Kaufen АМГ3
Lager
Zusätzliche Felder
| Markierung | W. Nr. | Titel | Stahl Typ | Form | Größe | Kommentar | Die Balance |
|---|---|---|---|---|---|---|---|
| AMG3M | Aluminium | Blatt | 6mm | Aluminium 1,5x2м (an den Ecken Löcher ф5мм) 1g | 46 | ||
| AMG3M | Aluminium | Blatt | 4,0*1500*3500 | 100er | |||
| AMG3M | Aluminium | Blatt | 6,0*1500*0 | Stück | |||
| AMG3M | Aluminium | Blatt | 6,0*1500*4050 | 24x | |||
| AMG3M | Aluminium | Blatt | 6,0*1600*4000 | 4 | |||
| AMG3M | Aluminium | Blatt | 4х1500х3500 | 154 | |||
| AMG3M | Aluminium | Blatt | 6х1600х4000 | 112 | |||
| AMG3 | Aluminium | Kreis | 40 | 450 | |||
| AMg3N | Rohr | 34х1; 34х2 | 139,4 | ||||
| AMG3 | Aluminium | Draht | 2 | 62,72 |