| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Blatt |
0,8х920х2470 |
1-Blatt |
15kg |
Ru120 |
|
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Blatt |
1,5х1030х1820-2100 |
8лист-Blatt |
214kg |
Ru120 |
|
| XN77TYURU |
EI437BU |
|
|
|
|
|
Blatt |
2,5х1000х2100 |
1-Blatt |
44kg |
Ru120 |
|
| XN77TYURU |
EI437BU |
|
|
|
|
|
Blatt |
2,5х1000х2100 |
5лист-Blatt |
209kg |
Ru120 |
|
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Blatt |
3,0х1010-1020х2110-2280 |
с167ф 3лист-Blatt |
168kg |
Ru120 |
|
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Blatt |
10,0х600х1430-1490 |
2лист-Blatt |
195kg |
Ru120 |
|
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Blatt |
10,0х600х1440 |
1-Blatt |
66kg |
Ru120 |
|
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Blatt |
10,0х600х900-1370 |
2лист-Blatt |
104kg |
Ru120 |
|
| XN77TYu |
EI437A |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Kreis |
Durchmesser 12 Länge 3000-3700 |
|
13 |
Ru120 |
|
| XN77TYu |
EI437A |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Kreis |
Durchmesser 18 Länge 2980-3070 |
|
13 |
Ru120 |
|
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Kreis |
Durchmesser 43 Länge 690;730 |
|
17 |
Ru120 |
|
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Kreis |
Durchmesser 53 Länge 650 |
|
12 |
Ru120 |
|
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Kreis |
Durchmesser 53 Länge 2300-3400 |
|
115 |
Ru120 |
|
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Kreis |
Durchmesser 114 Länge 1000 |
|
84 |
Ru120 |
|
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Kreis |
ф10mm |
|
78 |
Ru130 |
|
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Kreis |
ф16mm |
|
147 |
Ru130 |
|
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Kreis |
ф17mm |
|
50 |
Ru130 |
|
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Kreis |
ф18mm |
|
145 |
Ru130 |
|
| XN77TYu |
EI437A |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Kreis |
ф43mm |
|
244 |
Ru130 |
|
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Kreis |
ф20mm |
|
3 |
Ru130 |
|
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Kreis |
ф30mm |
|
28 |
Ru130 |
|
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Blatt |
#2х1000х1640-2000mm |
|
65 |
Ru130 |
|
| XN77TYu |
EI437A |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Draht |
2,0 mm |
|
20 kg |
Ru150 |
|
| XN77TYu |
EI437A |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Kreis |
35 mm |
|
116 kg |
Ru150 |
|
| XN77TYu-ш |
EI437A |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Kreis |
60 mm |
|
118 kg |
Ru150 |
|
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Kreis |
13 mm |
|
42 kg |
Ru150 |
|
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Blatt |
2 х715х1275 mm mm |
|
15,1 kg |
Ru310 |
|
| XN77TYUR |
EI437BU-вд |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Kreis |
Ø 22х2500 mm mm |
|
32 kg |
Ru310 |
|
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Kreis |
ф16mm-1,0-1,5 m |
|
43 |
Ua010 |
Ukraine |
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Kreis |
Ф22 415 |
|
1.3 |
Ua120 |
Ukraine |
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Draht |
Durchmesser 5 |
|
4.6 |
Ua140 |
Ukraine |
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Draht |
Durchmesser 6 |
|
5.6 |
Ua140 |
Ukraine |
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Draht |
Durchmesser 4 |
|
13 |
Ua140 |
Ukraine |
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Kreis |
20mm |
0,91+0,96 m=5kg Stigma ei-437 |
5.0 |
Ua210 |
Ukraine |
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Kreis |
25 mm |
1M(4,5 kg) - 1Stück |
4.5 |
Ua210 |
Ukraine |
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Kreis |
27,5 mm |
0,43 m(10,6 kg) - 5er |
10.7 |
Ua210 |
Ukraine |
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Kreis |
37 mm |
1+1,43 m=21,2 kg |
21.2 |
Ua210 |
Ukraine |
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Kreis |
40 mm |
|
21.7 |
Ua210 |
Ukraine |
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Kreis |
45 mm |
|
13.3 |
Ua210 |
Ukraine |
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Kreis |
45 mm |
|
18.8 |
Ua210 |
Ukraine |
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Kreis |
53 mm |
|
25.4 |
Ua210 |
Ukraine |
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Kreis |
55 mm |
|
33.3 |
Ua210 |
Ukraine |
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Kreis |
86 mm |
|
5.2 |
Ua210 |
Ukraine |
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Kreis |
153 mm |
|
41.3 |
Ua210 |
Ukraine |
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Draht |
5mm |
|
31.9 |
Ua210 |
Ukraine |
| XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Kreis |
40mm |
0,38 m 4kg Stigma ei-437БВД D |
4 |
Ua220 |
Ukraine |