| OT4-0 |
|
|
|
|
Titan gost OT4-0 |
Titanmetall |
Kreis |
20х270-920 |
4St |
5.1 |
Ru240 |
|
| OT4-0 |
|
|
|
|
Titan gost OT4-0 |
Titanmetall |
Kreis |
34х300 |
1Stück |
2.4 |
Ru240 |
|
| OT4-0 |
|
|
|
|
Titan gost OT4-0 |
Titanmetall |
Kreis |
36х300 |
1Stück |
2.9 |
Ru240 |
|
| OT4-0 |
|
|
|
|
Titan gost OT4-0 |
Titanmetall |
Kreis |
38х260-360 |
7шт |
11.9 |
Ru240 |
|
| OT4-0 |
|
|
|
|
Titan gost OT4-0 |
Titanmetall |
Kreis |
40х400-520 |
2St |
12.8 |
Ru240 |
|
| OT4-0 |
|
|
|
|
Titan gost OT4-0 |
Titanmetall |
Kreis |
50х230 |
1Stück |
2 |
Ru240 |
|
| OT4-0 |
|
|
|
|
Titan gost OT4-0 |
Titanmetall |
Kreis |
60х200 |
1Stück |
2.5 |
Ru240 |
|
| OT4-0 |
|
|
|
|
Titan gost OT4-0 |
Titanmetall |
Kreis |
90х250 |
1Stück |
7 |
Ru240 |
|
| OT4-0 |
|
|
|
|
Titan gost OT4-0 |
Titanmetall |
Blatt |
0.5х600х2000 |
|
5 |
Ru240 |
|
| OT4-0 |
|
|
|
|
Titan gost OT4-0 |
Titanmetall |
Blatt |
3х350х910 |
Karten |
4.2 |
Ru240 |
|
| OT4-0 |
|
|
|
|
Titan gost OT4-0 |
Titanmetall |
Rohr |
25x2.5x |
1Stück |
2.4 |
Ru240 |
|
| OT4-0 |
|
|
|
|
Titan gost OT4-0 |
Titanmetall |
Blatt |
0.5х600х2000 |
14шт ver. |
38,3 |
Ru250 |
|
| OT4-0 |
|
|
|
|
Titan gost OT4-0 |
Titanmetall |
Kreis |
16 |
VSMPO |
198 |
Ru260 |
|
| OT4-0 |
|
|
|
|
Titan gost OT4-0 |
Titanmetall |
Kreis |
40х1300 |
|
1240 |
Ru260 |
|
| OT4-0 |
|
|
|
|
Titan gost OT4-0 |
Titanmetall |
Kreis |
45х1300 |
|
1410 |
Ru260 |
|
| OT4-0 |
|
|
|
|
Titan gost OT4-0 |
Titanmetall |
Kreis |
70 |
|
504 |
Ru260 |
|
| OT4-0 |
|
|
|
|
Titan gost OT4-0 |
Titanmetall |
Rohr |
12x1 |
|
75 |
Ru260 |
|
| OT4-0 |
|
|
|
|
Titan gost OT4-0 |
Titanmetall |
Kreis |
ф14 28,1 - 34,7 |
|
1 |
Ua010 |
Ukraine |
| OT4-0 |
|
|
|
|
Titan gost OT4-0 |
Titanmetall |
Kreis |
Ф10 25,1 |
|
1 |
Ua010 |
Ukraine |
| OT4-0 |
|
|
|
|
Titan gost OT4-0 |
Titanmetall |
Kreis |
68 mm |
0,64 m(11kg) Stigma 1Stück |
11 |
Ua210 |
|
| OT4-0 |
|
|
|
|
Titan gost OT4-0 |
Titanmetall |
Kreis |
77 mm |
0,57 m(12kg) 1Stück gemeißelt |
12 |
Ua210 |
|
| OT4-0 |
|
|
|
|
Titan gost OT4-0 |
Titanmetall |
Kreis |
80 mm |
0,9 m(20,6 kg) Stigma 1Stück |
20.6 |
Ua210 |
|
| OT4-0 |
|
|
|
|
Titan gost OT4-0 |
Titanmetall |
Kreis |
89 mm |
0,61 m(18,9 kg) Stigma 1Stück |
18.9 |
Ua210 |
|
| OT4-0 |
|
|
|
|
Titan gost OT4-0 |
Titanmetall |
Blatt |
3,5 mm |
0,49x1,48m(11,6 kg) 1Stück |
11.6 |
Ua210 |
|
| OT4-0 |
|
|
|
|
Titan gost OT4-0 |
Titanmetall |
Blatt |
3,5 mm |
1x2м(31,6 kg) 1Stück markiert |
31.6 |
Ua210 |
|