 |
Kovar® |
Nilo |
Kreis |
ф60mm |
GOST 14082-78 |
148kg |
Ru020 |
|
| 29NK |
|
1.3981 |
K94610 |
NiCo29-18 |
Kovar® |
Nilo |
Kreis |
ф70mm |
GOST 14082-78 |
116kg |
Ru020 |
|
| 29NK |
|
1.3981 |
K94610 |
NiCo29-18 |
Kovar® |
Nilo |
Kreis |
ф130mm |
GOST 14082-78 |
215kg |
Ru020 |
|
| 29NK |
|
1.3981 |
K94610 |
NiCo29-18 |
Kovar® |
Nilo |
Draht |
benachbarte Anschlüsse # 0,4mm |
GOST 14081-78 |
84kg |
Ru020 |
|
| 29NK |
|
1.3981 |
K94610 |
NiCo29-18 |
Kovar® |
Nilo |
Draht |
benachbarte Anschlüsse # 0,45mm |
GOST 14081-78 |
51kg |
Ru020 |
|
| 29NK |
|
1.3981 |
K94610 |
NiCo29-18 |
Kovar® |
Nilo |
Draht |
benachbarte Anschlüsse # 0,5mm |
GOST 14081-78 |
27kg |
Ru020 |
|
| 29NK |
|
1.3981 |
K94610 |
NiCo29-18 |
Kovar® |
Nilo |
Draht |
benachbarte Anschlüsse # 0,8mm |
GOST 14081-78 |
40kgs |
Ru020 |
|
| 29NK |
|
1.3981 |
K94610 |
NiCo29-18 |
Kovar® |
Nilo |
Draht |
F1,0mm |
GOST 14081-78 |
64kg |
Ru020 |
|
| 29NK |
|
1.3981 |
K94610 |
NiCo29-18 |
Kovar® |
Nilo |
Draht |
F1-2mm |
GOST 14081-78 |
55kg |
Ru020 |
|
| 29NK |
|
1.3981 |
K94610 |
NiCo29-18 |
Kovar® |
Nilo |
Draht |
F1,4mm |
GOST 14081-78 |
38kg |
Ru020 |
|
| 29NK |
|
1.3981 |
K94610 |
NiCo29-18 |
Kovar® |
Nilo |
Draht |
ф3mm |
GOST 14081-78 |
54kg |
Ru020 |
|
| BrB2 |
|
2.1447 |
|
CuBe2 |
CB2 |
Berylliumbronze |
Band |
0.15 x 240mm |
Feste |
auf Anfrage |
Ru020 |
|
| BrB2 |
|
2.1447 |
|
CuBe2 |
CB2 |
Berylliumbronze |
Band |
0.5 x 40mm |
Feste |
auf Anfrage |
Ru020 |
|
| BrB2 |
|
2.1447 |
|
CuBe2 |
CB2 |
Berylliumbronze |
Band |
0.5 x 40mm |
weiche |
auf Anfrage |
Ru020 |
|
| BrB2 |
|
2.1447 |
|
CuBe2 |
CB2 |
Berylliumbronze |
Band |
0.5 x 40mm |
Feste |
auf Anfrage |
Ru020 |
|
| 50NP |
50 |
1.3927 |
K94840 |
NiFe50 |
Permalloy® |
Präzisions-Legierung |
Band |
0,05х9mm |
|
10kg |
Ru020 |
|
| 12X18H10T |
EP2 |
1.4541 |
321 |
X12CrNiTi18-10 |
|
Edelstahl |
Band |
0,05х400 |
|
23 |
Ru010 |
|
| 12X18H10T |
EP2 |
1.4541 |
321 |
X12CrNiTi18-10 |
|
Edelstahl |
Band |
0,1х400 |
|
225,3 |
Ru010 |
|
| 12X18H10T |
EP2 |
1.4541 |
321 |
X12CrNiTi18-10 |
|
Edelstahl |
Band |
0,15х400 |
|
47 |
Ru010 |
|
| 12X18H10T |
EP2 |
1.4541 |
321 |
X12CrNiTi18-10 |
|
Edelstahl |
Band |
0,2х400 |
|
101,2 |
Ru010 |
|
