LS59-1 2.0402 CuZn39Pb1 Messing Band 3х600х1500 mm 21,8 kg Ru310
LS59-1 2.0402 CuZn39Pb1 Messing Band 3х600х1500 mm 21,8 kg Ru310
Messing Kreis 20mm auf 1,02 m-2St 1g 5.4 Ua220 Ukraine
Messing hexahedron №17 (0,55 m) 1.1 Ua220 Ukraine
LS59-1 2.0402 CuZn39Pb1 Messing hexahedron №5,0 0.5 Ua430 Ukraine
LS59-1 2.0402 CuZn39Pb1 Messing hexahedron №5,5 0.5 Ua430 Ukraine
LS59-1 2.0402 CuZn39Pb1 Messing hexahedron №6,0 0.5 Ua430 Ukraine
LS59-1 2.0402 CuZn39Pb1 Messing hexahedron №7,0 30 Ua430 Ukraine
LS59-1 2.0402 CuZn39Pb1 Messing hexahedron №8,0 15.4 Ua430 Ukraine
LS59-1 2.0402 CuZn39Pb1 Messing hexahedron №8,0 9.5 Ua430 Ukraine
LS59-1 2.0402 CuZn39Pb1 Messing hexahedron №10 38 Ua430 Ukraine
LS59-1 2.0402 CuZn39Pb1 Messing hexahedron №11 78.1 Ua430 Ukraine
LS59-1 2.0402 CuZn39Pb1 Messing hexahedron №14 124 Ua430 Ukraine
LS59-1 2.0402 CuZn39Pb1 Messing hexahedron №17 10 Ua430 Ukraine
LS59-1 2.0402 CuZn39Pb1 Messing hexahedron №19 1102 Ua430 Ukraine
LS59-1 2.0402 CuZn39Pb1 Messing hexahedron №27*5 12.3 Ua430 Ukraine
LS59-1 2.0402 CuZn39Pb1 Messing hexahedron №24 5 Ua430 Ukraine
LS59-1 2.0402 CuZn39Pb1 Messing hexahedron №30 2.5 Ua430 Ukraine
LS59-1 2.0402 CuZn39Pb1 Messing hexahedron №41 4.1 Ua430 Ukraine
LS59-1 2.0402 CuZn39Pb1 Messing hexahedron №8,0 32 Ua430 Ukraine
LS59-1 2.0402 CuZn39Pb1 Messing hexahedron 3*30 150kg Ua430 Ukraine
LS59-1 2.0402 CuZn39Pb1 Messing hexahedron 3*30 42.9 Ua430 Ukraine
LS59-1 2.0402 CuZn39Pb1 Messing hexahedron 6*50 480 Ua430 Ukraine