| Markierung | W. Nr. | Titel | Stahl Typ | Form | Größe | Kommentar | Die Balance |
|---|---|---|---|---|---|---|---|
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Blatt | 5,0 x 800 x 1000 mm | 470 kg | |
| BT5 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 20x | L = 2,8 m m/O | 4 |
| BT5 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 30х1290-3600 | G/K | 388.2 |
| BT5 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 35х1750-2460 | Presse. (Einrisse auf, Krümmung) | 107.5 |
| BT5 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 65х1350 | 19.5 | |
| BT5 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 70х780 | 3.5 | |
| BT5 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 123х325-390 | 104 | |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 14х2700-3500 | 213 | |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 20х934-1992 | m/O | 12.5 |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 35х440-500 | G/K | 19 |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 50er | 22 | |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 65х1170-1415 | 77.5 | |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 70х1100-2070 | 77 | |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Blatt | 2.5х1000х1810-2000 | ГОСТ1-90218-76 | 66.7 |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Blatt | 4х1000х2000 | 1140 | |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Blatt | 8х420х775 | Karten | 11.6 |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Rohr | 110х14х450mm | 8.2 | |
| BT5 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 10 | 36,7 | |
| BT5 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 18х2180 | VFR | 2,6 |
| BT5 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 20х1430 | VFR | 2 |
| BT5 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 20х2900 | G/K | 4,1 |
| BT5 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 24х920 | G/K | 2 |
| BT5 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 25х820-1500 | 51,2 | |
| BT5 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 25х330 | G/K | 1,4 |
| BT5 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 28х1045 | m/O | 2,8 |
| BT5 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 30х310-490 | G/K | 6 |
| BT5 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 35х955-1060 | 2St G/K | 8,6 |
| BT5 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 35х955-1060 | 2 Stück G/zum auflegen auf kalt. 4,1 kg + 4,5 kg | 8,6 |
| BT5 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 40х220-330 | G/K | 3 |
| BT5 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 45х280-600 | G/K | 6,4 |
| BT5 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 50х300 | G/K | 2,6 |
| BT5 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 54х630 | G/K | 6,4 |
| BT5 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 55х250 | G/K | 2,6 |
| BT5 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 65 | G/K | 18,5 |
| BT5 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 150х850 | Ing. | 65,8 |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 10х870-1460 | 30,8 | |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 16х1500 | 61,9 | |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 20х1500 | 30,3 | |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 25х1000 | 14,5 | |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 30х855 | m/O | 2,6 |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 40х200-300 | G/K | 13,2 |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 45х380-1000 | 9,8 | |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 50х1200 | 25,3 | |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 55х250-1000 | 11,7 | |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 60 | 24,5 | |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 65х1350 | G/K | 20,1 |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 65 | unter die Bestellung | 600 |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 70х270 | G/K | 5 |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 70 | unter die Bestellung | 600 |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 75 | 136,6 | |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 80 | unter die Bestellung | 600 |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 90 | unter die Bestellung | 600 |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 100х1100-2200 | 740 | |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 110х1050-2100 | 746 | |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 120х1050-1550 | 730 | |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 130х1000-1500 | 750 | |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 140х1000-1500 | m/O | 745 |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 150х1000-1410 | 7 Stück G/zum auflegen | 724,9 |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 10 | 180kg | |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 40 | 12 | |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 12 | Kern(h9) | 3 |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 25 | G/K ОСТ1 90173-75 | 114 |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Kreis | 42 | 500 m/O 9006 | 412 |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Blatt | 4mm | 0,91x1,5m(25,1 kg) 1pc | 25.1 |
| VT5-1 | 3.7115 | Titan Grade 6 | Titanmetall | Blatt | 4mm | 1x2м(36,2+35,8+35,2+37,5+35+35,6+35,7+35,6 kg) nach 1piece | 286.6 |
| BT5 | 3.7115 | Titan Grade 6 | Titanmetall | Blatt | 4х1000х2000 | 357,1 |