| 12X18H10T |
EP2 |
1.4541 |
321 |
X12CrNiTi18-10 |
|
Edelstahl |
Band |
0,25х400 |
|
50 |
Ru010 |
|
| 12X18H10T |
EP2 |
1.4541 |
321 |
X12CrNiTi18-10 |
|
Edelstahl |
Band |
0,3х400 |
|
93,9 |
Ru010 |
|
| 12X18H10T |
EP2 |
1.4541 |
321 |
X12CrNiTi18-10 |
|
Edelstahl |
Band |
0,4х400 |
|
38,2 |
Ru010 |
|
| 12X18H10T |
EP2 |
1.4541 |
321 |
X12CrNiTi18-10 |
|
Edelstahl |
Band |
0,5х400 |
|
41,8 |
Ru010 |
|
| 12X18H10T |
EP2 |
1.4541 |
321 |
X12CrNiTi18-10 |
|
Edelstahl |
Band |
1х400 |
|
25,3 |
Ru010 |
|
| 20X13N4G9N |
EI100 |
|
|
|
|
|
Band |
0,25х400 |
|
74 |
Ru010 |
|
| 20 H13 |
EZH2 |
1.4021 |
420 |
X20Cr13 |
|
Edelstahl |
Band |
0,3х400 |
|
109,5 |
Ru010 |
|
| Kh23Yu5T |
|
1.4765 |
|
|
Kanthal AF® |
Fechral |
Draht |
0,40 |
|
21,41 |
Ru010 |
|
| Kh23Yu5T |
|
1.4765 |
|
|
Kanthal AF® |
Fechral |
Draht |
1,40 |
|
48,7 |
Ru010 |
|
| Kh23Yu5T |
|
1.4765 |
|
|
Kanthal AF® |
Fechral |
Draht |
1,40 |
|
122,2 |
Ru010 |
|
| X27Yu5T |
EI626 |
|
|
|
Kanthal AF® |
Fechral |
Draht |
1,40 |
|
54,8 |
Ru010 |
|
| Kh23Yu5T |
|
1.4765 |
|
|
Kanthal AF® |
Fechral |
Draht |
1,40 |
|
68,8 |
Ru010 |
|
| Х15Н60 |
EHN60 |
2.4867 |
N06004 |
NiCr60-15 |
NIKROTHAL 60® |
Nichrome |
Draht |
1,40 |
|
10,3 |
Ru010 |
|
| 04Х17Н13М2 |
|
1.4404 |
316L |
X2CrNiMo17-12-2 |
|
Korrosionsbeständige Edelstahl |
Rohr |
6*1 |
|
650,9 |
Ru010 |
|
| VT1-0 |
|
3.7035 |
R50400 |
|
Titan Grade 2 |
Titanmetall |
Rohr |
52х2 |
|
7,8 |
Ru010 |
|
| 50N |
EI467 |
1.3922 |
K94840 |
NiFe50 |
Permalloy® |
Präzisions-Legierung |
Draht |
8,00 |
|
90 |
Ru010 |
|
| MNTs15-20 |
|
2.0740 |
|
CuNi18Zn20 |
|
Nickel Silber |
Band |
1,20 |
|
3,4 |
Ru010 |
|
| MNMts40-1.5 |
|
|
|
CuNi40 |
|
Konstantanfolie |
Draht |
3,20 |
|
91,94 |
Ru010 |
|
| MNMts40-1.5 |
|
|
|
CuNi40 |
|
Konstantanfolie |
Draht |
3,20 |
|
90,14 |
Ru010 |
|
| MNMts40-1.5 |
|
|
|
CuNi40 |
|
Konstantanfolie |
Draht |
1,50 |
|
0,25 |
Ru010 |
|
| MNMts40-1.5 |
|
|
|
CuNi40 |
|
Konstantanfolie |
Draht |
1,50 |
|
0,2 |
Ru010 |
|
| MNMts40-1.5 |
|
|
|
CuNi40 |
|
Konstantanfolie |
Draht |
0,80 |
|
7 |
Ru010 |
|
| XN65MV |
EP567 |
2.4819 |
N10276 |
NiMo16Cr15W |
Hastelloy C276® |
Nickel-Molybdän-Legierung |
Kreis |
ф40mm |
TU 14-1-3239-81, GOST 2590-2006 |
