| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
10x |
G/K |
207 |
Ru240 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
20х300 |
|
1.2 |
Ru240 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
25х280-590 |
10er |
8 |
Ru240 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
25х1880 |
1Stück,G/K |
4.1 |
Ru240 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
28х270 |
|
2.7 |
Ru240 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
30x |
m/O, L =500mm |
15 |
Ru240 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
30х250 |
|
19.2 |
Ru240 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
32х300 |
|
2.9 |
Ru240 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
35x |
G/K, L =640mm |
2.8 |
Ru240 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
35х280-360 |
|
5.5 |
Ru240 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
37х245 |
|
1.2 |
Ru240 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
40х270-450 |
3tlg |
6.5 |
Ru240 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
45х170-250 |
2St |
2.8 |
Ru240 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
50er |
G/K, L =500-706мм |
10 |
Ru240 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
55х200-300 |
9pcs |
14.3 |
Ru240 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
58х230-310 |
|
29.7 |
Ru240 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
60х190-250 |
10er |
14.8 |
Ru240 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
65х190-250 |
4St |
13.5 |
Ru240 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
70х220-235 |
2St |
8.6 |
Ru240 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
75х200-210 |
2St |
8.5 |
Ru240 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
90х160 |
1Stück |
4.8 |
Ru240 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
100х170 |
1Stück |
6.1 |
Ru240 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
10х3200 |
G/K |
26,9 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
10х420-1200 |
VFR |
3,8 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
10х1040-2400 |
VFR |
109,6 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
10х3200 |
G/K |
26,9 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
13х2680 |
Kaliber. |
1,6 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
16х500-1050 |
G/K |
23,5 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
16х200 |
Kaliber. |
50 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
16х1130-1260 |
G/K |
18 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
16х1150-1880 |
VFR |
94,9 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
16х200 |
shlif. |
11 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
18х1960 |
shlif. |
2,2 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
18х1065-1120 |
shlif. |
20,3 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
19х200 |
Kaliber. |
50 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
19х200 |
shlif. |
9,8 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
20х210-500 |
Kern, G/K |
7,8 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
20х1060-1140 |
6ST Schliff., Mark. Stirnseitig |
9,2 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
20х1400-1700 |
VFR |
36,9 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
20х1250 |
m/O |
1,7 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
20х1000 |
G/K |
1,5 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
24х840 |
shlif. |
1,7 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
25х320-500 |
G/K |
9,3 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
25х2045 |
shlif. |
4,4 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
25х200 |
shlif. |
5 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
25х1030-2115 |
Kaliber. |
16,3 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
25х2115 |
shlif. |
4,6 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
25х3230-3555 |
2St G/K |
14,6 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
27х1040-1110 |
11шт Schliff., Mark. Stirnseitig |
30,4 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
27х1050-1500 |
shlif. |
52,8 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
28х200-300 |
Kaliber. |
50 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
28х1990 |
1 Stück m/O |
5,4 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
28х1030-1240 |
shlif. |
60,2 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
30х1490 |
1 Stück m/O |
4,7 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
30х1500 |
G/K |
5,4 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
30х790 |
shlif. |
2,5 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
32х1050-1110 |
11шт Schliff., Mark. Stirnseitig |
42,6 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
32х1050-1140 |
10er Kaliber. |
38,5 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
35х1080-1140 |
8st Schliff., Mark. Stirnseitig |
38 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
35х2235-2800 |
4St G/K |
43,6 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
35х210-880 |
G/K |
20,7 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
35х1130-2800 |
papierzwischenlagen, G/K |
73,3 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
36х220 |
m/O |
1 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
38х470 |
G/K |
2,4 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
40х830 |
G/K |
4,6 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
40х1000 |
G/zum auflegen |
5,6 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
40х830 |
G/K |
4,6 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
40х330-540 |
G/K |
7,9 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
45х200 |
m/O |
1,4 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
50х590-800 |
2 Stück (5kg und 6,9 kg) G/K |
11.9 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
50х200 |
G/K |
1,7 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
55х500 |
shlif. |
5,3 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
60х310 |
G/K |
3,7 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
60х810 |
papierzwischenlagen, Mark. Stirnseitig |
10,3 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
60х380 |
G/K |
5,1 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
65х1110 |
shlif. |
16,2 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
65х385 |
m/O Mark. Stirnseitig |
5,9 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
65х1130 |
shlif. |
16,4 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
65х910 |
Ing. |
15,9 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
70х120х370 |
14,4 |
|
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
70х185 |
G/K |
3,3 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
90х380 |
shlif. |
11 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
90х175 |
m/O |
5,2 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
100х135 |
G/K |
4,9 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
100х1700 |
G/K |
63,7 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
110х135 |
m/O |
5,8 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
110х220 |
G/K |
9,4 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
130х165 |
m/O |
10,1 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
130х150 |
m/O |
9,1 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
130х400 |
m/O |
24,1 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
130х135 |
m/O |
8,1 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
130х1470 |
G/K |
88,8 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
130х210 |
G/K |
12,6 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
130х140 |
m/O |
8,4 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
150 |
|
30,3 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
150х140 |
G/K |
11,1 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
160х100 |
m/O |
50,5 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
165х100 |
10er Ausschnitt aus der Platte |
103,9 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
190х180 |
Ing. Aufleg |
25,8 |
Ru250 |
|
| VT3-1 |
|
|
|
|
Titan gost VT3-1 |
Titanmetall |
Kreis |
200х190 |
Ing. |
25,8 |
Ru250 |
|