232 |
Ru010 |
|
| 10X17H13M3T |
EI432 |
|
|
|
|
|
Blatt |
14,0х1040-1060х1440-1460 |
5лист-Blatt |
945kg |
Ru120 |
|
| ХН78Т |
EI435 |
2.4630 |
N06075 |
NiCr20Ti |
Nimonic 75® |
Nickel-Legierung |
Blatt |
0,2х400 |
|
69 |
Ru120 |
|
| ХН78Т |
EI435 |
2.4630 |
N06075 |
NiCr20Ti |
Nimonic 75® |
Nickel-Legierung |
Blatt |
0,5х540-790х1090-1250 |
6лист-Blatt |
15kg |
Ru120 |
|
| ХН78Т |
EI435 |
2.4630 |
N06075 |
NiCr20Ti |
Nimonic 75® |
Nickel-Legierung |
Blatt |
1,0х480-510х1220-1810 |
С40ф 6лист-Blatt |
41kg |
Ru120 |
|
| ХН78Т |
EI435 |
2.4630 |
N06075 |
NiCr20Ti |
Nimonic 75® |
Nickel-Legierung |
Blatt |
1,0х1010-1040х1900-2170 |
5лист-Blatt |
89kg |
Ru120 |
|
| ХН78Т |
EI435 |
2.4630 |
N06075 |
NiCr20Ti |
Nimonic 75® |
Nickel-Legierung |
Blatt |
1.2х1040х2030 |
С25ф 1-Blatt |
21,5 kg |
Ru120 |
|
| ХН78Т |
EI435 |
2.4630 |
N06075 |
NiCr20Ti |
Nimonic 75® |
Nickel-Legierung |
Blatt |
2.0х710х400 |
|
6 |
Ru120 |
|
| ХН78Т |
EI435 |
2.4630 |
N06075 |
NiCr20Ti |
Nimonic 75® |
Nickel-Legierung |
Blatt |
2.0х970-1050х1400-2630 |
С362ф 9лист-Blatt |
364kg |
Ru120 |
|
| ХН78Т |
EI435 |
2.4630 |
N06075 |
NiCr20Ti |
Nimonic 75® |
Nickel-Legierung |
Blatt |
4,0х1010х1940-2070 |
3лист-Blatt |
205kg |
Ru120 |
|
| ХН78Т |
EI435 |
2.4630 |
N06075 |
NiCr20Ti |
Nimonic 75® |
Nickel-Legierung |
Blatt |
11,0х1000х1200-1400 |
4лист-Blatt |
474kg |
Ru120 |
|
| ХН78Т |
|
|
|
|
|
|
Blatt |
14,0х1040-1060х1060-1080 |
2St |
323kg |
Ru120 |
|
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Blatt |
10,0х600х1440 |
1-Blatt |
66kg |
Ru120 |
|
| HN75MBTYu |
EI602 |
2.4856 |
N06625 |
NiCr22Mo9Nb |
Inconel 625® |
Nickel-Legierung |
Blatt |
0,8х1040х2060-2220 |
4лист-Blatt |
75kg |
Ru120 |
|
| HN75MBTYu |
EI602 |
2.4856 |
N06625 |
NiCr22Mo9Nb |
Inconel 625® |
Nickel-Legierung |
Blatt |
3,0х710х640 |
1-Blatt |
10kg |
Ru120 |
|
| 10x11n20t2r |
EI696 |
|
|
|
|
|
Blatt |
1,5х330-710х940-1500 |
34лист-Blatt |
372kg |
Ru120 |
|
| ХН38VT |
|
|
|
|
|
|
Blatt |
0,8х0.8х1040х1950 |
1-Blatt |
13kg |
Ru120 |
|
| ХН38VT |
|
|
|
|
|
|
Blatt |
0,8х0.8х1040-1070х1950-2020 |
с40ф 3лист-Blatt |
41kg |
Ru120 |
|
| ХН38VT |
|
|
|
|
|
|
Blatt |
1,0х1010-1070х340-2180 |
с67ф 6лист-Blatt |
68kg |
Ru120 |
|